Mechanical properties of a Ti-15V-3Cr-3Sn-3Al alloy affected by the impurity hydrogen

被引:4
|
作者
Itoh, G [1 ]
Kanno, M [1 ]
Niwa, N [1 ]
机构
[1] KOGAKUIN UNIV, DEPT ENGN MECH, KOGAKUIN 160, JAPAN
关键词
beta titanium alloy; hydrogen; impurity effect; ductility; hydrogen charging; dehydrogenation;
D O I
10.1016/0921-5093(96)10230-6
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of hydrogen on the tensile properties of a beta titanium alloy (Ti-15V-3Cr-3Sn-3Al) has been studied. Cold-rolled specimens and specimens charged with hydrogen (annealed at 500 degrees C for Ih at atmospheric pressure of hydrogen gas) were solution-treated at 800 degrees C for 1 h, water-quenched and subsequently aged at 510 degrees C. Significant retardation in the age-hardening characteristics of the alloy occurred by the hydrogen charging. The effect of hydrogen charging on the ductility was not found except in the as-solution-treated condition, where slight decrease (from 65% to 60%) in the reduction in area by the charging was detected. However, when tensile tests were carried out using a unique testing machine equipped with an ultra high vacuum chamber and a quadrupole mass spectrometer, a large amount of hydrogen gas was evolved from the specimen at the moment of fracture. Furthermore, the ductility of the uncharged specimen was improved with a reduction in the hydrogen content. Thus it can be concluded that the impurity hydrogen event at the uncharged level has a strong correlation with the fracture and causes a deleterious effect on the ductility.
引用
收藏
页码:93 / 97
页数:5
相关论文
共 50 条
  • [21] MECHANICAL-PROPERTIES OF AGED TI-15V-3CR-3AL-3SN ALLOY
    SAKAMOTO, K
    SATO, K
    KITANO, K
    NIWA, N
    ITO, K
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 25 (11) : B328 - B328
  • [22] FORMATION OF (ALPHA+BETA) MICRODUPLEX STRUCTURE IN A TI-15V-3CR-3SN-3AL ALLOY
    INABA, T
    AMEYAMA, K
    TOKIZANE, M
    ISIJ INTERNATIONAL, 1991, 31 (08) : 792 - 798
  • [23] Precipitation in carbon-doped Ti-15V-3Cr-3Sn-3Al
    Hu, D
    Huang, AJ
    Song, XP
    Wu, X
    RARE METAL MATERIALS AND ENGINEERING, 2006, 35 : 225 - 229
  • [24] 2-STEP AGING TREATMENT FOR LOWERING OF SUSCEPTIBILITY TO HYDROGEN EMBRITTLEMENT OF TI-15V-3CR-3SN-3AL ALLOY
    NOZUE, A
    SAKAMAKI, H
    SAITA, Y
    OKUBO, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1993, 57 (10) : 1136 - 1140
  • [25] Improvement of formability for multistage deep drawing of Ti-15V-3Cr-3Sn-3Al alloy sheet
    Harada, Yasunori
    Maeda, Yutaro
    Ueyama, Minoru
    Fukuda, Izumi
    11TH INTERNATIONAL CONFERENCE ON TECHNOLOGY OF PLASTICITY, ICTP 2014, 2014, 81 : 819 - 824
  • [26] MORPHOLOGY OF ALPHA-PRECIPITATE IN TI-15V-3CR-3SN-3AL BETA-TITANIUM ALLOY
    INABA, T
    AMEYAMA, K
    TOKIZANE, M
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1992, 56 (08) : 881 - 888
  • [27] Effect of Aged Microstructure on the Strength and Work Hardening Behavior of Ti-15V-3Cr-3Sn-3Al Alloy
    Sarkar, Rajdeep
    Mukhopadhyay, A.
    Ghosal, P.
    Nandy, T. K.
    Ray, K. K.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (08): : 3516 - 3527
  • [28] THE EFFECT OF HEAT-TREATMENT CONDITIONS ON TENSILE PROPERTIES OF TI-15V-3CR-3SN-3AL
    TSUMORI, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1589 - 1589
  • [29] Fatigue Crack Growth Characteristics of a Ti-15V-3Cr-3Sn-3Al Alloy with Variously Aged Conditions
    Tsay, Leu-Wen
    Chang, S. T.
    Chen, Chun
    MATERIALS TRANSACTIONS, 2013, 54 (03) : 326 - 331
  • [30] DEFORMATION CHARACTERISTICS OF TI-15V-3CR-3SN-3AL AT ELEVATED-TEMPERATURE
    SUZUKI, HG
    FUJII, H
    ISIJ INTERNATIONAL, 1991, 31 (08) : 814 - 819