Setting and Hardening Behaviour of Alkali-Activated Landfilled Fly Ash-Slag Binder at Room Temperature

被引:9
|
作者
Liu, Wei [1 ,2 ]
Lin, Lin [3 ]
Wang, Shuping [3 ]
Peng, Xiaoqin [3 ]
Wu, Bobo [3 ,4 ]
Sun, Keke [3 ]
Zeng, Lu [3 ]
机构
[1] Shenzhen Univ, Guangdong Prov Key Lab Durabil Marine Civil Engn, Shenzhen 518060, Peoples R China
[2] Shenzhen Univ, Shenzhen Durabil Ctr Civil Engn, Shenzhen 518060, Peoples R China
[3] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400045, Peoples R China
[4] Zunyi Transportat & Tourism Investment Grp Co Ltd, Dept Project Management, Zunyi 563000, Peoples R China
基金
中国国家自然科学基金;
关键词
landfilled fly ash; alkali activation; setting time; strength development; microstructure; C-S-H; GEOPOLYMER CONCRETE; STRENGTH; METAKAOLIN; MORTAR; CEMENT; FTIR;
D O I
10.3390/ma13143130
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A geopolymer is normally considered an environmentally friendly binder due to the utilisation of industrial wastes. This study focusses on the potential of geopolymer preparation at room temperature from landfilled fly ash (LFA) which has been discharged to the land for more than three years. To accelerate the reaction process, 20-30 wt.% LFA was replaced by ground-granulated blast-furnace slag (GGBS). The effect of water glass modulus, Na2O content, water-to-solid ratio, and GGBS content on the setting time and strength development of the binder was discussed. Results showed that to activate LFA, the optimal value of the sodium silicate modulus for alkaline solution was 1.4-1.6 with a Na2O content of 10%, and the water-to-solid ratio was 0.4. In addition, the setting time of the binder reduced with increasing content of GGBS replacement, and the compressive strength increased due to the coexistence of C-(A)-S-H and zeolite-like phases. The maximum compressive strength of the binder was 29.2 MPa after 56 days of curing. The relatively low strength was likely due to the absence of the Q(4)unit with a three-dimensional structure.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Design and microstructural analysis of the mixture proportion of alkali-activated fly ash-slag composite cementitious material
    Xu, Hongchun
    Yin, Hang
    Ge, Pei
    MATERIALS RESEARCH EXPRESS, 2024, 11 (11)
  • [32] Study on optimization of mixing ratio and shrinkage property of alkali-activated ultrafine fly ash-slag mortar
    Wang, Jun
    Wang, Haofan
    Li, Zhaoxi
    Yan, Jun
    MATERIALS TODAY COMMUNICATIONS, 2024, 41
  • [33] Study on the Macroscopic Properties and Microstructure of High Fly Ash Content Alkali-Activated Fly Ash Slag Concrete Cured at Room Temperature
    Yuan, Zhu
    Jia, Yanmin
    Xie, Xuanben
    Xu, Junming
    MATERIALS, 2025, 18 (03)
  • [34] Influence of calcium oxide and sodium silicate on the setting, hardening and shrinkage properties of alkali-activated slag/fly ash mortars
    Tao, Yongzhi
    Sun, Keke
    Yang, Jie
    Shen, Bo
    Zhang, Yongjun
    Hui, David
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 453
  • [35] Effects of Mg-based admixtures on chloride diffusion in alkali-activated fly ash-slag mortars
    Zhang, Jingxiao
    Ma, Yuwei
    Zhang, Zuhua
    Yang, Xiaocong
    Nong, Xingzhong
    Wang, Hao
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2024, 21
  • [36] The strength of alkali-activated slag/fly ash mortar blends at ambient temperature
    Wardhono, Arie
    Law, David W.
    Strano, Anthony
    CIVIL ENGINEERING INNOVATION FOR A SUSTAINABLE, 2015, 125 : 650 - 656
  • [37] Effect of active MgO on the hydration kinetics characteristics and microstructures of alkali-activated fly ash-slag materials
    Ma, Hongqiang
    Li, Xiaomeng
    Zheng, Xuan
    Niu, Xiaoyan
    Fang, Youliang
    CONSTRUCTION AND BUILDING MATERIALS, 2022, 361
  • [38] In-situ X-ray tomographic imaging of microstructure evolution of fly ash and slag particles in alkali-activated fly ash-slag paste
    Fang, Guohao
    Wang, Qiang
    Zhang, Mingzhong
    COMPOSITES PART B-ENGINEERING, 2021, 224
  • [39] Effect of admixture on the pore structure refinement and enhanced performance of alkali-activated fly ash-slag concrete
    Keulen, A.
    Yu, Q. L.
    Zhang, S.
    Grunewald, S.
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 162 : 27 - 36
  • [40] DIABIND - AN ALKALI-ACTIVATED SLAG FLY-ASH BINDER FOR ACID-RESISTANT CONCRETE
    BLAAKMEER, J
    ADVANCED CEMENT BASED MATERIALS, 1994, 1 (06): : 275 - 276