Stress corrosion cracking growth rates of candidate canister materials for spent nuclear fuel storage in chloride-containing atmosphere

被引:20
|
作者
Tani, Jun-Ichi [1 ]
Mayuzumi, Masarni
Arai, Taku
Hara, Nobuyoshi
机构
[1] Cent Res Inst Elect Power Ind, Mat Sci Res Lab, Yokosuka, Kanagawa 2400196, Japan
[2] Tokyo Inst Technol, Grad Sch Sci & Engn, Dept Engn Sci & Mech, Tokyo 1528552, Japan
[3] Tohoku Univ, Grad Sch Engn, Dept Met, Sendai, Miyagi 9808579, Japan
关键词
concrete cask; stainless steel; canister; stress corrosion cracking; sea salt;
D O I
10.2320/matertrans.MRA2006367
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Chloride-induced stress corrosion crack growth rates were measured for candidate canister materials in a simulated marine atmospheric environment. Half-inch compact tension specimens were used to obtain stress corrosion crack growth rates by applying a direct-current potential-drop method to measure crack lengths. The crack growth rates of S31603 and S31260 stainless steels were 3 x 10(-10) m center dot s(-1) and 4 x 10(-13) m center dot S-1 for an applied stress intensity factor of 30 MPa center dot m (0.5), respectively, at a test temperature of 353 K at a relative humidity of 35%. S31254 specimens did not show stress corrosion cracking susceptibility under the same conditions as above, suggesting their superior resistance to chloride-induced stress corrosion cracking. These data were consistent with the results that S31260 and S31254 stainless steels did not fail after up to 37700 h although S31603 failed after 533 h in constant-load tests under the same environmental conditions. Assuming active-path corrosion to be an anodic subprocess of stress corrosion crack growth, anodic polarization Curves of the test materials were obtained in a synthetic seawater solution of pH I at 353 K. The maximum anodic current density of the active dissolution of S31603 stainless steel was ten times as large as that of S31260 stainless steel. This result qualitatively explains the difference in the crack growth behavior between S31603 and S31260 stainless steels.
引用
收藏
页码:1431 / 1437
页数:7
相关论文
共 42 条
  • [41] Evaluation of crack growth of chloride-induced stress corrosion cracking in dry storage system under different environmental conditions
    Wang, Wen-Yu
    Tseng, Yung-Shin
    Yeh, Tsung-Kuang
    [J]. PROGRESS IN NUCLEAR ENERGY, 2020, 130
  • [42] The effect of prior deformation on stress corrosion cracking growth rates of Alloy 600 materials in a simulated pressurized water reactor primary water
    Yamazaki, Seiya
    Lu, Zhanpeng
    Ito, Yuzuru
    Takeda, Yoichi
    Shoji, Tetsuo
    [J]. CORROSION SCIENCE, 2008, 50 (03) : 835 - 846