Stress corrosion cracking of a recent rare-earth containing magnesium alloy, EV31A, and a common Al-containing alloy, AZ91E

被引:64
|
作者
Padekar, Bharat S. [1 ,3 ]
Raman, R. K. Singh [1 ,2 ]
Raja, V. S. [3 ]
Paul, Lyon [4 ]
机构
[1] Monash Univ, Dept Mech & Aerosp Engn, Melbourne, Vic 3800, Australia
[2] Monash Univ, Dept Chem Engn, Melbourne, Vic 3800, Australia
[3] Indian Inst Technol, Dept Met Engn & Mat Sci, Mumbai 400076, Maharashtra, India
[4] Magnesium Elektron Ltd, Manchester, Lancs, England
关键词
Magnesium; SEM; Stress corrosion; SIMULATED BODY-FLUID; PHYSIOLOGICAL ENVIRONMENT; TRANSGRANULAR SCC; MG; MICROSTRUCTURE; BEHAVIOR; ZN; SUSCEPTIBILITY; EMBRITTLEMENT; DEGRADATION;
D O I
10.1016/j.corsci.2013.01.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Stress corrosion cracking of the magnesium alloy Elektron 21 (ASTM-EV31A) and AZ91E was studied using constant load test in 0.1 M NaCl solution (saturated with Mg(OH)(2), and slow strain rate test using glycerol, distilled water and Mg(OH)(2) saturated, 0.01 M and 0.1 M NaCl solutions. Slow strain rate test indicated that EV31A was less susceptible to stress corrosion cracking than AZ91E. Under less intense loading of constant load, EV31A was found to be resistant to stress corrosion cracking. Fractography of EV31A specimens showed little evidence of hydrogen embrittlement. The superior resistance of EV31A is attributed to a more robust oxide/hydroxide layer. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1 / 9
页数:9
相关论文
共 50 条
  • [21] Effect of a Novel Al-SiC Grain Refiner on the Microstructure and Properties of AZ91E Magnesium Alloy
    A. Azad
    L. Bichler
    A. Elsayed
    International Journal of Metalcasting, 2013, 7 : 49 - 59
  • [22] Characterization of rare-earth conversion films formed on the AZ31 magnesium alloy and its relation with corrosion protection
    Montemor, M. F.
    Simoes, A. M.
    Carmezim, M. J.
    APPLIED SURFACE SCIENCE, 2007, 253 (16) : 6922 - 6931
  • [23] Microstructure and corrosion resistance of warm sprayed titanium coatings with polymer sealing for corrosion protection of AZ91E magnesium alloy
    Moronczyk, B.
    Ura-Binczyk, E.
    Kuroda, S.
    Jaroszewicz, J.
    Molak, R. M.
    SURFACE & COATINGS TECHNOLOGY, 2019, 363 : 142 - 151
  • [24] Hydrogen behaviour during stress-corrosion cracking of an AZ31 magnesium alloy
    Kuramoto, S.
    Araki, I.
    Kanno, M.
    Keikinzoku/Journal of Japan Institute of Light Metals, 2001, 51 (08): : 397 - 402
  • [26] EFFECT OF A NOVEL Al-SiC GRAIN REFINER ON THE MICROSTRUCTURE AND PROPERTIES OF AZ91E MAGNESIUM ALLOY
    Azad, A.
    Bichler, L.
    Elsayed, A.
    INTERNATIONAL JOURNAL OF METALCASTING, 2013, 7 (04) : 49 - 59
  • [27] Influence of SRB on corrosion of AZ91 magnesium alloy in solution containing chlorine ions
    College of Materials Science and Engineering, Jilin University, Changchun 130022, China
    Huanan Ligong Daxue Xuebao, 2008, 7 (92-96):
  • [28] On the stability of the oxides film formed on a magnesium alloy containing rare-earth elements
    Leleu, Samuel
    Rives, Bertrand
    Bour, Jerome
    Causse, Nicolas
    Pebere, Nadine
    ELECTROCHIMICA ACTA, 2018, 290 : 586 - 594
  • [29] Investigations into stress corrosion cracking behaviour of AZ91D magnesium alloy in physiological environment
    Choudhary, Lokesh
    Szmerling, Jeremy
    Goldwasser, Robert
    Raman, R. K. Singh
    11TH INTERNATIONAL CONFERENCE ON THE MECHANICAL BEHAVIOR OF MATERIALS (ICM11), 2011, 10
  • [30] Corrosion behavior of AZ31 magnesium alloy in the chloride solution containing ammonium nitrate
    Cui, Zhongyu
    Ge, Feng
    Lin, Yi
    Wang, Liwei
    Lei, Li
    Tian, Huiyun
    Yu, Mingdong
    Wang, Xin
    ELECTROCHIMICA ACTA, 2018, 278 : 421 - 437