The Effect of Microstructural Variation on the Hydrogen Environment-Assisted Cracking of Monel K-500

被引:33
|
作者
Harris, Zachary D. [1 ]
Dolph, Justin D. [1 ,3 ]
Pioszak, Greger L. [1 ,4 ]
Troconis, Brendy C. Rincon [1 ]
Scully, John R. [2 ]
Burns, James T. [1 ]
机构
[1] Univ Virginia, Dept Mat Sci & Engn, Ctr Electrochem Sci & Engn, Charlottesville, VA 22904 USA
[2] Univ Virginia, Dept Mat Sci & Engn, Ctr Electrochem Sci & Engn, Mat Sci & Engn, Charlottesville, VA 22904 USA
[3] Elzly Technol Corp, Reston, VA 20190 USA
[4] Exxon Mobil Corp, Houston, TX 77386 USA
关键词
GRAIN-BOUNDARY SEGREGATION; MECHANICAL-PROPERTIES; SULFUR SEGREGATION; POTENTIAL METHOD; NICKEL; FRACTURE; EMBRITTLEMENT; STRENGTH; PRECIPITATION; DIFFUSION;
D O I
10.1007/s11661-016-3486-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The influence of microstructural variation on hydrogen environment-assisted cracking (HEAC) of Monel K-500 was evaluated using five nominally peak-aged lots of material tested under slow-rising stress intensity loading while immersed in NaCl solution under cathodic polarizations. Minimal variation in HEAC resistance among material lots was observed for an applied potential of -950 mV(SCE) (E (app), vs saturated calomel), whereas lot-to-lot variability in the fracture morphology demonstrates a significant difference in the HEAC resistance at the less negative potential of -850 mV(SCE), suggesting that relatively severe H environments produce sufficient crack-tip H to minimize the impact of metallurgical differences. Sensitivity analyses accomplished by varying the inputs used in decohesion-based, micromechanical models imply significant variations in HEAC resistance are possible for realistic changes in grain boundary toughness, hydrogen uptake behavior, and yield strength. Grain size, impurity segregation (including the effects of gettering elements), grain boundary character/connectivity, and crack path tortuosity are also considered in the context of HEAC susceptibility. Yield strength, global hydrogen content, as well as impurity segregation to grain boundaries, especially boron and sulfur, are speculatively considered to be the dominant contributions in determining HEAC resistance. Modifications that would incorporate the effects of grain boundary segregation are proposed for the K (TH) model; detailed validation of such changes require high-fidelity and quantitative inputs for the degree of grain boundary segregation. Regardless, fracture mechanics-based HEAC results, detailed microstructural characterization, and micromechanical modeling were successfully coupled to gain insights into the influences governing the microstructure-dependent HEAC susceptibility of Monel K-500.
引用
下载
收藏
页码:3488 / 3510
页数:23
相关论文
共 50 条
  • [31] Experimental investigation of precision turning of Monel K-500 under dry conditions
    Zahrani, Esmaeil Ghadiri
    Sedghi, Ali
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2014, 73 (9-12): : 1265 - 1272
  • [32] PRECIPITATION HARDENING IN NICKEL-COPPER BASE ALLOY MONEL K-500
    DEY, GK
    TEWARI, R
    RAO, P
    WADEKAR, SL
    MUKHOPADHYAY, P
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1993, 24 (12): : 2709 - 2719
  • [33] Experimental investigation of precision turning of Monel K-500 under dry conditions
    Esmaeil Ghadiri Zahrani
    Ali Sedghi
    The International Journal of Advanced Manufacturing Technology, 2014, 73 : 1265 - 1272
  • [34] STRENGTH AND DUCTILITY OF Ni-Cu-BASE ALLOY MONEL K-500
    Wang
    Zhixing Xie
    Shishu Liu
    Shigui Yuan
    Chao Yang
    Hongcai(Department of Materials Science and EngineeringNortheastern University
    Transactions of Nonferrous Metals Society of China, 1995, (01) : 111 - 115
  • [35] STRENGTH AND DUCTILITY OF NI-CU-BASE ALLOY MONEL K-500
    WANG, ZX
    XIE, SH
    LIU, SG
    YUAN, C
    YANG, HG
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 1995, 5 (01) : 111 - 115
  • [36] Environment-assisted cracking of Al 2195 alloy
    Gan, Lu
    Meletis, Efstathios I.
    Materials Science Forum, 2000, 331 (II : 1619 - 1624
  • [37] MONEL K-500合金中沉淀相的沉淀行为
    袁超
    刘世贵
    杨洪才
    王志兴
    物理测试, 1994, (06) : 9 - 13
  • [38] Performance analysis of electrode materials in electro discharge machining of monel K-500
    Akgun, Mahir
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2022, 10 (03)
  • [39] Effect of strain rate on environment-assisted cracking of TiAl in aqueous solution
    Haruna, T
    Sundararajan, T
    Fujimoto, S
    Shibata, T
    HYDROGEN EFFECTS ON MATERIAL BEHAVIOR AND CORROSION DEFORMATION INTERACTIONS, 2003, : 691 - 698
  • [40] Investigating the effects of hydrogen trapping on hydrogen environment-assisted cracking of vanadium-added steels
    Vanni, Gabriel
    Simoni, Leonardo
    Schneider, Tárique H.
    Cardoso, Henrique R.P.
    Rigoni, Rômulo F.G
    Ferreira, Daniel C.F.
    Scheid, Adriano
    Kwietniewski, Carlos E.F.
    Theoretical and Applied Fracture Mechanics, 2025, 136