Tailoring AC magnetic properties of FeCoNi(MnSi)x (0 ≤ x ≤ 0.4) high-entropy alloys by the addition of Mn and Si elements

被引:37
|
作者
Li, Zhong [1 ]
Gu, Yong [1 ,2 ]
Pan, Minxiang [1 ,3 ]
Wang, Chenxu [1 ]
Wu, Zhongyuan [1 ]
Hou, Xueling [1 ]
Tan, Xiaohua [1 ]
Xu, Hui [1 ]
机构
[1] Shanghai Univ, Sch Mat Sci & Engn, Inst Mat Sci, Shanghai 200072, Peoples R China
[2] Hangzhou Normal Univ, Qianjiang Coll, Hangzhou 310036, Zhejiang, Peoples R China
[3] China Jiliang Univ, Magnetism Key Lab Zhejiang Prov, Hangzhou 310018, Zhejiang, Peoples R China
基金
中国国家自然科学基金;
关键词
High-entropy alloys (HEAs); AC magnetic properties; Specific total loss (P-s); Eddy current loss (P-e); PHASE-FORMATION; MICROSTRUCTURE; BEHAVIOR; COMPOSITES; SEPARATION;
D O I
10.1016/j.jallcom.2019.03.411
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this work, we investigate the evolution with x of the microstructure and alternating current (AC) magnetic properties of FeCoNi(MnSi)(x) (0 <= x <= 0.4) high-entropy alloys (HEAs) with the motivation of exploring the potential applications of soft magnetic HEAs. The suitable addition of MnSi improves AC remanence (AC B-r), AC coercivity (AC H-c) and especially specific total loss (P-s) while it suppresses amplitude permeability (mu a) and AC maximum magnetic flux density (AC B-m), which suggests that the HEAs can be used as a new soft magnetic material with low Br and low Hc. Ps can be divided into two parts: hysteresis loss (P-h), eddy current loss (P-e), and further studies show that the P-h plays an important role at the frequency of 50 Hz, while the P-e is dominant in the total losses when the frequency is 950 Hz. This provides the direction of efforts to reduce the P-s. The XRD, SEM and TEM results show that these alloys contain simple FCC structure, but a new Mn6Ni16Si7 intermetallic compound appears when x >= 0.3, and it has a big influence on the AC magnetic properties of HEAs. (C) 2019 Elsevier B.V. All rights reserved.
引用
收藏
页码:215 / 221
页数:7
相关论文
共 50 条
  • [41] Effect of Al/Si ratio on magnetic properties and microstructure of FeCoMnAlSi high-entropy soft magnetic alloys with various Mn contents
    Song, Z. B.
    Huang, T. X.
    Jain, Aditya
    Wang, Y. G.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1017
  • [42] Effect of Mo addition on AC soft magnetic property, hardness and microstructure of FeCoNiMox (0 < x ≤ 0.25) medium entropy alloys
    Xu, Hui
    Xia, Yubing
    Chen, Mengya
    Ma, Le
    Li, Haonan
    Li, Bin
    Wu, Zhongyuan
    Tan, Xiaohua
    MATERIALS CHARACTERIZATION, 2023, 206
  • [43] The effect of Cr and Nb addition on the structural, morphological, and magnetic properties of the mechanically alloyed high entropy FeCoNi alloys
    Yakin, Alican
    Simsek, Telem
    Avar, Baris
    Chattopadhyay, Arun K.
    Ozcan, Sadan
    Simsek, Tuncay
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2022, 128 (08):
  • [44] Beyond Solid Solution High-Entropy Alloys: Tailoring Magnetic Properties via Spinodal Decomposition
    Rao, Ziyuan
    Dutta, Biswanath
    Kormann, Fritz
    Lu, Wenjun
    Zhou, Xuyang
    Liu, Chang
    da Silva, Alisson Kwiatkowski
    Wiedwald, Ulf
    Spasova, Marina
    Farle, Michael
    Ponge, Dirk
    Gault, Baptiste
    Neugebauer, Jorg
    Raabe, Dierk
    Li, Zhiming
    ADVANCED FUNCTIONAL MATERIALS, 2021, 31 (07)
  • [45] Microstructure and properties of FeCoNiCrX (X=Mn, Al) high-entropy alloy coatings
    Rong, Zhiyi
    Wang, Chaohui
    Wang, You
    Dong, Meiling
    You, Yuan
    Wang, Jianing
    Liu, Huinan
    Liu, Jiaqi
    Wang, Yuhang
    Zhu, Zhongyu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 921
  • [46] The effect of Cr and Nb addition on the structural, morphological, and magnetic properties of the mechanically alloyed high entropy FeCoNi alloys
    Alican Yakın
    Telem Şimşek
    Barış Avar
    Arun K. Chattopadhyay
    Sadan Özcan
    Tuncay Şimşek
    Applied Physics A, 2022, 128
  • [47] Dry Sliding Wear Behavior of Al0.4FeCrNiCox(x = 0, 0.25, 0.5, 1.0 mol) High-Entropy Alloys
    Saurav Kumar
    Amar Patnaik
    Ajaya Kumar Pradhan
    Vinod Kumar
    Metallography, Microstructure, and Analysis, 2019, 8 : 545 - 557
  • [48] Dry Sliding Wear Behavior of Al0.4FeCrNiCox(x=0, 0.25, 0.5, 1.0 mol) High-Entropy Alloys
    Kumar, Saurav
    Patnaik, Amar
    Pradhan, Ajaya Kumar
    Kumar, Vinod
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2019, 8 (04) : 545 - 557
  • [49] Effect of Cobalt Content on Thermal, Mechanical, and Microstructural Properties of Al0.4FeCrNiCox (x = 0, 0.25, 0.5, 1.0 mol) High-Entropy Alloys
    Saurav Kumar
    Amar Patnaik
    Ajaya Kumar Pradhan
    Vinod Kumar
    Journal of Materials Engineering and Performance, 2019, 28 : 4111 - 4119
  • [50] Microstructures and properties of CrxFeNi(3-x)Al high-entropy alloys
    Wen Zhang
    Xicong Ye
    Dong Xu
    Chang Liu
    Dong Fang
    Bo Li
    Applied Physics A, 2022, 128