Dissimilar Laser Welding of Ti-6Al-4V to Ti-6Al-6V-2Sn

被引:2
|
作者
Chiu, C. Y. [1 ]
Lu, M. Y. [1 ]
Tsay, L. W. [1 ]
机构
[1] Natl Taiwan Ocean Univ, Inst Mat Engn, Keelung 202, Taiwan
来源
关键词
Laser welding; Notched tensile strength; Ti-6Al-4V; Ti-6A16V-2Sn; POSTWELD HEAT-TREATMENT; CRACK GROWTH-BEHAVIOR; FRACTURE-TOUGHNESS; TITANIUM-ALLOYS; MICROSTRUCTURE;
D O I
10.4028/www.scientific.net/AMR.295-297.2353
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Notched tensile strength (NTS) of the Ti-6Al-4V (Ti-6-4) to Ti-6A16V-2Sn (Ti-6-6-2) dissimilar laser yields were determined, which had been subjected to post-weld heat treatment (PWHT) over the temperature range of 482-704 degrees C. The results indicated for the weld with the PWFIT at 482 degrees C the fusion zone (FZ) and heat-affected zone (HAZ) showed a peak hardness, as compared with other welds at the counterpart regions, whereas, the weld with the PWHT at 704 degrees C had the lowest hardness among the welds. In all the welds, the FZ of the weld subjected to PWHT at 482 degrees C possessed the lowest NTS, while the as-welded and the weld with PWHT at 704 degrees C had superior NTS to others. The presence of grain boundary alpha, which promoted grain boundary shear, accounted for the typical features of mainly transgranular fracture with intergranular dimples of the welds.
引用
收藏
页码:2353 / 2357
页数:5
相关论文
共 50 条
  • [1] The effect of post-weld heat treatment on the notched tensile fracture of Ti-6Al-4V to Ti-6Al-6V-2Sn dissimilar laser welds
    Hsieh, C. T.
    Chu, C. Y.
    Shiue, R. K.
    Tsay, L. W.
    MATERIALS & DESIGN, 2014, 59 : 227 - 232
  • [2] ENHANCEMENT OF FATIGUE-CRACK GROWTH AND FRACTURE RESISTANCE IN TI-6AL-4V AND TI-6AL-6V-2SN
    YODER, GR
    COOLEY, LA
    CROOKER, TW
    ASTRONAUTICS & AERONAUTICS, 1977, 15 (10): : B22 - B22
  • [3] Diffusion bonding superplastic forming of Ti-6Al-6V-2Sn/SUS 304 stainless steel Ti-6Al-6V-2Sn
    Shyu, JS
    Chuang, TH
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1996, 5 (01) : 84 - 88
  • [4] Laser welding of Ti-6Al-4V to Nitinol
    Zoeram, A. Shojaei
    Mousavi, S. A. A. Akbari
    MATERIALS & DESIGN, 2014, 61 : 185 - 190
  • [5] ENHANCEMENT OF FATIGUE CRACK GROWTH AND FRACTURE RESISTANCE IN TI-6AL-4V AND TI-6AL-6V-2SN THROUGH MICROSTRUCTURAL MODIFICATION
    YODER, GR
    COOLEY, LA
    CROOKER, TW
    REPORT OF NRL PROGRESS, 1976, (NOV): : 19 - 19
  • [6] ENHANCEMENT OF FATIGUE CRACK GROWTH AND FRACTURE RESISTANCE IN TI-6AL-4V AND TI-6AL-6V-2SN THROUGH MICROSTRUCTURAL MODIFICATION
    YODER, GR
    COOLEY, LA
    CROOKER, TW
    JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1977, 99 (04): : 313 - 318
  • [7] SOME OBSERVATIONS ON HARDENABILITY OF TI-6AL-6V-2SN
    HICKEY, CF
    FOPIANO, PJ
    METALLURGICAL TRANSACTIONS, 1970, 1 (06): : 1775 - &
  • [8] WELDING OF Ti-6Al-4V IN AIR
    Schwandt, Carsten
    Allen, Chris
    Fray, Derek J.
    TMS 2014 SUPPLEMENTAL PROCEEDINGS, 2014, : 87 - 92
  • [9] Fiber laser welding of NiTi to Ti-6Al-4V
    Miranda, R. M.
    Assuncao, E.
    Silva, R. J. C.
    Oliveira, J. P.
    Quintino, L.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2015, 81 (9-12): : 1533 - 1538
  • [10] Fiber laser welding of NiTi to Ti-6Al-4V
    R. M. Miranda
    E. Assunção
    R. J. C. Silva
    J. P. Oliveira
    L. Quintino
    The International Journal of Advanced Manufacturing Technology, 2015, 81 : 1533 - 1538