Thermal stability of carbon nitride thin films

被引:43
|
作者
Hellgren, N
Lin, N
Broitman, E
Serin, V
Grillo, SE
Twesten, R
Petrov, I
Colliex, C
Hultman, L
Sundgren, JE
机构
[1] Univ Illinois, Frederick Seitz Mat Res Lab, Ctr Microanal Mat, Urbana, IL 61801 USA
[2] Linkoping Univ, Dept Phys, Thin Film Phys Div, S-58183 Linkoping, Sweden
[3] Ctr Elaborat Mat Etud Struct, Ctr Rech Sci, F-31055 Toulouse, France
[4] Univ Paris 11, Phys Solides Lab, F-91405 Orsay, France
基金
欧洲研究理事会;
关键词
D O I
10.1557/JMR.2001.0440
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The thermal stability of carbon nitride films, deposited by reactive direct current magnetron sputtering in N-2 discharge, was studied for postdeposition annealing temperatures T-A up to 1000 degreesC. Films were grown at temperatures of 100 degreesC (amorphous structure) and 350 and 550 degreesC (fullerenelike structure) and were analyzed with respect to thickness, composition, microstructure, bonding structure, and mechanical properties as a function of T-A and annealing time. All properties investigated were found to be stable for annealing up to 300 degreesC for long times (> 48 h). For higher T-A, nitrogen is lost from the films and graphitization takes place. At T-A = 500 degreesC the graphitization process takes up to 48 h while at T-A = 900 degreesC it takes less than 2 min. A comparison on the evolution of x-ray photoelectron spectroscopy, electron energy loss spectroscopy and Raman spectra during annealing shows that for T-A > 800 degreesC, preferentially pyridinelike N and -C equivalent toN is lost from the films, mainly in the form of molecular N-2 and C2N2, while N substituted in graphite is preserved the longest in the structure. Films deposited at the higher temperature exhibit better thermal stability, but annealing at temperatures a few hundred degrees Celsius above the deposition temperature for long times is always detrimental for the mechanical properties of the films.
引用
收藏
页码:3188 / 3201
页数:14
相关论文
共 50 条
  • [21] Nanohardness measurement of carbon nitride thin films
    Kojima, I
    Xu, WT
    Fujimoto, T
    SURFACE AND INTERFACE ANALYSIS, 2001, 32 (01) : 74 - 78
  • [22] Preparation and characterization of carbon nitride thin films
    Wan, L
    Egerton, RF
    THIN SOLID FILMS, 1996, 279 (1-2) : 34 - 42
  • [23] Evidence of nanodomes in carbon nitride thin films
    Chowdhury, S
    Laugier, MT
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2004, 201 (02): : R1 - R4
  • [24] Bonding characterization, density measurement, and thermal diffusivity studies of amorphous silicon carbon nitride and boron carbon nitride thin films
    Chattopadhyay, S
    Chen, LC
    Chien, SC
    Lin, ST
    Chen, KH
    JOURNAL OF APPLIED PHYSICS, 2002, 92 (09) : 5150 - 5158
  • [26] Thermal diffusivity in amorphous silicon carbon nitride thin films by the traveling wave technique
    Chattopadhyay, S
    Chen, LC
    Wu, CT
    Chen, KH
    Wu, JS
    Chen, YF
    Lehmann, G
    Hess, P
    APPLIED PHYSICS LETTERS, 2001, 79 (03) : 332 - 334
  • [27] Thermal expansion coefficient of amorphous carbon nitride thin films deposited by glow discharge
    Champi, A
    Lacerda, RG
    Marques, FC
    THIN SOLID FILMS, 2002, 420 : 200 - 204
  • [28] A thermal study of amorphous and textured carbon and carbon nitride thin films via transient grating spectroscopy
    Cometto, Olivier
    Dennett, Cody A.
    Tsang, Siu Hon
    Short, Michael P.
    Teo, Edwin H. T.
    CARBON, 2018, 130 : 355 - 361
  • [29] Carbon nitride (CNx) films formed by ion implantation into thin carbon films
    Husein, IF
    Zhou, YZ
    Chan, C
    Kleiman, JI
    Gudimenko, Y
    Leung, KN
    ION-SOLID INTERACTIONS FOR MATERIALS MODIFICATION AND PROCESSING, 1996, 396 : 255 - 260
  • [30] Preparation of oriented aluminum nitride thin films on polyimide films and piezoelectric response with high thermal stability and flexibility
    Akiyama, Morito
    Morofuji, Yukari
    Kamohara, Toshihiro
    Nishikubo, Keiko
    Ooishi, Yasunobu
    Tsubai, Masayoshi
    Fukuda, Osamu
    Ueno, Naohiro
    ADVANCED FUNCTIONAL MATERIALS, 2007, 17 (03) : 458 - 462