Investigation on the alloy phases in as-aged ZK60 magnesium alloy

被引:8
|
作者
Pan, FS [1 ]
Wang, WM
Ma, YL
Zuo, RL
Tang, AT
Zhang, J
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400044, Peoples R China
[2] Chongqing Univ, Chongqing Engn Res Ctr Magnesium Alloys, Chongqing 400044, Peoples R China
关键词
wrought magnesium alloy; aging treatment; alloy phase; precipitates;
D O I
10.4028/www.scientific.net/MSF.488-489.181
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Alloy phases in the as-aged (T6) ZK60 magnesium alloy were investigated. More attentions were paid to types and morphologies of main alloy phases in the as-aged ZK60 magnesium alloy. The experimental results indicated that there was an abundant flower-shaped segregation in the solution-treated ZK60 magnesium alloy. A small quantity of undissolved compounds, MgZn2, was also found. They distributed irregularly in the form of similar parallelogram, with a dimension of 200nm-500nm and not sensitive to heat-treatment. Mg2Zn3 was found to be a main secondary compound in the as-aged ZK60 alloy, which precipitated during aging. Another precipitation phase, MgZn, in the as-aged ZK60 magnesium alloy was also found in the form of long and thin rods with a dimension of 500nm.
引用
收藏
页码:181 / 184
页数:4
相关论文
共 50 条
  • [31] Materials processing for structural stability in a ZK60 magnesium alloy
    Watanabe, H
    Moriwaki, K
    Mukai, T
    Ohsuna, T
    Hiraga, K
    Higashi, K
    MATERIALS TRANSACTIONS, 2003, 44 (04) : 775 - 781
  • [32] Processing maps for hot working of ZK60 magnesium alloy
    Wang, C. Y.
    Wang, X. J.
    Chang, H.
    Wu, K.
    Zheng, M. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 464 (1-2): : 52 - 58
  • [33] Role of second phases and grain boundaries on dynamic recrystallization behavior in ZK60 magnesium alloy
    Peng, Peng
    Zhang, Kunmin
    She, Jia
    Tang, Aitao
    Zhang, Jianyue
    Song, Kai
    Yang, Qingshan
    Pan, Fusheng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 861
  • [34] Microstructure evolution within adiabatic shear band in peak aged ZK60 magnesium alloy
    Jiang, Lihong
    Yang, Yang
    Wang, Zhen
    Hu, Haibo
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 711 : 317 - 324
  • [35] Forming limit diagram of magnesium alloy ZK60 at elevated temperature
    Liu, Hongwei
    Yao, Shengjie
    Liu, Wenliang
    Zhang, Zhaoduo
    ADVANCED DESIGN TECHNOLOGY, PTS 1-3, 2011, 308-310 : 2442 - +
  • [36] Influence of impurities on microstructure and mechanical properties of ZK60 magnesium alloy
    潘复生
    毛建军
    陈先华
    彭建
    王敬丰
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20 (07) : 1299 - 1304
  • [37] Correlation of plastic deformation and dynamic recrystallization in magnesium alloy Zk60
    Galiyev, A
    Kaibyshev, R
    Gottstein, G
    ACTA MATERIALIA, 2001, 49 (07) : 1199 - 1207
  • [38] Thermal simulation on hot deformation behavior of ZK60 magnesium alloy
    School of Materials Science and Engineering, Central South University, Changsha 410083, China
    Cailiao Gongcheng, 2009, 11 (45-50):
  • [39] Microstructure and Corrosion of Cast Magnesium Alloy ZK60 in NaCl Solution
    Li, Zhen
    Peng, Zeyin
    Qi, Kai
    Li, Hui
    Qiu, Yubing
    Guo, Xingpeng
    MATERIALS, 2020, 13 (17)
  • [40] Plastic deformation behavior of ZK60 magnesium alloy with addition of neodymium
    余琨
    王晓艳
    芮守泰
    王日初
    Journal of Central South University of Technology, 2008, (04) : 434 - 437