The fracture resistance of a ferritic-austenitic duplex steel

被引:14
|
作者
Kolednik, O
Albrecht, M
Berchthaler, M
Germ, H
Pippan, R
Riemelmoser, F
Stampfl, J
Wei, J
机构
[1] Erich-Schmid-Inst. Festkorperphysik, Osterreichischen Akad. der Wiss., A-8700 Leoben
[2] Department of Modern Mechanics, Univ. of Sci. and Technol. of China, Hefei
关键词
D O I
10.1016/1359-6454(95)00412-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
For a nitrogen alloyed ferritic-austenitic duplex steel X3CrMnNiMoN 25 6 4 the crack growth resistance is recorded in terms of the J-integral, J, and the energy dissipation rate, D. Due to the anisotropic microstructure of elongated ferrite and austenite domains, very different resistance curves appear for three different crack plane orientations. Metallographic and stereophotogrammetric studies lead to a model which is able to explain these curves. It is found that the geometrical arrangement of the (brittle) ferrite and the (ductile) austenite domains is the main influence factor on the crack growth resistance (and not the volumetric fraction of ferrite and austenite). Since no standard J(IC)-values can be determined, a procedure is proposed to evaluate an alternative measure of the fracture initiation toughness, i.e. ''quasi-initiation'' J-integral values. Copyright (C) 1996 Acta Metallurgica Inc.
引用
收藏
页码:3307 / 3319
页数:13
相关论文
共 50 条
  • [21] CHARACTERISTICS OF LOW NICKEL FERRITIC-AUSTENITIC CORROSION RESISTANT CAST STEEL
    Kalandyk, B.
    Zapala, R.
    Sobula, S.
    Gorny, M.
    Boron, L.
    [J]. METALURGIJA, 2014, 53 (04): : 613 - 616
  • [22] PROPERTIES OF THE FERRITIC-AUSTENITIC STEEL X-3-CRMNNIMON 2564
    KOREN, M
    HOCHORTLER, G
    [J]. STAHL UND EISEN, 1982, 102 (10): : 509 - 513
  • [23] ALPHA-REVERSIBLE-GAMMA TRANSFORMATIONS AND STRUCTURE OF FERRITIC-AUSTENITIC STEEL
    BERNSHTEIN, ML
    KAPUTKINA, LM
    DOBATKIN, SB
    TIKHOMIROVA, OY
    PAKHOMOVA, MY
    [J]. RUSSIAN METALLURGY, 1988, (06): : 39 - 43
  • [24] Effect of nitrided layer on ferritic-austenitic steel on hydrogen absorption and desorption
    Zakroczymski, Tadeusz
    Maminska, Karolina
    [J]. OCHRONA PRZED KOROZJA, 2009, 52 (11): : 564 - 566
  • [25] INTER-CRYSTALLINE CORROSION AND PRECIPITATION BEHAVIOR OF A FERRITIC-AUSTENITIC STEEL
    SCHUSTER, C
    SERCHEN, R
    ECKSTEIN, HJ
    [J]. NEUE HUTTE, 1978, 23 (01): : 16 - 22
  • [26] Deformation and Recrystallization of Acid-resistant Ferritic-Austenitic Steel.
    Blicharski, Marek
    [J]. Hutnik Warszawa, 1984, 51 (7-8): : 258 - 266
  • [27] The effect of sigma-phase precipitation on the corrosion resistance of ferritic-austenitic duplex steels in an REA-pump impeller
    Storz, O
    Pohl, M
    [J]. PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2004, 41 (12): : 627 - 634
  • [28] Improvement of toughness of high chromium white cast iron: duplex ferritic-austenitic matrix
    Jena, P. S. M.
    Rai, Rajesh Kumar
    Sahu, J. K.
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (03) : 299 - 304
  • [29] Liquid, gaseous and plasma nitrocarburizing using three stainless steels types (austenitic, ferritic and duplex ferritic-austenitic) as a substrate: a comparative study
    Netto, EBD
    Kliauga, AM
    Plaut, RL
    Padilha, AF
    [J]. REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 2003, 100 (01): : 83 - 91
  • [30] CORROSION-RESISTANCE OF HIGH-ALLOY FERRITIC-AUSTENITIC STEELS
    SCHUSTER, C
    ECKSTEIN, HJ
    [J]. NEUE HUTTE, 1977, 22 (05): : 266 - 272