INFLUENCE OF THE MODES OF ION NITRIDING ON THE FRETTING-FATIGUE OF 40KH STEEL

被引:0
|
作者
Kaplun, P., V [1 ]
Honchar, V. A. [1 ]
机构
[1] Khmelnytskyi Natl Univ, Khmelnytskyi, Ukraine
关键词
fretting-fatigue with bending; ion nitriding; service life; hydrogen-free medium; hydrogen-containing medium; HYDROGEN;
D O I
10.1007/s11003-019-00266-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We present the results of experimental investigation of the fretting-fatigue with bending for 40Kh steel after ion nitriding in hydrogen-free and hydrogen-containing media. The optimal mode of ion nitriding in hydrogen-free media is determined according to the criterion of maximum service life of 40Kh steel under the conditions of fretting-fatigue. We also establish the effect of hydrogen on steel after nitriding in hydrogen-containing medium.
引用
收藏
页码:796 / 802
页数:7
相关论文
共 50 条
  • [21] HYDROGEN PERMEABILITY OF 40KH STEEL IN STRESSED STATE
    VOLKOV, AK
    RYABOV, RA
    STEEL IN TRANSLATION, 1994, 24 (03) : 27 - 28
  • [22] Corrosion Cracking of 40Kh Steel with Oxygen Depolarization
    Yurchenko A.N.
    Simonov Y.N.
    Efimova O.V.
    Nikitin D.A.
    Kravchenko A.V.
    Steel in Translation, 2023, 53 (5) : 467 - 472
  • [23] Physicochemical Properties of the Surface Layers of 40Kh Steel After Hydrogen-Free Nitriding in Glow Discharge
    M. S. Stechyshyn
    M. E. Skyba
    N. M. Stechyshyna
    A. V. Martynyuk
    R. S. Mardarevych
    Materials Science, 2020, 55 : 892 - 898
  • [24] Physicochemical Properties of the Surface Layers of 40Kh Steel After Hydrogen-Free Nitriding in Glow Discharge
    Stechyshyn, M. S.
    Skyba, M. E.
    Stechyshyna, N. M.
    Martynyuk, A., V
    Mardarevych, R. S.
    MATERIALS SCIENCE, 2020, 55 (06) : 892 - 898
  • [25] Influence of the Deformation Mode on the Force Conditions of Formation of the Surface Nanostructure of 40Kh Steel
    V. І. Kyryliv
    V. І. Gurey
    О. V. Maksymiv
    І. V. Hurey
    Yu. О. Kulyk
    Materials Science, 2021, 57 : 422 - 427
  • [26] FATIGUE-STRENGTH OF FRICTION-WELDED JOINTS BETWEEN STEEL 20 AND 40KH
    VOINOV, VP
    WELDING PRODUCTION, 1972, 19 (07): : 51 - 54
  • [27] INFLUENCE OF PRELIMINARY CYCLIC LOADING ON THE DAMPING CAPACITY AND RESIDUAL LIFE OF 40KH STEEL
    SHULGINOV, BS
    BYKOVSKII, AI
    STRENGTH OF MATERIALS, 1983, 15 (08) : 1135 - 1138
  • [28] Determination of fretting parameters of hoisting rope in coalmine and fretting-fatigue behavior of steel wires
    Wang, Dagang
    Zhang, Dekun
    Ge, Shirong
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2013, 65 (06) : 436 - 448
  • [29] Influence of the Deformation Mode on the Force Conditions of Formation of the Surface Nanostructure of 40Kh Steel
    Kyryliv, V., I
    Gurey, V., I
    Maksymiv, O., V
    Hurey, I., V
    Kulyk, Yu O.
    MATERIALS SCIENCE, 2021, 57 (03) : 422 - 427
  • [30] Heat treatment effect on hydrogen permeability of steel 40Kh
    Volkov, A.K.
    Ryabov, R.A.
    Metallovedenie i Termicheskaya Obrabotka Metallov, 1997, (01): : 31 - 33