Effect of hydrogen on fatigue crack growth in austenitic Fe-Mn-Al steel

被引:0
|
作者
Mittal, SC
Prasad, RC
Deshmukh, MB
机构
[1] Indian Inst Technol, DEPT MET ENGN & MAT SCI, BOMBAY, MAHARASHTRA, INDIA
[2] NAVAL MAT RES LAB, BOMBAY, MAHARASHTRA, INDIA
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The decrease in fatigue resistance of an austenitic Fe-Mn-Al steel, due to presence of cathodically precharged hydrogen has been evaluated in the present study. Compact tension (CT) specimens precharged with hydrogen and a control without hydrogen charging were subjected to sinusoidal, tension-tension, cyclic loading at stress ratios (R) of 0.1,0.3, and 0.5. The tests were conducted in the applied stress intensity range (Delta K) of 10-60 MPa root m at 10 Hz frequency and plots of fatigue crack growth rate (FCGR) versus Delta K were obtained. It has been observed that presence of internal hydrogen leads to enhancement of FCGR by a factor of 2 to 15 depending on the value of Delta K acid R. The enhancement increased with increase in R and Delta K, and was maximum for ail R values around 40 MPa root m. The fractographic features observed using scanning electron microscope (SEM) support the trends in FCGR data. The crack growth enhancement has been found to increase with increase in Delta K upto a value of 40 MPa root m. Around Delta K = 40 MPa root m, where maximum crack growth enhancement due to hydrogen has been observed, the fracture face had prominent cleavage facets compared to a few small regions of cleavage facets at lesser stress intensities. At stress intensities greater than 40 MPa root m inclusion interface separation and formation of microvoids appear to play a significant role on the fatigue fracture process and correspondingly, the role of hydrogen seems to be insignificant. The origin of the cleavage facets and the consequent enhancement in FCGR due to hydrogen is explained on the basis of hydrogen accumulation and transport at the edge crack tip.
引用
收藏
页码:185 / 196
页数:12
相关论文
共 50 条
  • [21] Fatigue crack growth of a metastable austenitic stainless steel
    Martelo, D. F.
    Mateo, A. M.
    Chapetti, M. D.
    INTERNATIONAL JOURNAL OF FATIGUE, 2015, 80 : 406 - 416
  • [22] Influence of TiN Additions on the Microstructure of a Lightweight Fe-Mn-Al Steel
    Penna, Rairu Vaz
    Bartlett, Laura N.
    O'Malley, Ron
    INTERNATIONAL JOURNAL OF METALCASTING, 2020, 14 (02) : 342 - 355
  • [23] Hydrogen isotope effect on the embrittlement and fatigue crack growth of steel
    Connolly, Matthew
    Martin, May
    Amaro, Robert
    Slifka, Andrew
    Drexler, Elizabeth
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 753 : 331 - 340
  • [24] Superplasticity in a lean Fe-Mn-Al steel (vol 8, 2017)
    Han, Jeongho
    Kang, Seok-Hyeon
    Lee, Seung-Joon
    Kawasaki, Megumi
    Lee, Han-Joo
    Ponge, Dirk
    Raabe, Dierk
    Lee, Young-Kook
    NATURE COMMUNICATIONS, 2018, 9
  • [25] Hydrogen Effect on the Fatigue Crack Growth in Austenitic Stainless Steel Investigated by a New Method Based on Nanohardness Distribution
    Huimin Tao
    Yuanjian Hong
    Xingyang Chen
    Chengshuang Zhou
    Jinyang Zheng
    Lin Zhang
    Journal of Materials Engineering and Performance, 2018, 27 : 6485 - 6492
  • [26] Fatigue crack initiation and crystallographic crack growth in an austenitic stainless steel
    Chauvot, C
    Sester, M
    COMPUTATIONAL MATERIALS SCIENCE, 2000, 19 (1-4) : 87 - 96
  • [27] Hydrogen Effect on the Fatigue Crack Growth in Austenitic Stainless Steel Investigated by a New Method Based on Nanohardness Distribution
    Tao, Huimin
    Hong, Yuanjian
    Chen, Xingyang
    Zhou, Chengshuang
    Zheng, Jinyang
    Zhang, Lin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (12) : 6485 - 6492
  • [28] Fatigue crack initiation and crystallographic crack growth in an austenitic stainless steel
    Chauvot, C
    Sester, M
    ADVANCES IN MECHANICAL BEHAVIOUR, PLASTICITY AND DAMAGE, VOLS 1 AND 2, PROCEEDINGS, 2000, : 955 - 960
  • [29] CORROSION OF FE-MN-AL ALLOYS
    BENTLEY, AP
    FOURIE, JW
    ALTSTETTER, C
    JOURNAL OF METALS, 1985, 37 (11): : A42 - A42
  • [30] Microstructures and mechanical properties evaluation of hard chromized austenitic Fe-Mn-Al alloys
    Lee, JW
    APPLIED SURFACE SCIENCE, 2005, 244 (1-4) : 248 - 251