Stirring an Al-7Si-0.3Mg casting alloy during solidification inhibits the creation of the dendritic structure such that the primary alpha-Al forms as spheroids and other compact irregular shapes owing to thixotropic behaviour. The extruded stir cast alloy exhibits improved mechanical properties, particularly high elongation (15%) and impact energy (14.5 J) but with slightly lower ultimate tensile strength (270 MPa). Ir is suggested that the superior ductility and impact properties of the extruded stir cast alloy compared with the standard product is a result of the presence of alternately arranged bands of alpha-Al and eutectic silicon, such that cracks nucleated preferentially on silicon particles are arrested as they approach the adjacent alpha-Al. The presence of iron in the alloy results in the formation of coarse beta-FeSiAl5 phase associated with poor mechanical properties. However, trace additions of beryllium lead to formation of a new (Be-Fe)-BeSiFe2Al8 phase which mitigates solve of the deleterious effects of the iron. (C) 1997 The Institute of Materials.
引用
收藏
页码:337 / 342
页数:6
相关论文
共 50 条
  • [21] Effect of SiC particles on the laser sintering of Al-7Si-0.3Mg alloy
    Simchi, A.
    Godlinski, D.
    [J]. SCRIPTA MATERIALIA, 2008, 59 (02) : 199 - 202
  • [22] MODIFICATION OF AL-7SI-0.3MG ALLOY BY SODIUM AND STRONTIUM IN PRESENCE OF ANTIMONY
    WANG, W
    GRUZLESKI, JE
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 1989, 5 (05) : 471 - 475
  • [24] The effect of Sr and Fe additions on the microstructure and mechanical properties of a direct squeeze cast Al-7Si-0.3Mg alloy
    J. X. Dong
    P. A. Karnezis
    G. Durrant
    B. Cantor
    [J]. Metallurgical and Materials Transactions A, 1999, 30 : 1341 - 1356
  • [25] INFLUENCE OF BISMUTH IMPURITY ON THE SOLIDIFICATION KINETIC AND MICROSTRUCTURE OF GD-CONTAINING Al-7Si-0.3Mg CAST ALLOYS
    Gursoy, Ozen
    Timelli, Giulio
    [J]. 32ND INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, METAL 2023, 2024, : 38 - 44
  • [26] The effect of Sr and Fe additions on the microstructure and mechanical properties of a direct squeeze cast Al-7Si-0.3Mg alloy
    Dong, JX
    Karnezis, PA
    Durrant, G
    Cantor, B
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (05): : 1341 - 1356
  • [27] Tensile and creep properties of Al-7Si-0.3Mg alloy with Zr and Er addition
    Rashno, S.
    Reihanian, M.
    Ranjbar, Khalil
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 2020, 36 (14) : 1603 - 1613
  • [28] THE FORMATION OF BETA-FESIAL5, AND BE-FE PHASES IN AL-7SI-0.3MG ALLOY CONTAINING BE
    MURALI, S
    RAMAN, KS
    MURTHY, KSS
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 190 (1-2): : 165 - 172
  • [29] Microstructure and Impression Creep Behavior of Al-7Si-0.3Mg Alloy with Zr Addition
    Reihanian, M.
    Ranjbar, Khalil
    Rashno, S.
    [J]. METALS AND MATERIALS INTERNATIONAL, 2021, 27 (08) : 2530 - 2540
  • [30] Optimization of Solution Treatment of Cast Al-7Si-0.3Mg and Al-8Si-3Cu-0.5Mg Alloys
    Sjolander, Emma
    Seifeddine, Salem
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (04): : 1916 - 1927