Effects of silica addition on chromium distribution in stainless-steel slag

被引:8
|
作者
Li, Wanli [1 ]
Xue, Xiangxin [1 ,2 ]
机构
[1] Northeastern Univ, Sch Met, Shenyang 110819, Liaoning, Peoples R China
[2] Liaoning Key Lab Met Resources Recycling Sci, Shenyang 110819, Liaoning, Peoples R China
基金
中国国家自然科学基金;
关键词
Silica addition; chromium distribution; spinel; liquid; VISCOSITY; AKERMANITE; PARTITION; CAF2; NA2O; MGO;
D O I
10.1080/03019233.2017.1412386
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The present study was aimed at highlighting the effect of silica on chromium distribution and enrichment in certain stainless-steel slag when basicity ranged from 0.96 to 1.96. Industrial slag samples of the CaO-Al2O3-MgO-SiO2-CrOX-FeXO system were investigated with different silica addition contents and soaked at the targeted regime. X-ray diffraction, electron probe micro-analyzer with wavelength-dispersive X-ray spectrometer, as well as Fourier-transform infrared spectroscopy and NIH ImageJ software were used for sample characterisation. FactSage version 6.4 was employed to calculate phase equilibria at 1200 degrees C for the slag system to understand the crystallisation procedure. Results indicated that chromium was enriched in CaCr2O4 at high basicity, but in spinel at lower basicity. The spinel phase increased in size and chromium distribution with Fe(II) participated in growth with the decrease in depolymerisation of the slag structure.
引用
收藏
页码:929 / 936
页数:8
相关论文
共 50 条
  • [31] CHROMIUM DEPLETION OF VACUUM ANNEALED STAINLESS-STEEL SURFACES
    PARK, RL
    SCHREINER, DG
    HOUSTON, JE
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1972, 9 (02): : 1023 - +
  • [32] DECARBURIZATION OF MOLTEN CHROMIUM STAINLESS-STEEL IN MEDIUM VACUUM
    NOSOV, YN
    NEIGEBAUER, GO
    LEVIN, AM
    SALNIKOV, AG
    DMITRIENKO, VI
    KUTAKOV, AV
    [J]. STEEL IN THE USSR, 1978, 8 (02): : 85 - 88
  • [33] NEW HIGH-CHROMIUM FERRITIC STAINLESS-STEEL
    PINNOW, KE
    BRESSANELLI, JP
    MOSKOWITZ, A
    [J]. METALS ENGINEERING QUARTERLY, 1975, 15 (03): : 32 - 41
  • [34] ELIMINATION OF CHROMIUM IN URINE AFTER STAINLESS-STEEL WELDING
    WELINDER, H
    LITTORIN, M
    GULLBERG, B
    SKERFVING, S
    [J]. SCANDINAVIAN JOURNAL OF WORK ENVIRONMENT & HEALTH, 1983, 9 (05) : 397 - 403
  • [35] HIGH ALUMINUM, LOW CHROMIUM AUSTENITIC STAINLESS-STEEL
    MCGURTY, JA
    NEKKANTI, R
    MOTEFF, J
    [J]. JOURNAL OF METALS, 1986, 38 (05): : 22 - 25
  • [36] CHROMIUM - REVIVAL IN STAINLESS-STEEL BOLSTERS DEMAND FOR FECR
    SMITH, WE
    [J]. E&MJ-ENGINEERING AND MINING JOURNAL, 1984, 185 (03): : 53 - 54
  • [37] Stability of Chromium in Stainless Steel Slag during Cooling
    Zhao, Qing
    Liu, Chengjun
    Cao, Longhu
    Zheng, Xiang
    Jiang, Maofa
    [J]. MINERALS, 2018, 8 (10):
  • [38] Effect of Lime on Stability of Chromium in Stainless Steel Slag
    Zhao, Qing
    Liu, Chengjun
    Cao, Longhu
    Zheng, Xiang
    Jiang, Maofa
    [J]. MINERALS, 2018, 8 (10):
  • [39] THE EFFECTS OF LEACHING ON THE MINERAL PHASES IN ARGON-OXYGEN DECARBURIZATION OF STAINLESS-STEEL SLAG
    Wang, Ya-Jun
    Zeng, Ya-Nan
    Li, Jun-Guo
    [J]. MATERIALI IN TEHNOLOGIJE, 2020, 54 (03): : 293 - 300
  • [40] Processing fine stainless-steel slag using spiral concentration
    Wolfe, Eric R.
    Klima, Mark S.
    [J]. JOURNAL OF ENVIRONMENTAL SCIENCE AND HEALTH PART A-TOXIC/HAZARDOUS SUBSTANCES & ENVIRONMENTAL ENGINEERING, 2008, 43 (05): : 495 - 502