Attrition resistance and catalytic performance of spray-dried iron Fischer-Tropsch catalysts in a stirred-tank slurry reactor

被引:10
|
作者
Bukur, DB [1 ]
Ma, WP
Carreto-Vazquez, V
Nowicki, L
Adeyiga, AA
机构
[1] Texas A&M Univ, Dept Chem Engn, College Stn, TX 77843 USA
[2] Hampton Univ, Dept Chem Engn, Hampton, VA 23688 USA
关键词
D O I
10.1021/ie034056o
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Attrition properties of two spray-dried iron Fischer-Tropsch (F-T) catalysts with compositions 100:5:4.2:11 Fe/Cu/K/(P)SiO2 (catalyst P; P = precipitated) and 100:5:4.2:1.1 Fe/Cu/K/(B)SiO2 (catalyst B; B = binder) were studied under reactive conditions in a stirred-tank slurry reactor (STSR) by determining particle size distribution and morphology before and after reaction tests. Catalyst P experienced a large reduction in Sauter mean diameter (87%) after 380 h of testing in the STSR, which is attributed to its morphology (large number of irregularly shaped particles). Low attrition strength of this catalyst was also evident from considerable generation of fine particles (<10 mum) during the STSR test (62.5% increase in fraction of fines). Catalyst B, consisting of largely spherical particles, experienced a smaller reduction in Sauter mean diameter (39.9%) and generation of fine particles was much smaller (3.7%). These two catalysts had excellent selectivity characteristics (low methane and high C-5(+) yields), but their productivity and stability (deactivation rate) need to be improved.
引用
收藏
页码:1359 / 1365
页数:7
相关论文
共 50 条
  • [41] SLURRY PHASE FISCHER-TROPSCH SYNTHESIS WITH IRON-MANGANESE CATALYSTS
    PENNLINE, HW
    ZAROCHAK, MF
    TISCHER, RE
    SCHEHL, RR
    APPLIED CATALYSIS, 1986, 21 (02): : 313 - 328
  • [42] PRODUCT DISTRIBUTION FROM IRON CATALYSTS IN FISCHER-TROPSCH SLURRY REACTORS
    SATTERFIELD, CN
    HUFF, GA
    LONGWELL, JP
    INDUSTRIAL & ENGINEERING CHEMISTRY PROCESS DESIGN AND DEVELOPMENT, 1982, 21 (03): : 465 - 470
  • [43] Characterization of bubble column slurry phase iron Fischer-Tropsch catalysts
    Jin, Y
    Datye, AK
    NATURAL GAS CONVERSION V, 1998, 119 : 209 - 214
  • [44] MASS-TRANSFER AND PRODUCT SELECTIVITY IN A MECHANICALLY STIRRED FISCHER-TROPSCH SLURRY REACTOR
    SATTERFIELD, CN
    HUFF, GA
    ACS SYMPOSIUM SERIES, 1982, 196 : 225 - 236
  • [45] The activity, stability and selectivity of Fischer-Tropsch iron catalysts in slurry reactors
    Nowicki, L
    Ledakowicz, S
    Bukur, DB
    PRZEMYSL CHEMICZNY, 2003, 82 (8-9): : 580 - 582
  • [46] Attrition studies with precipitated iron Fischer-Tropsch catalysts under reaction conditions
    Bukur, DB
    Ma, WP
    Carreto-Vazquez, V
    TOPICS IN CATALYSIS, 2005, 32 (3-4) : 135 - 141
  • [47] Attrition resistance of spray-dried iron F-T catalysts: effect of activation conditions
    Zhao, R
    Sudsakorn, K
    Goodwin, JG
    Jothimurugesan, K
    Gangwal, SK
    Spivey, JJ
    CATALYSIS TODAY, 2002, 71 (3-4) : 319 - 326
  • [48] Fischer-Tropsch synthesis in milli-fixed bed reactor: Comparison with centimetric fixed bed and slurry stirred tank reactors
    Chambrey, S.
    Fongarland, P.
    Karaca, H.
    Piche, S.
    Griboval-Constant, A.
    Schweich, D.
    Luck, F.
    Savin, S.
    Khodakov, A. Y.
    CATALYSIS TODAY, 2011, 171 (01) : 201 - 206
  • [49] The role of catalyst activation on the activity and attrition of precipitated iron Fischer-Tropsch catalysts
    Datye, AK
    Shroff, MD
    Harrington, MS
    Sault, AG
    Jackson, NB
    NATURAL GAS CONVERSION IV, 1997, 107 : 169 - 174
  • [50] FISCHER-TROPSCH SYNTHESIS - A MEASURE OF THE CONTRIBUTION OF HYDROGENOLYSIS USING A DOUBLY PROMOTED IRON CATALYST IN A CONTINUOUS STIRRED TANK REACTOR
    HUANG, C
    DABBAGH, HA
    DAVIS, BH
    APPLIED CATALYSIS, 1991, 73 (02): : 237 - 248