Effects of antiwear additives on the friction and wear of Si3N4/steel sliding contacts

被引:9
|
作者
Zhao, XZ
Liu, JJ
Zhu, BL
Miao, HZ
Luo, ZB
机构
[1] Tribology Research Institute, Tsinghua University
关键词
ceramics; tribochemistry; adhesive wear; microfracture;
D O I
10.1016/S0043-1648(96)07215-8
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Si3N4-based ceramics have been used for machining cast iron at very high speeds. However, they have been found to be unsuitable for machining steel because of the severe wear of the ceramic cutting tools, which is thought to be mainly caused by the chemical dissolution of the ceramic in the chip at the high temperatures reached at the cutting edge. In this paper, a simulation test was carried out on a pin-on-disk tribometer in order to investigate the effects of two antiwear additives on the friction and wear of Si3N4/1045 steel sliding contacts. Sliding speeds 1.6 m s(-1) and 3.2 m s(-1) were used, respectively, the selected test load was 117.6 N. The test results show that lubricants containing antiwear additives used in this test could greatly reduce the friction coefficient and wear rate of Si3N4 ceramics. Scanning electron microscopy, energy dispersive X-ray spectroscopy and X-ray diffraction spectroscopy were used for the analyses of the worn surfaces. Tribochemical reactions about the additives occurred on the frictional surfaces, the tribochemical films formed on the rubbing surfaces improved the boundary lubrication conditions of the sliding contacts, the interdiffusion and adhesion between the rubbing surfaces were prevented or were greatly reduced.
引用
收藏
页码:99 / 105
页数:7
相关论文
共 50 条
  • [41] Pressureless sintering of dense Si3N4 and Si3N4/SiC composites with nitrate additives
    Kim, Jae-Yuk
    Iseki, Takayoshi
    1996, American Ceramic Soc, Westerville, OH, United States (79)
  • [42] Sliding wear characteristics of Mg/Si3N4 nanocomposites at room and elevated temperatures
    Pasha, Mahammod Babar
    Sharma, Rahul Chandra
    Rao, R. Narasimha
    Ismail, Syed
    Gupta, Manoj
    Materials Letters, 2022, 329
  • [43] Sliding wear characteristics of Mg/Si3N4 nanocomposites at room and elevated temperatures
    Pasha, Mahammod Babar
    Sharma, Rahul Chandra
    Rao, R. Narasimha
    Ismail, Syed
    Gupta, Manoj
    MATERIALS LETTERS, 2022, 329
  • [44] Effect of laser surface texturing on Si3N4/TiC ceramic sliding against steel under dry friction
    Xing Youqiang
    Deng Jianxin
    Feng Xiuting
    Yu Sheng
    MATERIALS & DESIGN, 2013, 52 : 234 - 245
  • [45] Dry sliding friction and wear behaviour of hybrid AA7075/Si3N4/Gr self lubricating composites
    Ul Haq, Mir Irfan
    Anand, Ankush
    MATERIALS RESEARCH EXPRESS, 2018, 5 (06):
  • [46] Friction and Wear Behavior of AA 7075- Si3N4 Composites Under Dry Conditions: Effect of Sliding Speed
    Mir Irfan Ul Haq
    Ankush Anand
    Silicon, 2019, 11 : 1047 - 1053
  • [47] Properties of friction and wear of Si3N4 ceramics against gray cast iron
    Si, Songhua
    Fang, Liang
    Gao, Yimin
    Zhou, Qingde
    Mocaxue Xuebao/Tribology, 1997, 17 (01): : 32 - 37
  • [48] Wear and friction behaviour of Si3N4 ceramics under diesel and biodiesel lubrication
    Aparecida De Almeida, Flávia
    Maru, Marcia Marie
    Do Nascimento Batista, Luciano
    José Alves De Oliveira, Filipe
    Ramos Ferreira E Silva, Rui
    Achete, Carlos Alberto
    Journal of Materials Research and Technology, 2013, 2 (02) : 110 - 116
  • [49] BEHAVIOR OF A SI3N4 CERAMIC IN HIGH-TEMPERATURE FRICTION AND WEAR EXPERIMENTS
    GUILLOT, I
    ARMANET, F
    BERANGER, G
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1989, 120 : 483 - 488
  • [50] Friction and wear of grey cast iron against Si3N4 in emulsion and water
    Xian Jiatong Univ, Xian, China
    Lubr Sci, 3 (247-254):