Effect of Minor Addition of Ni and Zr on the High-Temperature Performance of Al-Si-Cu-Mg Cast Alloys

被引:6
|
作者
Hernandez-Sandoval, J. [1 ]
Zedan, Y. [2 ]
Songmene, V [2 ]
Abdelaziz, M. H. [3 ]
Samuel, F. H. [4 ]
Garza-Elizondo, G. H. [4 ]
机构
[1] Univ Autonoma Nuevo Leon, Fac Ingn Mecan & Elect, San Nicolas, Mexico
[2] Ecole Technol Super, Dept Genie Mecan, Montreal, PQ, Canada
[3] Univ Francaise Egypte, Dept PEC, Ville Shorouk, Le Caire, Egypt
[4] UQAC, Dept Sci Appl, Saguenay, PQ, Canada
关键词
aluminum alloys; heat treatment; high-temperature testing; fractography; MECHANICAL-PROPERTIES; FOUNDRY ALLOYS; ALUMINUM; TENSILE; MICROSTRUCTURE; PRECIPITATION; SC; OPTIMIZATION; STRENGTH; BEHAVIOR;
D O I
10.1007/s40962-021-00670-z
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this study, the results pertaining to the influence of various metallurgical parameters on the tensile properties of Al-Si-Cu-Mg 354-type casting alloys are presented. This is discussed with an emphasis on acquiring an insight regarding the mechanical limits of Al-Si-Cu-Mg 354-type alloys in the context of these parameters, and to obtain an understanding of the effects of the addition of nickel and/or zirconium on alloy 354 with respect to the mechanical properties obtained at high temperature (155 degrees C and 300 degrees C for holding times at temperature ranging from 10 to 100 h). Based on an analysis of the results obtained, the following conclusions may be drawn. The results show that additions of Zr and Zr + Ni increase the high-temperature tensile properties, in particular for the alloy containing 0.2 wt% Zr + 0.2 wt% Ni, which exhibits an increase of more than 30% in the tensile properties at 300 degrees C compared with the base 354 alloy. In other words, the addition of 0.4 wt% Ni + 0.4 wt% Zr to the 354 alloy is not sufficient to resist softening at 300 degrees C/100 h (cf. UTS: 52 MPa, YS: 45 MPa, %El: 23% with UTS: 361 MPa, YS: 343 MPa, %El 1.23%, observed after T6 treatment). The addition of 0.4 wt% Ni to alloy 354 leads to a decrease in the tensile properties, compared to the base alloy. This decrease may be attributed to a Ni-Cu reaction which could interfere with the formation of the Al2Cu strengthening precipitates, thereby affecting the age hardening process. As a consequence, percentage elongation increases with the testing temperature, from as-cast to T6-treated samples tested at high temperature (155 degrees C and 300 degrees C, respectively). In summary, the best high-temperature tensile properties are displayed by the alloy containing 0.2 wt% Zr + 0.2 wt% Ni.
引用
收藏
页码:1235 / 1251
页数:17
相关论文
共 50 条
  • [31] Effect of Be on aging behavior of an Al-Si-Cu-Mg cast alloy
    Wang, GQ
    Bian, XF
    Qiao, JG
    Zhang, JY
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2004, 13 (01) : 99 - 102
  • [32] Effect of minor Sc and Zr addition on grain refinement of as-cast Al-Zn-Mg-Cu alloys
    He Yongdong
    Zhang Xinming
    Cao Zhiqiang
    CHINA FOUNDRY, 2009, 6 (03) : 214 - 218
  • [33] Effect of Be on aging behavior of an Al-Si-Cu-Mg cast alloy
    Guiqing Wang
    Xiufang Bian
    Junyan Zhang
    Jinguo Qiao
    Journal of Materials Engineering and Performance, 2004, 13 : 99 - 102
  • [34] Ageing characteristics and high-temperature tensile properties of Al-Si-Cu-Mg alloys with micro-additions of Cr, Ti, V and Zr
    Shaha, S. K.
    Czerwinski, F.
    Kasprzak, W.
    Friedman, J.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 652 : 353 - 364
  • [35] Strengthening precipitates and mechanical performance of Al-Si-Cu-Mg cast alloys containing transition elements
    Abdelaziz, M. H.
    Elgallad, E. M.
    Doty, H. W.
    Samuel, F. H.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 820
  • [36] Ni- and Zr-Based Intermetallics in Al–Si–Cu–Mg Cast Alloys
    Hernandez-Sandoval J.
    Samuel A.M.
    Valtierra S.
    Samuel F.H.
    Metallography, Microstructure, and Analysis, 2014, 3 (5) : 408 - 420
  • [37] Effect of Cd and Sn addition on the microstructure and mechanical properties of Al-Si-Cu-Mg cast alloy
    Li, RD
    Li, RX
    Yu, L
    Hu, ZQ
    14TH CONGRESS OF INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING, VOLS 1 and 2, PROCEEDINGS, 2004, : 113 - 116
  • [38] Dispersoid strengthening of a high temperature Al-Si-Cu-Mg alloy via Mo addition
    Farkoosh, A. R.
    Chen, X. Grant
    Pekguleryuz, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 620 : 181 - 189
  • [39] Effect of Ni and Mn Additions on the Ambient and High-Temperature Performance of Zr-Containing Al–Si–Cu–Mg-Based Alloys: Role of Precipitation Hardening
    Loay Alyaldin
    M. H. Abdelaziz
    Agnes M. Samuel
    Herbert W. Doty
    Salvador Valtierra
    Fawzy H. Samuel
    International Journal of Metalcasting, 2018, 12 : 825 - 838
  • [40] EFFECT OF Ni AND Mn ADDITIONS ON THE AMBIENT AND HIGH-TEMPERATURE PERFORMANCE OF Zr-CONTAINING Al-Si-Cu-Mg-BASED ALLOYS: ROLE OF PRECIPITATION HARDENING
    Alyaldin, Loay
    Abdelaziz, M. H.
    Samuel, Agnes M.
    Samuel, Fawzy H.
    Doty, Herbert W.
    Valtierra, Salvador
    INTERNATIONAL JOURNAL OF METALCASTING, 2018, 12 (04) : 825 - 838