Using nanoindentation to investigate the temperature cycling of Sn-37Pb solders

被引:3
|
作者
Wen, Hua-Chiang [1 ]
Chou, Wu-Ching [1 ]
Lin, Po-Chen [2 ]
Jeng, Yeau-Ren [3 ]
Chen, Chien-Chang [4 ]
Chen, Hung-Ming [5 ]
Jiang, Don Son [6 ]
Cheng, Chun-Hu [7 ]
机构
[1] Natl Chiao Tung Univ, Dept Electrophys, Hsinchu 300, Taiwan
[2] Natl Chiao Tung Univ, Dept Mech Engn, Hsinchu 300, Taiwan
[3] Natl Chung Cheng Univ, Dept Mech Engn, Chiayi 621, Taiwan
[4] Natl Chiao Tung Univ, Res Grp Biomed Image Proc, Shing Tung Yau Ctr, Hsinchu 300, Taiwan
[5] Natl Chiao Tung Univ, Dept Elect Engn, Hsinchu 300, Taiwan
[6] Siliconware Precis Ind Co Ltd, Mat & Design Engn Div, Engn Ctr, Taichung 400, Taiwan
[7] Natl Taiwan Normal Univ, Dept Mechatron Engn, Taipei 106, Taiwan
关键词
Intermetallic compounds; Diffusion; Recrystallization; Electron microscopy; LOW-COST; RECRYSTALLIZATION; JOINTS; MICROSTRUCTURE; ALLOYS; INTERCONNECTIONS; MORPHOLOGY; EVOLUTION; STRESS;
D O I
10.1016/j.microrel.2017.05.004
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Using nanoindentation and energy dispersive X-ray spectrometry (EDS), we have conducted an investigation into corner failures to elucidate not only the nanomechanical properties of Sn-37Pb solder balls but also the effects of temperature cycling tests (TCTs). We found that the hardness of Sn-37Pb solder balls was greater in central locations [1.18 +/- 0.05 GPa for room-temperature (RT) sample; 1.3 +/- 0.05 GPa for TCT sample], but had standard values in corner locations (>0.2 +/- 0.02 GPa). The modulus increased after the TCTs. Nevertheless, the mechanical properties were closely related to the average area of the alpha-Pb phase. The average area of the Pb-rich region was more stable after the TCTs than that of the RT sample, due to the enhanced mechanical properties of the Sn-37Pb solder, suggesting good reliability. From an analysis of average areas in the RT sample, it appears that the Pb-rich solid solution that formed led to weak Sn-Pb bonds near the corner locations. Electron back scattered diffraction measurements revealed that grains with grain boundaries formed as a result of accelerated TCT cycling. We conclude that Sn-Pb recrystallization was initiated and propagated after the TCTs, followed by propagation to the interfacial region. (C) 2017 Published by Elsevier Ltd.
引用
收藏
页码:111 / 117
页数:7
相关论文
共 50 条
  • [31] The wetting phenomenon and precursor film characteristics of Sn-37Pb/Cu under ultrasonic fields
    Yang, Yao
    Li, Shaorong
    Liang, Yuxin
    Li, Bangsheng
    MATERIALS LETTERS, 2019, 234 : 92 - 95
  • [32] Dependence of Electrical Resistivity on Temperature and Sn Content in Pb-Sn Solders
    Cadirli, E.
    Boyuk, U.
    Kaya, H.
    Marasli, N.
    Aksoz, S.
    Ocak, Y.
    JOURNAL OF ELECTRONIC MATERIALS, 2011, 40 (02) : 195 - 200
  • [33] Dependence of Electrical Resistivity on Temperature and Sn Content in Pb-Sn Solders
    E. ÇadIrlI
    U. Böyük
    H. Kaya
    N. Maraşli
    S. Aksöz
    Y. Ocak
    Journal of Electronic Materials, 2011, 40 : 195 - 200
  • [34] Analysis of interfacial reactions between Sn-37Pb and Ni by phase diagram calculation method
    Material Science and Engineering College, Harbin University Science Technique, Harbin 150040, China
    Hanjie Xuebao, 2006, 6 (29-32):
  • [35] Mechanical reliability evaluation of Sn-37Pb solder joint using high speed lap-shear test
    Jeon, Seong-jae
    Hyun, Seungmin
    Lee, Hak-Joo
    Kim, Jong-Woong
    Ha, Sang-Su
    Yoon, Jeong-Won
    Jung, Seung-Boo
    Lee, Hoo-Jeong
    MICROELECTRONIC ENGINEERING, 2008, 85 (10) : 1967 - 1970
  • [36] Brittle fracture of Sn-37Pb solder joints induced by enhanced intermetallic compound growth under extreme temperature changes
    Tian, Ruyu
    Hang, Chunjin
    Tian, Yanhong
    Xu, Jikai
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2019, 268 : 1 - 9
  • [37] Evaluation of drop reliability of Sn-37Pb solder/Cu joints using a high speed lap-shear test
    Jeon, Seong-jae
    Kim, Jong-Woong
    Lee, Byunghoon
    Lee, Hak-Joo
    Jung, Seung-Boo
    Hyun, Seungmin
    Lee, Hoo-Jeong
    MICROELECTRONIC ENGINEERING, 2012, 91 : 147 - 153
  • [38] Creep-fatigue properties of Sn-37Pb solder material evaluated by room temperature testing under various strain waveforms
    Tokimasa, K
    JSME INTERNATIONAL JOURNAL SERIES A-SOLID MECHANICS AND MATERIAL ENGINEERING, 2004, 47 (03) : 380 - 388
  • [39] Experiments and simulations of uniaxial ratchetting deformation of Sn-3Ag-0.5Cu and Sn-37Pb solder alloys
    Kobayashi, Takuji
    Sasaki, Katsuhiko
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2009, 20 (04) : 343 - 353
  • [40] Sn-37Pb焊球与Ni/NiP UBM界面反应特性研究
    田飞飞
    刘清君
    李勇
    固体电子学研究与进展, 2020, 40 (02) : 154 - 158