Dry sliding wear behavior of Saffil fiber-reinforced Mg-10Gd-3Y-0.5Zr magnesium alloy-based composites

被引:2
|
作者
Hu, Bin [1 ,2 ]
Peng, Liming [1 ,2 ]
Ding, Wenjiang [1 ,2 ]
机构
[1] Shanghai Jiao Tong Univ, Natl Engn Res Ctr Light Alloy Net Forming, Shanghai 200240, Peoples R China
[2] Shanghai Jiao Tong Univ, State Key Lab Met Matrix Composites, Shanghai 200240, Peoples R China
关键词
Magnesium alloy; metal matrix composites; dry sliding wear; wear mechanism; METAL-MATRIX COMPOSITES; ALUMINUM COMPOSITES; HYBRID COMPOSITES; MECHANISM; FRICTION; AL2O3;
D O I
10.1177/0021998310377938
中图分类号
TB33 [复合材料];
学科分类号
摘要
Dry sliding wear behavior of the creep-resistant magnesium alloy Mg-10Gd-3Y-0.5Zr and its composites have been investigated in this study. Magnesium matrix composites are prepared by squeezing casting infiltration of Mg alloy into Saffil preforms. Wear tests are conducted using ball-on-flat sliding wear set up under a sliding velocity range of 1-15 cm/s and at an applied load range of 1-8 N for a constant sliding distance of 150 m. According to results, mechanical and wear-resistance properties of magnesium alloy improved by introducing Saffil fibers, and the alumina binder composite has a higher strength and lower wear rate than silica binder composite. The wear rates of the matrix alloy, composites and their counter-face balls increase with increasing applied load. The increment of sliding velocities decreases the wear rate of the matrix alloy under the tested sliding velocities. A critical threshold of sliding velocity for the wear rate of both composites and their counter-faces is about 9 cm/s. Abrasion and plastic deformation are considered to be the dominant mechanism for the matrix alloy in tested conditions, and for both composites under low sliding velocity (< 10 cm/s) and at low applied loads (1-5 N). Delamination is the wear mechanism of the silica binder composites at a high applied load (8 N). Adhesion and oxidation are the controlling wear mechanism of matrix alloy and composites under a sliding velocity of 15 cm/s.
引用
收藏
页码:683 / 693
页数:11
相关论文
共 50 条
  • [21] Influence of GdCl3 addition on purifying effectiveness and properties of Mg-10Gd-3Y-0.5Zr alloy
    吴国华
    王玮
    孙明
    王渠东
    丁文江
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20 (07) : 1177 - 1183
  • [22] Influence of GdCl3 addition on purifying effectiveness and properties of Mg-10Gd-3Y-0.5Zr alloy
    Wu Guo-hua
    Wang Wei
    Sun Ming
    Wang Qu-dong
    Ding Wen-jiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (07) : 1177 - 1183
  • [23] Operating slip modes and inhomogeneous plastic deformation of Mg-10Gd-3Y-0.5Zr alloy during compression
    Jiang, Zhi-wei
    Yin, Dong-di
    Wan, You-fu
    Ni, Ran
    Zhou, Hao
    Zheng, Jiang
    Wang, Qu-dong
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2023, 33 (01) : 79 - 94
  • [24] Influence of heat treatment on cyclic deformation and low-cycle fatigue behavior of sand-cast Mg-10Gd-3Y-0.5Zr magnesium alloy
    Wang, Quan
    Liu, Wencai
    Wu, Guohua
    Chen, Xiangjun
    Zhang, Haohao
    JOURNAL OF MATERIALS RESEARCH, 2017, 32 (11) : 2179 - 2187
  • [25] EFFECT OF MINOR Ag and Ce ADDITIONS ON HOT TEARING SUSCEPTIBILITY OF Mg-10Gd-3Y-0.5Zr ALLOY
    Liao, Jinge
    Song, Jiangfeng
    Chen, Gong
    Zhao, Hua
    Tong, Shengkun
    Zhou, Jun
    Jiang, Bin
    Xu, Junyao
    Pan, Fusheng
    INTERNATIONAL JOURNAL OF METALCASTING, 2023, 17 (04) : 2689 - 2701
  • [26] Mg-10Gd-3Y-0.5Zr合金热压缩动态析出规律
    郑婷婷
    李德江
    曾小勤
    丁文江
    材料科学与工程学报, 2016, 34 (06) : 867 - 873
  • [27] Dry sliding wear behavior of cast Mg-11Y-5Gd-2Zn magnesium alloy
    Hu Mao-liang
    Wang Qu-dong
    Li Cheng
    Ding Wen-jiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 (08) : 1918 - 1923
  • [28] Microstructure evolution of semi-solid Mg-10Gd-3Y-0.5Zr alloy during isothermal heat treatment
    Wu, Guohua
    Zhang, Yang
    Liu, Wencai
    Ding, Wenjiang
    JOURNAL OF MAGNESIUM AND ALLOYS, 2013, 1 (01) : 39 - 46
  • [29] Influence of flux containing YCl3 additions on purifying effectiveness and properties of Mg-10Gd-3Y-0.5Zr alloy
    Wang, Wei
    Huang, Yuguang
    Wu, Guohua
    Wang, Qudong
    Sun, Ming
    Ding, Wenjiang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 480 (02) : 386 - 391
  • [30] Gd contents, mechanical and corrosion properties of Mg-10Gd-3Y-0.5Zr alloy purified by fluxes containing GdCl3 additions
    Wang, Wei
    Wu, Guohua
    Wang, Qudong
    Huang, Yuguang
    Ding, Wenjiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 507 (1-2): : 207 - 214