Strength and failure characteristics of rock-like material containing single crack under freeze-thaw and uniaxial compression

被引:98
|
作者
Huang, Shibing [1 ,2 ]
Liu, Yanzhang [1 ,2 ]
Guo, Yunlin [1 ]
Zhang, Zelin [1 ,2 ]
Cai, Yuantian [1 ]
机构
[1] Wuhan Univ Sci & Technol, Sch Resources & Environm Engn, Wuhan, Hubei, Peoples R China
[2] Hubei Key Lab Efficient Utilizat & Agglomerat Met, Wuhan, Hubei, Peoples R China
基金
中国国家自然科学基金;
关键词
Fractured rock mass; Freeze-thaw; Frost propagation; Uniaxial compressive strength; Rupture mode; MECHANICAL-PROPERTIES; MODEL; INITIATION; BEHAVIOR; DAMAGE; FLAW; DEGRADATION; TEMPERATURE; PROPAGATION; PARAMETERS;
D O I
10.1016/j.coldregions.2019.03.013
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
The frost heaving pressure in cracks, caused by 9% volumetric expansion of freezing water, may deteriorate fractured rock. Several freeze-thaw cycles and uniaxial compressive experiments were conducted on crack-containing specimens to study the frost propagation of open cracks and uniaxial compressive strength (UCS) of these frost-cracking specimens. The experimental results show that new frost-heaving cracks initiate at the crack tip and grow along the coplanar direction firstly, then most of them turn to the short side of specimens because of boundary effect. The frost cracking of saturated rock is greatly affected by the freezing direction. If the preexisted crack is saturated before freezing, new frost-heaving cracks will appear after only 1-4 freeze-thaw cycles. However, no frost-heaving crack occurs after 20 freeze-thaw cycles if water is injected into the precooling crack after freezing, because > 8% crack ice is squeezed out of crack. Morever, the UCS of crack-containing rock-like specimens will be reduced by these new frost-heaving cracks when the inclination angle of pre-existed crack is close to the rupture angle, and the UCS increases with increasing inclination angle or decreasing crack length.
引用
收藏
页码:1 / 10
页数:10
相关论文
共 50 条
  • [21] Crack coalescence morphology in rock-like material under compression
    Jooeun Lee
    Youn Doh Ha
    Jung-Wuk Hong
    International Journal of Fracture, 2017, 203 : 211 - 236
  • [22] Experimental and numerical study on crack development characteristics between two cavities in rock-like material under uniaxial compression
    Liu, Bing
    Zhou, Yu
    Gao, Yong-Tao
    Xu, Chaoshui
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2020, 109
  • [23] A damage constitutive model of rock-like materials containing a single crack under the action of chemical corrosion and uniaxial compression
    Pan, Ji-liang
    Cai, Mei-feng
    Li, Peng
    Guo, Qi-feng
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2022, 29 (02) : 486 - 498
  • [24] Influence of Two Cross-Flaws Geometry on the Strength and Crack Coalescence of Rock-Like Material Specimens under Uniaxial Compression
    Zhang, B.
    Li, Y.
    Yang, X. Y.
    Li, S. C.
    Liu, B.
    Xu, Z. H.
    Pei, Y.
    INTERNATIONAL JOURNAL OF GEOMECHANICS, 2020, 20 (08)
  • [25] Research on dynamic compressive characteristics of rock-like material considering the influence of crack angles and freeze–thaw cycles
    Songtao Yu
    Hongwei Deng
    Guanglin Tian
    Yuxian Ke
    Arabian Journal of Geosciences, 2022, 15 (6)
  • [26] On the Strength and Crack Propagation Process of the Pre-Cracked Rock-Like Specimens under Uniaxial Compression
    Haeri, H.
    Shahriar, K.
    Marji, M. F.
    Moarefvand, P.
    STRENGTH OF MATERIALS, 2014, 46 (01) : 140 - 152
  • [27] On the Strength and Crack Propagation Process of the Pre-Cracked Rock-Like Specimens under Uniaxial Compression
    H. Haeri
    K. Shahriar
    M. F. Marji
    P. Moarefvand
    Strength of Materials, 2014, 46 : 140 - 152
  • [28] Experimental and numerical investigation on crack mechanism of folded flawed rock-like material under uniaxial compression
    Fan, Wenchen
    Yang, Hui
    Jiang, Xueliang
    Cao, Ping
    ENGINEERING GEOLOGY, 2021, 291
  • [29] Study on Failure Characteristics and Acoustic Emission Laws of Rock-like Specimens under Uniaxial Compression
    Dai, Shuhong
    Sun, Qinglin
    Hao, Ruiqi
    Xiao, Yuxuan
    APPLIED SCIENCES-BASEL, 2024, 14 (19):
  • [30] Failure characteristics of brittle rock-like specimen with fractured internal structure under uniaxial compression
    Yusong Zhao
    Yongtao Gao
    Shunchuan Wu
    Congcong Chen
    Arabian Journal of Geosciences, 2020, 13