Effect of TiC addition on structure and properties of spark plasma sintered ZrB2-SiC-TiC ultrahigh temperature ceramic composite

被引:34
|
作者
Sengupta, Pradyut [1 ,2 ]
Sahoo, Siba Sundar [1 ]
Bhattacharjee, Arjak [1 ]
Basu, Suddhasatwa [2 ,3 ]
Manna, Indranil [1 ]
机构
[1] Indian Inst Technol Kharagpur, Dept Met & Mat Engn, Kharagpur 721302, W Bengal, India
[2] CSIR Inst Minerals & Mat Technol, Bhubaneswar 751013, India
[3] Indian Inst Technol Delhi, Dept Chem Engn, New Delhi 110016, India
关键词
TiC; ZrB2; SiC; Density; Microstructure; Mechanical properties; MECHANICAL-PROPERTIES; ZIRCONIUM DIBORIDE; OXIDATION BEHAVIOR; FRACTURE-TOUGHNESS; CARBON NANOTUBE; MICROSTRUCTURE; ZRB2; CARBIDE; STRENGTH; DENSIFICATION;
D O I
10.1016/j.jallcom.2020.156668
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, the role of 5 and 10 vol% TiC addition on densification, microstructure, phase evolution and mechanical properties of ZrB2-20 vol% SiC composite has been investigated maintaining the volume fraction of SiC constant. It is found that TiC addition reduces the spark plasma sintering (SPS) temperature from 1900 degrees C to 1700 degrees C producing in a nearly fully dense (similar to 99.6% theoretical density) material and forming (Zr,Ti)B-2, a mixed compound of Zr and Ti. The lattice parameters (c and a) of (Zr,Ti)B-2 are found to lie between that of pure ZrB2 and TiB2 with its c/a ratio varying inversely with the extent of TiC addition. Phase and microstructure analyses reveal that, while the entire amount of TiC dissolves in ZrB2 in the ZrB2-20SiC-5TiC (vol%), undissolved TiC exist in the ZrB2-20SiC-10TiC (vol%) composite after sintering indicating that the solubility limit of TiC in sintered ZrB2 lies in between 5 and 10 vol%. The elastic modulus values of the TiC added composites predicted by model based calculation agree well with the values experimentally determined by nano-indentation suggesting that these sintered composites are highly dense and nearly defect-free. The calculated residual stress of the matrix phase (using appropriate analytical models) was found to be tensile in nature but decreasing with increase in TiC addition. The residual stress of the reinforcement phase manifests similar trend but is compressive in nature. Compared to the conventional ZrB2-20SiC (vol%) composite, TiC added composites record better bulk and nano-mechanical properties (e.g., hardness, indentation fracture toughness, flexural strength, stiffness and elastic modulus) at ambient temperature indicating that the ZrB2-SiC-TiC system is a more promising ultrahigh temperature ceramics than the base composite. (C) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Spark plasma sintering of ceramic matrix composite of TiC: microstructure, densification, and mechanical properties: a review
    Samson D. Oguntuyi
    Oluwagbenga T. Johnson
    Mxolisi B. Shongwe
    The International Journal of Advanced Manufacturing Technology, 2021, 116 : 69 - 82
  • [22] Strengthening of TiC ceramics sintered by spark plasma via nano-graphite addition
    Fattahi, Mehdi d
    Babapoor, Aziz
    Delbari, Seyed Ali
    Ahmadi, Zohre
    Namini, Abbas Sabahi
    Asl, Mehdi Shahedi
    CERAMICS INTERNATIONAL, 2020, 46 (08) : 12400 - 12408
  • [23] Role of nano-diamond addition on the characteristics of spark plasma sintered TiC ceramics
    Thang Phan Nguyen
    Pazhouhanfar, Yaghoub
    Delbari, Seyed Ali
    Quyet Van Lee
    Shaddel, Shahrzad
    Namini, Abbas Sabahi
    Shokouhimehr, Mohammadreza D.
    Asl, Mehdi Shahedi
    DIAMOND AND RELATED MATERIALS, 2020, 106
  • [24] Effect of tantalum addition on microstructure and oxidation of spark plasma sintered ZrB2-20vol% SiC composites
    Thimmappa, Sravan Kumar
    Golla, Brahma Raju
    CERAMICS INTERNATIONAL, 2019, 45 (11) : 13799 - 13808
  • [25] Effect of SiC and MgO addition on mechanical and ablation characteristics of spark plasma sintered ZrB2-based composites
    Ankur Sharma
    Dagarapu Benny Karunakar
    Journal of Materials Science, 2022, 57 : 15354 - 15373
  • [26] Densification behavior and mechanical properties of spark plasma-sintered ZrC–TiC and ZrC–TiC–CNT composites
    Ramazan Burak Acicbe
    Gultekin Goller
    Journal of Materials Science, 2013, 48 : 2388 - 2393
  • [27] Effect of SiC and MgO addition on mechanical and ablation characteristics of spark plasma sintered ZrB2-based composites
    Sharma, Ankur
    Karunakar, Dagarapu Benny
    JOURNAL OF MATERIALS SCIENCE, 2022, 57 (32) : 15354 - 15373
  • [28] Effect of Mo and TiC addition on the microstructure and mechanical properties of spark plasma sintered Si3N4 composites
    Ma, Zhiyuan
    Cheng, Huichao
    Fan, Jinglian
    Wang, Zhenwei
    Liu, Zhanggen
    CERAMICS INTERNATIONAL, 2022, 48 (15) : 22362 - 22369
  • [29] The fabrication and mechanical properties of SiC/ZrB2 laminated ceramic composite prepared by spark plasma sintering
    Wang, Hailong
    Fan, Bingbing
    Feng, Lun
    Chen, Deliang
    Lu, Hongxia
    Xu, Hongliang
    Wang, Chang-An
    Zhang, Rui
    CERAMICS INTERNATIONAL, 2012, 38 (06) : 5015 - 5022
  • [30] Investigation of the Properties of SiC-ZrB2-Based Ceramic Composite Materials Obtained by Spark Plasma Sintering
    Shchegoleva, N. E.
    Evdokimov, S. A.
    Modin, S. Yu.
    Karachevtsev, F. N.
    GLASS AND CERAMICS, 2018, 75 (7-8) : 253 - 257