Chi Phase after Short-term Aging and Corrosion Behavior in 2205 Duplex Stainless Steel

被引:21
|
作者
Sun, Qi [1 ,2 ]
Wang, Jian [1 ,2 ]
Li, Hua-bing [3 ]
Li, Yue [1 ,2 ]
Hu, Ya-di [1 ,2 ]
Bai, Jin gang [4 ]
de Han, Pei [1 ,2 ]
机构
[1] Taiyuan Univ Technol, Coll Mat Sci & Engn, Taiyuan 030021, Shanxi, Peoples R China
[2] Taiyuan Univ Technol, Key Lab Interface Sci & Engn Adv Mat, Taiyuan 030021, Shanxi, Peoples R China
[3] Northeastern Univ, Sch Met, Shenyang 110819, Liaoning, Peoples R China
[4] Technol Ctr Taiyuan Iron & Steel Grp Co Ltd, Taiyuan 030003, Shanxi, Peoples R China
基金
中国国家自然科学基金; 高等学校博士学科点专项科研基金;
关键词
duplex stainless steel; short-term aging; chi phase; pitting corrosion; selective corrosion; grain size; SIGMA-PHASE; DELETERIOUS PHASES; PRECIPITATION; TRANSFORMATION; RESISTANCE;
D O I
10.1016/S1006-706X(16)30159-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Correlation between pitting corrosion behavior and chi (chi) phase formed after a short-term aging (5, 10 and 15 min) at 850 degrees C of 2205 duplex stainless steel (DSS) was investigated using potentiodynamic polarization tests, optical microscopy, and scanning electron microscopy equipped with energy-dispersive spectrum system. Results showed that after aging for 5 min, the chi phase initially precipitated at ferrite grain boundaries, developed and then became linked with prolonging aging time. The chi phase was rich in Cr and Mo, resulting in formation of depleted zones nearby. The chi phase could reduce corrosion resistance of DSS and slightly influence its stability, but the specimens still displayed the capacity for repassivation. Some lines of evidence showed that stable pitting corrosion initiated at the boundaries of precipitates. The chi phase was selectively corroded during the first stage of corrosion and then the depleted zones nearby were attacked. In addition, the grain size and volume of precipitates also affected pit nucleation and progress, and suitable size and distribution of chi phase could aggravate pit initiation at precipitate boundaries. The chi phase with considerably low volume fraction and small size was not sensitive position for pit initiation.
引用
收藏
页码:1071 / 1079
页数:9
相关论文
共 50 条
  • [41] Effect of Ag Doping in 2205 Duplex Stainless Steel on Corrosion Resistance
    Lin, Dong-Yih
    Yang, Sheng-Min
    Chou, Yong-Chih
    Fang, Yi-Ya
    Wang, Huei-Sen
    MECHANICAL AND AEROSPACE ENGINEERING, PTS 1-7, 2012, 110-116 : 1207 - +
  • [42] Microstructural and electrochemical behavior of 2205 duplex stainless steel weldments
    Makhdoom, M. Atif
    Ahmad, A.
    Kamran, M.
    Abid, K.
    Haider, W.
    SURFACES AND INTERFACES, 2017, 9 : 189 - 195
  • [43] Effect of cold working and isothermal aging on the precipitation of sigma phase in 2205 duplex stainless steel
    Cho, Noon-Sung
    Lee, Kwangmin
    MATERIALS CHARACTERIZATION, 2013, 75 : 29 - 34
  • [44] The low-temperature aging embrittlement in a 2205 duplex stainless steel
    Weng, KL
    Chen, HR
    Yang, JR
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 379 (1-2): : 119 - 132
  • [45] Analysis of χ Phase Precipitation in Aged 2205 Duplex Stainless Steel
    刘和平
    SUN Huer
    LIU Bin
    LI Dazhao
    SUN Fenger
    ZHANG Yongtao
    Journal of Wuhan University of Technology(Materials Science Edition), 2015, 30 (03) : 591 - 595
  • [46] Analysis of χ phase precipitation in aged 2205 duplex stainless steel
    Heping Liu
    Hu’er Sun
    Bin Liu
    Dazhao Li
    Fenger Sun
    Yongtao Zhang
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2015, 30 : 591 - 595
  • [47] Analysis of χ Phase Precipitation in Aged 2205 Duplex Stainless Steel
    Liu Heping
    Sun Hu'er
    Liu Bin
    Li Dazhao
    Sun Fenger
    Zhang Yongtao
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2015, 30 (03): : 591 - 595
  • [48] Analysis of χ Phase Precipitation in Aged 2205 Duplex Stainless Steel
    刘和平
    SUN Hu'er
    LIU Bin
    LI Dazhao
    SUN Fenger
    ZHANG Yongtao
    Journal of Wuhan University of Technology(Materials Science), 2015, (03) : 591 - 595
  • [49] Chi-phase precipitation in a duplex stainless steel
    Escriba, D. M.
    Materna-Morris, E.
    Plaut, R. L.
    Padilha, A. F.
    MATERIALS CHARACTERIZATION, 2009, 60 (11) : 1214 - 1219
  • [50] EFFECT OF AGING TIME ON ELECTROCHEMICAL CORROSION BEHAVIOR OF 2101 DUPLEX STAINLESS STEEL
    Han Dong
    Jiang Yiming
    Deng Bo
    Zhang Lihua
    Zhang Wei
    Li Jin
    ACTA METALLURGICA SINICA, 2009, 45 (08) : 919 - 923