Fracture Mechanics Based Analysis of the Fatigue Life of Defective Welded Joints

被引:1
|
作者
Gajdos, Lubomir [1 ]
Sperl, Martin [1 ]
机构
[1] Czech Acad Sci, Inst Theoret & Appl Mech, Prosecka 76, Prague 19000 9, Czech Republic
关键词
welded structures; weld discontinuities; arc welding; carbon manganese steel; fatigue; stress intensity factor; STEEL; ALLOY;
D O I
10.2320/matertrans.MT-M2019258
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work was motivated by the endeavour to experimentally determine the influence of crack position on the fatigue life of weldments. Plates were cut from a pipe of X52 pipeline steel - 830mm in diameter and 10mm in wall thickness - and their contact edges were then prepared for single-bevel butt welds. The plates were then welded by manual arc welding, and separate specimens - 10mm in width and 5mm in thickness - were cut from the weldment perpendicularly to the weld bead. The electro-spark method was then used to produce blunt crack discontinuities for the initiation of fatigue cracks. The cracked weldment specimens then underwent cyclic loading at reference force level F-max = 5.5kN and stress asymmetry ratio R = F-min/F-max = 0.1. The test results made it possible to quantify the effects of the size and position of crack-like discontinuities on weld fatigue life.
引用
收藏
页码:926 / 934
页数:9
相关论文
共 50 条