Pilot Evaluation of Four Experimental Conditioning Treatments to Improve the Bond Strength between Resin Cement and Y-TZP Ceramic

被引:34
|
作者
Monaco, Carlo [2 ]
Cardelli, Paolo [2 ]
Scotti, Roberto [2 ]
Valandro, Luiz Felipe [1 ]
机构
[1] Univ Fed Santa Maria, Sch Dent, Dept Restorat Dent, Div Prosthodont, BR-97015372 Santa Maria, RS, Brazil
[2] Univ Bologna, Div Prosthodont, Dept Oral Sci, I-40126 Bologna, Italy
关键词
Y-TZP ceramic; surface conditioning; tribochemical silica coating; FIXED PARTIAL DENTURES; SURFACE-TREATMENT; DENTAL CERAMICS; AGED CONDITIONS; LUTING CEMENTS; ZIRCONIA; SHEAR; MICROTENSILE; ADHESION; AGENTS;
D O I
10.1111/j.1532-849X.2010.00677.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: This study evaluated the bond strength between resin cement and Y-TZP ceramic (Yttrium-stabilized Tetragonal Zirconia Polycrystalline) submitted to different surface conditionings. Materials and Methods: Fifty Y-TZP ceramic discs (empty set = 10 mm) were allocated into five groups: Gr1 (control)-no conditioning; Gr2-tribochemical silica coating (30-mu mSiO(2)) before sintering; Gr3-air abrasion with 50-mu m Al(2)O(3) before sintering; Gr4-air abrasion with 110-mu Al(2)O(3) before sintering; Gr5 - air abrasion with 50-mu m Al(2)O(3) after sintering. After specimen preparation, cylinders of composite resin were prepared and immediately cemented onto the ceramic. A shear test was performed. Results: One-way ANOVA indicated a statistically significant difference among the groups (p = 0.0019). The mean shear bond strengths (MPa) were: Gr1 = 4.7 +/- 0.8,(b) Gr2 = 4.6 +/- 0.9,(b) Gr3 = 6.4 +/- 1.0,(a) Gr4 = 6.5 +/- 1.8,(a) Gr5 = 6 +/- 1.3(ab) (same superscript letter indicates statistical similarity). Adhesive fracture between the ceramic and resin cement was the most common failure. No complete cohesive fracture at the ceramic or composite cylinders was noted. Conclusion: Within the limitations of this study, additional surface treatment with air abrasion before and after sintering provided a significant increase in bond strength. Tribochemical silica coating before sintering was not effective as a surface treatment.
引用
收藏
页码:97 / 100
页数:4
相关论文
共 50 条
  • [21] Effect of surface topography and wettability on shear bond strength of Y-TZP ceramic
    Wongsue, Suriyakul
    Thanatvarakorn, Ornnicha
    Prasansuttiporn, Taweesak
    Nimmanpipug, Piyarat
    Sastraruji, Thanapat
    Hosaka, Keiichi
    Foxton, Richard M.
    Nakajima, Masatoshi
    SCIENTIFIC REPORTS, 2023, 13 (01)
  • [22] A critical evaluation of bond strength tests for the assessment of bonding to Y-TZP
    Otani, Aline
    Amaral, Marina
    May, Liliana G.
    Cesar, Paulo F.
    Valandro, Luiz Felipe
    DENTAL MATERIALS, 2015, 31 (06) : 648 - 656
  • [23] The effect of a zirconia primer on the shear bond strength of Y-TZP ceramic to three different core materials by using a self-adhesive resin cement
    Giti, Rashin
    Zarkari, Reza
    JOURNAL OF INDIAN PROSTHODONTIC SOCIETY, 2019, 19 (02): : 134 - 140
  • [24] Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only
    Ozcan, Mutlu
    Kerkdijk, Sandra
    Valandro, Luiz Felipe
    CLINICAL ORAL INVESTIGATIONS, 2008, 12 (03) : 279 - 282
  • [25] The influence of Y-TZP surface treatment on topography and ceramic/resin cement interfacial fracture toughness
    Paes, P. N. G.
    Bastian, F. L.
    Jardim, P. M.
    DENTAL MATERIALS, 2017, 33 (09) : 976 - 989
  • [26] Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers’ instructions of the cements only
    Mutlu Özcan
    Sandra Kerkdijk
    Luiz Felipe Valandro
    Clinical Oral Investigations, 2008, 12 : 279 - 282
  • [27] In vitro shear bond strength of Y-TZP ceramics to different core materials with the use of three primer/resin cement systems
    Al-Harbi, Fahad A.
    Ayad, Neveen M.
    Khan, Zahid A.
    Mahrous, Amr A.
    Morgano, Steven M.
    JOURNAL OF PROSTHETIC DENTISTRY, 2016, 115 (01): : 84 - 89
  • [28] Early bond strength of two resin cements to Y-TZP ceramic using MPS or MPS/4-META silanes
    Mutlu Özcan
    Cenk Cura
    Luiz Felipe Valandro
    Odontology, 2011, 99 : 62 - 67
  • [29] Effect of Surface and Heat Treatments on the Biaxial Flexural Strength and Phase Transformation of a Y-TZP Ceramic
    Fonseca, Renata Garcia
    Abi-Rached, Filipe de Oliveira
    Correia Pereira da Silva, Filipe Samuel
    Pacheco de Castro Henriques, Bruno Alexandre
    Pereira Pinelli, Ligia Antunes
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (05): : 451 - 458
  • [30] Early bond strength of two resin cements to Y-TZP ceramic using MPS or MPS/4-META silanes
    Oezcan, Mutlu
    Cura, Cenk
    Valandro, Luiz Felipe
    ODONTOLOGY, 2011, 99 (01) : 62 - 67