Long-term corrosion of HTGR graphite with SiC coating

被引:0
|
作者
Zaurbekova, Zh A. [1 ]
Blynskiy, P. A. [1 ]
Chikhray, Ye, V [1 ]
Askerbekov, S. K. [1 ]
Tolenova, A. U. [1 ]
Kenzhina, I. Ye [1 ,2 ]
Bushnev, P. A. [3 ]
机构
[1] Al Farabi Kazakh Natl Univ, Alma Ata, Kazakhstan
[2] Satbayev Univ, Alma Ata, Kazakhstan
[3] KazAlfaTech Ltd, Res Ctr, Alma Ata, Kazakhstan
来源
RECENT CONTRIBUTIONS TO PHYSICS | 2022年 / 81卷 / 02期
关键词
HTGR; graphite; SiC coating; corrosion; NUCLEAR GRAPHITE; TRANSPORT; ACCIDENT; IG-110; FUEL;
D O I
10.26577/RCPh.2022.v81.i2.06
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
When creating a Kazakhstani high-temperature gas-cooled reactor (HTGR), a type of fuel with improved graphite and its gradient protective coating based on silicon carbide (SiC) will be used. So, the purpose of this work is determination the rate and features of the long-term high-temperature corrosion of reactor graphite and its SiC coating at a temperature of 1200K and a pressure of 200-250 kPa in helium with an admixture of water and oxygen in concentrations close to the normal operation of an HTGR; development a numerical model of a corrosion experiment with the convection method of supplying the working mixture. As a result, four successive test stages lasting 30 days each (the total duration of corrosion was 120 days), the weight loss of pure graphite samples (without SiC coating) range from 1.8% to 10.4%, depending on the manufacturer. In general, the average corrosion rate of unprotected graphite corresponds to the literature data. The use of a SiC coating over graphites reduces the corrosion rate of samples by a factor of 100-500. The developed model made it possible to describe both the high-temperature corrosion processes of HTGR graphite and the dynamics of the mass transfer of all gas components throughout the entire volume of the installation during the experiment.
引用
收藏
页码:41 / 52
页数:12
相关论文
共 50 条
  • [21] A multifunctional and long-term waterborne anti-corrosion coating with excellent ?hexagonal warrior? properties
    Pei, Luchao
    Lin, Dan
    Yuan, Sicheng
    Lu, Renjie
    Bai, Ziheng
    Sun, Yue
    Zhu, Yanji
    Jiang, Yuanxu
    Zhu, Jiajun
    Wang, Huaiyuan
    [J]. CHEMICAL ENGINEERING JOURNAL, 2023, 457
  • [22] Long-term stability of Mg/SiC multilayers
    Pelizzo, Maria Guglielmina
    Fineschi, Silvano
    Corso, Alain Jody
    Zuppella, Paola
    Nicolosi, Piergiorgio
    Seely, John
    Kjornrattanawanich, Benjawan
    Windt, David L.
    [J]. OPTICAL ENGINEERING, 2012, 51 (02)
  • [23] Advanced coatings for HTGR fuel particles against corrosion of SiC layer
    Minato, K
    Fukuda, K
    Ishikawa, A
    Mita, N
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1997, 246 (2-3) : 215 - 222
  • [24] REMOVABLE COATING GIVES LONG-TERM PROTECTION
    不详
    [J]. ENGINEERING MATERIALS AND DESIGN, 1977, 21 (02): : 18 - 18
  • [25] TEST OF LONG-TERM CORROSION OF DENTAL AMALGAMS
    DERAND, T
    [J]. SCANDINAVIAN JOURNAL OF DENTAL RESEARCH, 1986, 94 (03): : 253 - 258
  • [26] LONG-TERM INVESTIGATION OF THE CORROSION OF COPPER INUTERO
    KOCH, UJ
    STICHEL, W
    STANGE, J
    [J]. CONTRACEPTIVE DELIVERY SYSTEMS, 1984, 5 (03) : 68 - 68
  • [27] A study on long-term prediction of corrosion wastage
    Matsukura, T.
    Kawamura, Y.
    Khoo, Eeteng
    [J]. ADVANCES IN MARINE STRUCTURES, 2011, : 699 - 705
  • [28] THE LONG-TERM CORROSION OF ALUMINUM IN ALKALINE MEDIA
    TABRIZI, MR
    LYON, SB
    THOMPSON, GE
    FERGUSON, JM
    [J]. CORROSION SCIENCE, 1991, 32 (07) : 733 - 742
  • [29] Long-term corrosion tests with Hanford glasses
    Ebert, WL
    Lewis, MA
    Dietz, NL
    [J]. ENVIRONMENTAL ISSUES AND WASTE MANAGEMENT TECHNOLOGIES IN THE CERAMIC AND NUCLEAR INDUSTRIES VII, 2002, 132 : 279 - 285
  • [30] Long-term atmospheric corrosion of mild steel
    de la Fuente, D.
    Diaz, I.
    Simancas, J.
    Chico, B.
    Morcillo, M.
    [J]. CORROSION SCIENCE, 2011, 53 (02) : 604 - 617