Effects of austenitizing treatment on the corrosion resistance of 14Cr-3Mo martensitic stainless steel

被引:9
|
作者
Park, J. -Y. [1 ]
Park, Y. -S. [1 ]
机构
[1] Yonsei Univ, Dept Met Engn, Seoul 120749, South Korea
关键词
austenitizing; carbides; corrosion resistance; martensitic phase transformation; stainless steels;
D O I
10.5006/1.3279913
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Martensitic stainless steels with a carbon content higher than 0.2wt% need to be heat-treated and quenched for the dissolution of carbides. In this study, the transformation and the corrosion characteristics of the martensitic steels are studied with different austenitizing temperatures for 0.15C- and 0.3C-14Cr-3Mo steels.
引用
收藏
页码:541 / 547
页数:7
相关论文
共 50 条
  • [21] Heat Treatment, Microstructure, Hardness and Corrosion Resistance of Martensitic Stainless Steel X65Cr13 (1.4037)
    Rosemann, P.
    Sieber, P.
    Kukuk, L. D.
    Rossberg, S.
    Betke, U.
    Huetter, S.
    Jakob, P.
    Sehnert, K.
    HTM-JOURNAL OF HEAT TREATMENT AND MATERIALS, 2024, 79 (01): : 15 - 34
  • [22] Influence of Heat Treatment on the Microstructure and Corrosion Resistance of 13 Wt Pct Cr-Type Martensitic Stainless Steel
    Lu, Si-Yuan
    Yao, Ke-Fu
    Chen, Yun-Bo
    Wang, Miao-Hui
    Ge, Xue-Yuan
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (12): : 6090 - 6102
  • [23] Effect of Austenitizing Heat Treatment on the Microstructure and Hardness of Martensitic Stainless Steel AISI 420
    L. D. Barlow
    M. Du Toit
    Journal of Materials Engineering and Performance, 2012, 21 : 1327 - 1336
  • [24] Effect of Austenitizing Heat Treatment on the Microstructure and Hardness of Martensitic Stainless Steel AISI 420
    Barlow, L. D.
    Du Toit, M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (07) : 1327 - 1336
  • [25] Influence of the heat treatment on the corrosion resistance of the martensitic stainless steel type AISI 420
    Candelária, AF
    Pinedo, CE
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2003, 22 (16) : 1151 - 1153
  • [26] Heat Treatment Process for Martensitic Stainless Steel Pyrowear 675 for Improved Corrosion Resistance
    Trivedi, Hitesh K.
    Otto, Frederick
    Mccoy, Bryan
    Bhattacharya, Rabi S.
    Piazza, Timothy
    BEARING STEEL TECHNOLOGIES: 10TH VOLUME: ADVANCES IN STEEL TECHNOLOGIES FOR ROLLING BEARINGS, 2015, 1580 : 465 - 484
  • [27] Stress Corrosion Cracking of 13Cr-5Ni-2Mo Martensitic Stainless Steel in Methanol
    Sridhar, Narasi
    Cao, Liu
    CORROSION, 2022, 78 (08) : 740 - 750
  • [28] Pitting corrosion of super martensitic stainless steel 00Cr13Ni5Mo2
    Li, J. L.
    Qu, C. T.
    Zhu, S. D.
    Liu, L.
    Gao, Z. Q.
    ANTI-CORROSION METHODS AND MATERIALS, 2014, 61 (06) : 387 - 394
  • [29] Influence of Cutting Fluids on the Corrosion Resistance of X20Cr13 Martensitic Stainless Steel
    Kostadin, Tihana
    Cukor, Goran
    Jurkovic, Zoran
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2018, 13 (12): : 11986 - 11999
  • [30] Improving corrosion resistance of super-13Cr martensitic stainless steel by a homogenized amorphous film
    Yang, Zi-Chen
    Dong, Hui
    Han, Yan
    Yao, Jian-Tao
    Wang, Li-Shuang
    Zhou, Yong
    SURFACE & COATINGS TECHNOLOGY, 2024, 494