The low temperature oxidation of lithium thin films on HOPG by O2 and H2O

被引:3
|
作者
Wulfsberg, Steven M. [1 ]
Koel, Bruce E. [2 ]
Bernasek, Steven L. [1 ]
机构
[1] Princeton Univ, Dept Chem, Princeton, NJ 08544 USA
[2] Princeton Univ, Dept Chem & Biol Engn, Princeton, NJ 08544 USA
关键词
Lithium thin films; Oxidation; Adsorption; Lithiated graphite; METAL-COMPLEXES; AUGER-SPECTRA; ADSORPTION; CHARACTER; GRAPHITE;
D O I
10.1016/j.susc.2016.04.003
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Lithiated graphite and lithium thin films have been used in fusion devices. In this environment, lithiated graphite will undergo oxidation by background gases. In order to gain insight into this oxidation process, thin (<15 monolayer (ML)) lithium films on highly ordered pyrolytic graphite (HOPG) were exposed to O-2(g) and H2O(g) in an ultra-high vacuum chamber. High resolution electron energy loss spectroscopy (HREELS) was used to identify the surface species formed during O-2(g) and H2O(g) exposure. Auger electron spectroscopy (AES) was used to obtain the relative oxidation rates during O-2(g) and H2O(g) exposure. AES showed that as the lithium film thickness decreased from 15 to 5 to 1 ML, the oxidation rate decreased for both O-2(g) and H2O(g). HREELS showed that a 15 ML lithium film was fully oxidized after 9.7 L (L) of O-2(g) exposure and Li2O was formed. HREELS also showed that during initial exposure (<0.5 L) H2O(g), lithium hydride and lithium hydroxide were formed on the surface of a 15 ML lithium film. After 0.5 L of H2O(g) exposure, the H2O(g) began to physisorb, and after 15 L of H2O(g) exposure, the 15 ML lithium film was not fully oxidized. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:120 / 127
页数:8
相关论文
共 50 条
  • [1] Reprint of “The low temperature oxidation of lithium thin films on HOPG by O2 and H2O”
    Wulfsberg S.M.
    Koel B.E.
    Bernasek S.L.
    Bernasek, Steven L. (sberna@princeton.edu), 2016, Elsevier B.V., Netherlands (652) : 222 - 229
  • [2] The low temperature oxidation of lithium thin films on HOPG by O2 and H2O (Reprinted from Surface Science, vol 651, pg 120-127, 2016)
    Wulfsberg, Steven M.
    Koel, Bruce E.
    Bernasek, Steven L.
    SURFACE SCIENCE, 2016, 652 : 222 - 229
  • [3] Passivation of iron by oxidation in H2O and O2/H2O mixtures
    Roosendaal, SJ
    Bakker, JPR
    Vredenberg, AM
    Habraken, FHPM
    SURFACE SCIENCE, 2001, 494 (03) : 197 - 205
  • [4] OXIDATION OF IRON BY O2, H2O, AND AN O2-H2O MIXTURE
    TURNER, NH
    COLTON, RJ
    MURDAY, JS
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1981, 18 (02): : 593 - 594
  • [5] SURFACE COMPLEXES BETWEEN O2, H2O AND LITHIUM
    MCLEAN, W
    SCHULTZ, JA
    PEDERSEN, LG
    JARNAGIN, RC
    SURFACE SCIENCE, 1979, 83 (02) : 354 - 366
  • [6] INVESTIGATION OF EFFECT OF O2 N2 AND H2O ON NICKEL THIN FILMS
    FREEDMAN, JF
    JOURNAL OF APPLIED PHYSICS, 1965, 36 (3P2) : 964 - &
  • [7] Properties of Al2O3 Thin Films Grown by PE-ALD at Low Temperature Using H2O and O2 Plasma Oxidants
    Castillo-Saenz, Jhonathan
    Nedev, Nicola
    Valdez-Salas, Benjamin
    Curiel-Alvarez, Mario
    Isabel Mendivil-Palma, Maria
    Hernandez-Como, Norberto
    Martinez-Puente, Marcelo
    Mateos, David
    Perez-Landeros, Oscar
    Martinez-Guerra, Eduardo
    COATINGS, 2021, 11 (10)
  • [8] COMPARISON OF INSITU LOW-PRESSURE OXIDATION OF PURE IRON AT ROOM-TEMPERATURE IN O2 AND IN O2/H2O MIXTURES USING XPS
    STAMBOULI, V
    PALACIO, C
    MATHIEU, HJ
    LANDOLT, D
    APPLIED SURFACE SCIENCE, 1993, 70-1 : 240 - 244
  • [9] Oxidation of HIPed TiC ceramics in dry O2, wet O2, and H2O atmospheres
    Shimada, S
    Onuma, T
    Kiyono, H
    Desmaison, M
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2006, 89 (04) : 1218 - 1225
  • [10] Corrosion Behaviors of Ni–Cr Alloys in O2, H2O and H2O + O2 Gases at 700°C and the Effect of Temperature
    Jiarui Chen
    Chengyang Jiang
    Jianqiang Zhang
    High Temperature Corrosion of Materials, 2023, 100 : 775 - 789