Study of buckling behavior for 7A04-T6 aluminum alloy rectangular hollow columns

被引:30
|
作者
Hu, Yaowei [1 ]
Rong, Bin [1 ,2 ]
Zhang, Ruoyu [1 ]
Zhang, Yichun [1 ]
Zhang, Song [1 ]
机构
[1] Tianjin Univ, Sch Civil Engn, Tianjin 300072, Peoples R China
[2] Tianjin Univ, Key Lab Coast Civil Struct & Safety, Minist Educ, Tianjin 300072, Peoples R China
关键词
Eccentric load; Initial geometric imperfection; Ultimate strength; Finite element analysis; Design formula; PARAMETRIC ANALYSIS; STRENGTH; DESIGN; MEMBERS;
D O I
10.1016/j.tws.2021.108410
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
A series of eccentric load tests on aluminum alloy columns with square and rectangular hollow sections, fabricated by extrusion using 7A04-T6 aluminum alloy, were conducted in this paper. The initial geometric imperfections were measured prior to compression tests to investigate their impact on ultimate strength. The relevant load-displacement and load-strain curves acquired from testing reacted to the buckling behavior of columns subjected to combined axial load and bending, and the failure modes observed included overall buckling and the combination of local and overall buckling. Finite element models were developed and validated in conjunction with the experimental conditions and results. Then, an expanded parametric study was performed to explore the effect of the stability performance for columns over a wide range of normalized slenderness ratios and load eccentricity ratios. The experimental and numerical results were compared to the design strength provided by the current Chinese code, European code, American specification, and the Australian/New Zealand standard, as well as optional design approaches, the direct strength method and continuous strength method. The comparisons revealed that the majority of the current design provisions and methods presented relatively conservative predictions of ultimate strength for 7A04-T6 aluminum alloy columns under combined loading. A formula based on the Chinese code was proposed, with several parameters modified, to more accurately predict the ultimate strength of 7A04-T6 aluminum alloy columns.
引用
收藏
页数:17
相关论文
共 50 条
  • [21] Effects of Multiple Plastic Deformations on Microstructure and Mechanical Properties of 7A04-T6
    Zhang Zhimin
    Yu Jianmin
    Wang Qiang
    Zhang Xing
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 69 - 72
  • [22] Constitutive modeling on cyclic stress-strain behaviour of 7A04-T6 high-strength aluminium alloy
    Li, Beibei
    Hai, Letian
    Wang, Yuanqing
    Ban, Huiyong
    Hu, Zhihan
    Wang, Zhongxing
    STRUCTURES, 2024, 64
  • [23] Mechanical properties of 7A04-T6 high strength structural aluminium alloy at elevated temperatures and after cooling down
    Wang, Zhongxing
    Ma, Chunyin
    Li, Mengyu
    Han, Qinghua
    Li, Hai-Ting
    Zhao, Dongdong
    THIN-WALLED STRUCTURES, 2022, 180
  • [24] Experimental study on the hysteretic behavior of aluminum alloy gusset joint with rectangular hollow sections
    Wu, Mingze
    Fan, Shenggang
    Zhao, Ziwei
    Liu, Meijing
    Hu, Lizhi
    Yu, Tao
    THIN-WALLED STRUCTURES, 2024, 196
  • [25] Experimental Study on Local Buckling Behavior of 7075-T6 High-Strength Aluminum Alloy Stub Columns Under Axial Compression
    Zhi X.
    Wang Y.
    Li B.
    Zhang Y.
    Fan S.
    Ouyang Y.
    Tianjin Daxue Xuebao (Ziran Kexue yu Gongcheng Jishu Ban)/Journal of Tianjin University Science and Technology, 2022, 55 (07): : 745 - 753
  • [26] 7A04-T6铝合金圆管柱抗震性能研究
    丁永君
    周毅
    李进军
    荣彬
    建筑技术, 2022, 53 (02) : 246 - 249
  • [27] 7A04-T6铝合金棒材生产工艺研究
    林光磊
    轻合金加工技术, 2007, (11) : 33 - 35+57
  • [28] Flexural behaviour of 7A04-T6 high-strength aluminium alloy SHS and RHS beams under moment gradient
    Li, Beibei
    Wang, Yuanqing
    Zhang, Ying
    Yuan, Huanxin
    Zhi, Xinhang
    Baniotopoulos, Charalampos C.
    ENGINEERING STRUCTURES, 2022, 259
  • [29] Stability of 6082-T6 aluminium alloy columns with H-section and rectangular hollow sections
    Adeoti, Guy Oyeniran
    Fan, Feng
    Wang, Yujin
    Zhai, Ximei
    THIN-WALLED STRUCTURES, 2015, 89 : 1 - 16
  • [30] 7A04-T6铝合金中性盐雾腐蚀初期性能
    徐宏妍
    第五江涛
    李智勇
    杨亚琴
    材料保护, 2014, 47 (08) : 40 - 42+7