Sulfur tolerance and hydrocarbon stability of La0.75Sr0.25Cr0.5Mn0.5O3/Gd0.2Ce0.8O1.9 composite anode under anodic polarization

被引:33
|
作者
Chen, X. J.
Liu, Q. L.
Chan, S. H.
Brandon, N. P.
Khor, Khiam Aik [1 ]
机构
[1] Nanyang Technol Univ, Sch Mech & Aerosp Engn, Fuel Cell Strateg Res Program, Singapore 639798, Singapore
基金
英国工程与自然科学研究理事会;
关键词
D O I
10.1149/1.2780866
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
A La0.75Sr0.25Cr0.5Mn0.5O3/Gd0.2Ce0.8O1.9 (LSCM/GDC) composite electrode was developed and applied as a solid oxide fuel cell (SOFC) anode for the direct oxidation of sulfur-containing methane. The anode was fully activated in wet CH4 at 850 degrees C and a constant potential of -0.5 V with respect to a Pt/air reference before the fuel was shifted to wet 0.5% H2S+99.5% CH4. In the sulfur-containing methane fuel, the anodic current dropped from 0.233 A cm(-2) to 0.2 A cm(-2) in a 10 h period, showing a performance degradation rate of ca. 1.4%/hr possibly due to sulfur poisoning. In the subsequent 110 h period, the anodic current tended to be relatively stable with a very small degradation rate of 0.017%/h, which is most likely attributed to the coarsening of the electrode microstructure. Though some impurities, such as MnS, La2O2S, and alpha-MnOS, were detected in the X-ray diffraction analysis of the anode after 120 h of stability test, the scanning electron microscopy micrographs and energy-dispersive X-ray analysis showed that no carbon and sulfur deposition was found on the cross-sectional surface of the anode. The results suggest that the LSCM/GDC composite is a promising candidate material for an anode and has much better hydrocarbon stability and sulfur tolerance under the anodic polarization than Ni-based cermets.
引用
收藏
页码:B1206 / B1210
页数:5
相关论文
共 50 条
  • [21] (La0.75Sr0.25)0.95(Cr0.5Mn0.5)O3-δ-Ce0.8Gd0.2O1.9 scaffolded composite cathode for high temperature CO2 electroreduction in solid oxide electrolysis cell
    Zhang, Xiaomin
    Song, Yuefeng
    Guan, Fang
    Zhou, Yingjie
    Lv, Houfu
    Liu, Qingxue
    Wang, Guoxiong
    Bao, Xinhe
    JOURNAL OF POWER SOURCES, 2018, 400 : 104 - 113
  • [22] Characteristics of nano-sized La0.75Sr0.25Cr0.5Mn0.5O3 powders prepared by spray pyrolysis
    Jung, Dae Soo
    Jong, Hee Chan
    Kim, Jung Hyun
    Koo, Hye Young
    Kang, Yun Chan
    Cho, Yoon Ho
    Lee, Jong-Heun
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2010, 11 (03): : 322 - 327
  • [23] Sulfur poisoning and O2 2--pumping regeneration of La0.75Sr0.25Cr0.5Mn0.5O3-δ-Ni-CeO2 0.75 Sr 0.25 Cr 0.5 Mn 0.5 O 3-δ- Ni- CeO 2 anode
    Li, Yiqian
    Li, Yinhao
    Na, Liyuan
    Xiao, Tianyu
    Cui, Yingxin
    Li, Peng
    Lu, Zhe
    JOURNAL OF POWER SOURCES, 2024, 614
  • [24] Direct Utilization of Methanol and Ethanol on La0.75Sr0.25Cr0.5Mn0.5O3−δ Anodes for Solid Oxide Fuel Cells
    Massimiliano Cimenti
    Marco A. Buccheri
    Josephine M. Hill
    Electrocatalysis, 2012, 3 : 59 - 67
  • [25] Evaluation of La0.75Sr0.25Cr0.5Mn0.5O3 protective coating on ferritic stainless steel interconnect for SOFC application
    Lenka, R. K.
    Patro, P. K.
    Sharma, Jyothi
    Mahata, T.
    Sinha, P. K.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (44) : 20365 - 20372
  • [26] In situ study of electrochemical activation and surface segregation of the SOFC electrode material La0.75Sr0.25Cr0.5Mn0.5O3±δ
    Huber, Anne-Katrin
    Falk, Mareike
    Rohnke, Marcus
    Luerssen, Bjoern
    Gregoratti, Luca
    Amati, Matteo
    Janek, Juergen
    PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2012, 14 (02) : 751 - 758
  • [27] Effect of optimal GDC loading on long-term stability of La0.8Sr0.2Co0.2Fe0.8O3-δ/Gd0.2Ce0.8O1.9 composite cathodes
    Li, Dong
    Jin, Yingmin
    Liu, Chaojun
    Fu, Mengyu
    Zong, Xin
    Xiong, Yueping
    CERAMICS INTERNATIONAL, 2021, 47 (05) : 6591 - 6596
  • [28] Ce0.8Sm0.2O1.9中间层对La0.75Sr0.25Cr0.5Mn0.5O3-δ阳极电化学性能的影响
    何寿成
    陈涵
    郭露村
    南京工业大学学报(自然科学版), 2013, 35 (03) : 96 - 100
  • [29] Sulfur poisoning and attempt of oxidative regeneration of La0.75Sr0.25Cr0.5Mn0.5O3-δ anode for solid oxide fuel cell
    Li, Yiqian
    Wang, Zhihong
    Li, Jingwei
    Zhu, Xingbao
    Zhang, Yaohui
    Huang, Xiqiang
    Zhou, Yongjun
    Zhu, Lin
    Lu, Zhe
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 698 : 794 - 799
  • [30] Ce0.8Sm0.2O1.9-La0.8Sr0.2Cr0.5Fe0.5O3-δ Dual-Phase Hollow Fiber Membranes Operated under Different Gradients
    Liu, Tong
    He, Wei
    Huang, Hua
    Wang, Siwei
    Bouwmeester, Henny J. M.
    Chen, Chusheng
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2014, 53 (14) : 6131 - 6136