Effects of sintering protocol and dipping time on the optical properties of monolithic zirconia

被引:9
|
作者
Savas, Tuba Yilmaz [1 ]
Akin, Ceyda [2 ]
机构
[1] Selcuk Univ, Fac Dent, Dept Prosthodont, Alaaddin Keykubat Campus,Ismet Pasa St 309, TR-42250 Selcuklu, Konya, Turkey
[2] Necmettin Erbakan Univ, Fac Dent, Dept Prosthodont, Konya, Turkey
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2022年 / 127卷 / 05期
关键词
MECHANICAL-PROPERTIES; FLEXURAL STRENGTH; AGING STABILITY; CONTRAST RATIO; GRAIN-SIZE; COLOR; TRANSLUCENCY; CERAMICS; OPALESCENCE; PARAMETERS;
D O I
10.1016/j.prosdent.2021.12.004
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. The use of monolithic zirconia for restorations has become popular. However, the effects of the coloring process and sintering procedure on the optical properties of monolithic zirconia remain unclear. Purpose. The purpose of this in vitro study was to evaluate the effects of the different sintering protocols and dipping times on the CIELab color parameters, color difference (Delta E-00), translucency parameter (TP00), opalescence parameter (OP), and contrast ratio (CR) of monolithic zirconia. Materials and methods. One hundred and fifty monolithic zirconia specimens were prepared and divided into 5 groups according to different dipping times in A2 shade coloring liquid: no immersion (D0), 3 minutes (D3), 5 minutes (D5), 7 minutes (D7), and 9 minutes (D9). The specimens were further divided into 3 subgroups according to different sintering protocols (n=10): classic (C); speed (S); and super-speed sintering (SS). The CIE L*a*b* values, Delta E-00, TP00, OP, and CR values were determined with a spectrophotometer. The data were analyzed with 2-way ANOVA and Bonferroni post hoc tests (alpha=.05). Results. The effects of the sintering protocol, dipping time, and interaction of the sintering protocol and dipping time were significant for the L*, a*, b*, Delta E-00, TP00, OP, and CR parameters (P<.001). The Delta E-00 values of the SS groups were significantly higher than those of the C and S groups for all the dipping times assessed. However, only the CD3 and CD5 groups had Delta E-00 values below the acceptability threshold (<1.8). Coloring significantly reduced TP00 values and significantly increased OP and CR values in the colored groups compared with those in the D0 groups. The C and S protocols for different dipping times showed similar optical properties in TP00, OP, CR, and Delta E-00 (excluding the D0 and D9 groups) compared with the SS protocol. Conclusion. Different sintering protocols combined with various dipping times significantly affected the optical properties of monolithic zirconia. However, C and S sintering with a 3-minute and 5-minute coloring process yielded more favorable optical results than SS sintering and prolonged dipping times.
引用
收藏
页码:801.e1 / 801.e8
页数:8
相关论文
共 50 条
  • [21] Hardness and Density of Conventional and Monolithic Zirconia after Sintering
    Rukiqi, Genc
    Shal, Kujtim
    Pustina, Teuta
    Aliaj, Fisnik
    Musliu, Erik
    Lushaj, Mirjet
    INTERNATIONAL JOURNAL OF BIOMEDICINE, 2024, 14 (03)
  • [22] Optical properties of pre-colored dental monolithic zirconia ceramics
    Kim, Hee-Kyung
    Kim, Sung-Hun
    JOURNAL OF DENTISTRY, 2016, 55 : 75 - 81
  • [23] Effect of the number of coloring liquid applications on the optical properties of monolithic zirconia
    Kim, Hee-Kyung
    Kim, Sung-Hun
    DENTAL MATERIALS, 2014, 30 (09) : E229 - E237
  • [24] The effect of bleaching on the optical and physical properties of externally stained monolithic zirconia
    Tavangar, Maryam S.
    Mousavipour, Elaheh
    Ansarifard, Elham
    CLINICAL AND EXPERIMENTAL DENTAL RESEARCH, 2021, 7 (05): : 861 - 867
  • [25] Spectrophotometric examination of the optical effects of monolithic multilayered zirconia with different substrates
    Abram, Emese
    Gajtdatsy, Gabor
    Feher, Dora
    Salata, Jozsef
    Beleznai, Szabolcs
    Hermann, Peter
    Borbely, Judit
    Shen, Zhijian James
    ADVANCES IN APPLIED CERAMICS, 2020, 119 (5-6) : 261 - 266
  • [26] Effects of sintering time on translucency and color of translucent zirconia ceramics
    Durkan, Rukiye
    Simsek, Hatice
    Gokay, Gonca Deste
    Yilmaz, Burak
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2021, 33 (04) : 654 - 659
  • [27] Effect of sintering and aging processes on the mechanical and optical properties of translucent zirconia
    Kilinc, Hamiyet
    Sanal, Fatma A.
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 126 (01): : 129.e1 - 129.e7
  • [28] The influence of altering sintering protocols on the optical and mechanical properties of zirconia: A review
    Ahmed, Walaa M.
    Troczynski, Tom
    McCullagh, Anthony P.
    Wyatt, Chris C. L.
    Carvalho, Ricardo M.
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2019, 31 (05) : 423 - 430
  • [29] Evaluation of surface treatments of monolithic zirconia in different sintering stages
    Ebeid, Kamal
    Wille, Sebastian
    Salah, Tarek
    Wahsh, Marwa
    Zohdy, Maged
    Kern, Matthias
    JOURNAL OF PROSTHODONTIC RESEARCH, 2018, 62 (02) : 210 - 217
  • [30] Effect of coloring and sintering on the translucency and biaxial strength of monolithic zirconia
    Sen, Nazmiye
    Sermet, Ibrahim Bulent
    Cinar, Sevki
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (02):