Sensitive luminescence techniques to study the early stages of polymer oxidation

被引:19
|
作者
Colwell, John M. [1 ]
Nikolic, Melissa A. L. [1 ]
Bottle, Steven E. [1 ]
George, Graeme A. [1 ]
机构
[1] Queensland Univ Technol, Sch Chem Phys & Mech Engn, Brisbane, Qld 4000, Australia
基金
澳大利亚研究理事会;
关键词
Chemiluminescence; Profluorescent nitroxides; Induction period; cis-Polyisoprene; Polypropylene; Thermo-oxidation sensor; FREE-RADICAL REACTIONS; THERMOOXIDATIVE DEGRADATION; PROFLUORESCENT NITROXIDES; THERMAL-OXIDATION; POLYPROPYLENE; CHEMILUMINESCENCE; POLYETHYLENE; POLYOLEFINS; PRODUCTS; SENSORS;
D O I
10.1016/j.polymdegradstab.2013.06.010
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
This paper describes recent developments in the use of chemiluminescence (CL) and profluorescent nitroxides (PFNs) in probing the "induction period" of polymer oxidation. CL measures the instantaneous rate of reaction of hydroperoxides responsible for initiating degradation and the spreading of oxidation, while PFNs can be used to measure the concentration of alkyl radicals produced in oxidation events and thus provide an integrating sensor for the extent of cumulative damage. The PFN additive acts as an oxidation retarder by competing with oxygen to scavenge the alkyl radicals that generate chain carrying peroxy radicals and so mirrors the performance of hindered amine stabilisers (HAS) in one part of their stabilisation cycle. Using the example of polypropylene (PP) and cis-polyisoprene (PIP) as substrates which can rapidly spread oxidative damage, the factors controlling the reaction of PFNs can be determined from CL and fluorescence as well as infra-red (ER) spectroscopy through the detection of oxidation products as measured by the carbonyl index. Matrix effects on the reactivity are demonstrated using a polyethylene-norbornene copolymer (TOPAS) as carrier for both PIP and the PFN and it is seen that the PFN is a radical scavenger only above T-g of the carrier. When PIP alone is oxidized, the PFN is an integrating sensor for free radical production under ambient conditions for up to twelve months while also stabilizing the polymer. Critically, it is thus able to determine the underlying rate of radical production in the oxidation induction period. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2436 / 2444
页数:9
相关论文
共 50 条
  • [31] Oxidation-Sensitive Supramolecular Polymer Nanocylinders
    Nicolas, Clemence
    Ghanem, Tatiana
    Canevet, David
    Salle, Marc
    Nicol, Erwan
    Gautier, Christelle
    Levillain, Eric
    Niepceron, Frederick
    Colombani, Olivier
    MACROMOLECULES, 2022, 55 (14) : 6167 - 6175
  • [32] MRI techniques in early stages of cartilage disease
    Burstein, D
    Bashir, A
    Gray, ML
    INVESTIGATIVE RADIOLOGY, 2000, 35 (10) : 622 - 638
  • [33] Techniques for analyzing the early stages of crystallization reactions
    Schüth, F
    Bussian, P
    Ågren, P
    Schunk, S
    Lindén, M
    SOLID STATE SCIENCES, 2001, 3 (07) : 801 - 808
  • [34] THE EARLY STAGES OF THE OXIDATION OF ADRENALINE IN DILUTE SOLUTION
    TRAUTNER, EM
    BRADLEY, TR
    AUSTRALIAN JOURNAL OF SCIENTIFIC RESEARCH SERIES B-BIOLOGICAL SCIENCES, 1951, 4 (03): : 303 - 343
  • [35] Temperature effects in the early stages of titanium oxidation
    Vaquila, I
    Passeggi, MCG
    Ferron, J
    APPLIED SURFACE SCIENCE, 1996, 93 (03) : 247 - 253
  • [36] OBSERVATIONS ON THE EARLY STAGES OF OXIDATION OF TITANIUM CARBIDE
    CHATTERJEE, DK
    LIPSITT, HA
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1982, 13 (10): : 1837 - 1841
  • [37] The surface characterization of the early stages of the oxidation of titanium
    Mizuno, Y
    Tanaka, A
    Takakuwa, Y
    Ishida, F
    Takahiro, K
    Tonda, H
    Ishikawa, K
    Takano, T
    Ikeuchi, T
    Okada, T
    Yamaguchi, S
    Homma, T
    MATERIALS AT HIGH TEMPERATURES, 2000, 17 (01) : 13 - 21
  • [38] EARLY STAGES IN OXIDATION OF TANTALUM AT LOW TEMPERATURES
    COWGILL, MG
    STRINGER, J
    JOURNAL OF THE INSTITUTE OF METALS, 1963, 91 (06): : 220 - &
  • [39] TEM investigations of the early stages of TiAl oxidation
    Lang, C
    Schutze, M
    OXIDATION OF METALS, 1996, 46 (3-4): : 255 - 285
  • [40] Early stages of nucleation and growth in a polymer blend
    Balsara, NP
    Lin, C
    Hammouda, B
    PHYSICAL REVIEW LETTERS, 1996, 77 (18) : 3847 - 3850