Evolution of corrosion behavior for AA7075 aluminum alloy implanted with nitrogen

被引:9
|
作者
Abreu, C. M. [1 ]
Cristobal, M. J. [1 ]
Figueroa, R. [1 ]
Novoa, X. R. [2 ]
Pena, G. [1 ]
机构
[1] Univ Vigo, ENCOMAT Grp, Dept Mat Engn Appl Mech & Construct, Vigo 36310, Spain
[2] Univ Vigo, ENCOMAT Grp, Dept Chem Engn, Vigo 36310, Spain
关键词
Aluminum alloys; Ion implantation; Electrochemical impedance spectroscopy; Potentiodynamic polarization; Intergranular corrosion; Pitting corrosion; ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY; ION-IMPLANTATION; DIFFERENT TEMPERS; LOCALIZED CORROSION; AL; 2024-T3; DEGRADATION; INHIBITION; RESISTANCE; SYSTEMS;
D O I
10.1016/j.nimb.2019.01.013
中图分类号
TH7 [仪器、仪表];
学科分类号
0804 ; 080401 ; 081102 ;
摘要
This work reports the corrosion behavior of the AA7075 aluminum alloy under two different tempers (T6 and 173) after nitrogen implantation in 0.5 mol center dot L-1 NaCl solution. A combination of Electrochemical Impedance Spectroscopy and surface microstructure characterization was used to analyze the effects of nitrogen implantation on corrosion resistance. Nitrogen implantation, at 2 x 10(17) N+ ions center dot cm(-2) and 50 keV energy, induces the formation of AlN layer improving the corrosion resistance of aluminum alloys as evidenced by initial corrosion tests and a less corroded area. The evolution of the impedance indicates that the corrosion improvement vanishes over time. Implanted and unimplanted alloys show similar electrochemical parameters after 20 h immersion. However, microscopic examination shows less corrosion damage for implanted alloys after 72 h of immersion. These findings suggest that the implantation only delays the onset of corrosion probably due to degradation of AlN layer in aqueous medium. The corrosion resistance at long periods only depends on the aging heat treatment applied to the AA7075 aluminum alloy and the effect of implantation is negligible.
引用
收藏
页码:1 / 12
页数:12
相关论文
共 50 条
  • [21] Dynamic response of AA7075 aluminum alloy as a function of temperature
    Jin, Z
    Cassada, WA
    Cady, C
    Gray, GT
    HOT DEFORMATION OF ALUMINUM ALLOYS III, 2003, : 247 - 254
  • [22] Corrosion Protection Performance of YSZ Coating on AA7075 Aluminum Alloy Prepared by Aerosol Deposition
    Ryu, Hyun Sam
    Lim, Tae Seop
    Ryu, Jungho
    Hong, Seong-Hyeon
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2013, 160 (01) : C42 - C47
  • [23] The effect of chloride concentration and pH on pitting corrosion of AA7075 aluminum alloy coated with phenyltrimethoxysilane
    Younis, A. A.
    El-Sabbah, M. M. B.
    Holze, Rudolf
    JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2012, 16 (03) : 1033 - 1040
  • [24] Influence of nitrogen implantation on the localized corrosion resistance of different tempers of AA7075 aluminium alloy
    Abreu, C. M.
    Cristobal, M. J.
    Figueroa, R.
    Pena, G.
    Perez, M. C.
    SURFACE AND INTERFACE ANALYSIS, 2010, 42 (6-7) : 636 - 640
  • [25] Hot Deformation Behavior of Aluminum Alloys AA7010 and AA7075
    Gupta, R. K.
    Kumar, V. Anil
    Krishnan, A. Sarath
    Niteshraj, J.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (08) : 5021 - 5036
  • [26] Hot Deformation Behavior of Aluminum Alloys AA7010 and AA7075
    R. K. Gupta
    V. Anil Kumar
    A. Sarath Krishnan
    J. Niteshraj
    Journal of Materials Engineering and Performance, 2019, 28 : 5021 - 5036
  • [27] Stress Corrosion Cracking of AA7075 Aluminum Alloy Processed via Additive Friction Stir Deposition
    Acquah, Ebenezer
    Bhowmik, Shubhrodev
    Hossain, A. F. M. Monowar
    Kumar, Nilesh
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [28] Chemically synthesized polyaniline/polyvinyl chloride blended coatings for the corrosion protection of AA7075 aluminum alloy
    Bandeira, Rafael Marinho
    van Drunen, Julia
    de Souza Ferreira, Fabio Augusto
    Rodrigues-Filho, Ubirajara Pereira
    Tremiliosi-Filho, Germano
    CORROSION SCIENCE, 2018, 139 : 35 - 46
  • [29] Cerium citrate as ecologically friendly corrosion inhibitor for AA7075 alloy
    Marunkic, Dunja
    Pejic, Jovanka
    Jegdic, Bore
    Marinkovic, Aleksandar
    Radojkovic, Bojana
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2022, 73 (06): : 950 - 960
  • [30] Cerium citrate as ecologically friendly corrosion inhibitor for AA7075 alloy
    Marunkić, Dunja
    Pejić, Jovanka
    Jegdić, Bore
    Marinković, Aleksandar
    Radojković, Bojana
    Materials and Corrosion, 2022, 73 (06) : 950 - 960