Properties of hydraulic paste of basic oxygen furnace slag

被引:52
|
作者
Belhadj, Essia [1 ]
Diliberto, Cecile [1 ]
Lecomte, Andre [1 ]
机构
[1] Nancy Univ, UMR UPVM CNRS 7198, Inst Jean Lamour, IUT Nancy Brabois,CP2S 207, F-54601 Villers Les Nancy, France
来源
关键词
BOF slag; Hydraulic paste; Valorization; Activation; PHYSICAL-PROPERTIES; EXPANSION;
D O I
10.1016/j.cemconcomp.2013.09.016
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Basic Oxygen Furnace (BOF) slags are by-products of the conversion of pig iron to steel. They mainly contain C2S, C2F, Fe1-xO, CaO, Ca(OH)(2) and CaCO3. According to their chemical composition they are a valuable mineral resource as additions in certain hydraulic binders. This paper presents a hydration study of the BOF slag pastes preserved at different temperatures and in different environments. Pastes are characterized by X-ray diffraction and scanning electron microscopy. The compressive strengths of hydrated pastes are given at 7, 28, 90 and 190 days. Results show that - BOF slags containing 40% of C2S - have attractive mechanical properties. Hydration tests under water showed a pastes swelling due to the hydration of CaO contained in BOF slags. A lime extinction procedure was proposed as alternative to standard PR NF EN 13282-2. This approach is more effective for these materials: the volume expansion of pastes cured in water is avoided and the compressive strengths are thus significantly improved. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:15 / 21
页数:7
相关论文
共 50 条
  • [41] Sodium oxalate activation of basic oxygen furnace slag for building materials
    Santos, Winnie Franco
    Botterweg, Jan-Joost
    Figueiredo, Stefan Chaves
    Schollbach, Katrin
    van der Laan, Sieger
    Brouwers, H. J. H.
    RESOURCES CONSERVATION AND RECYCLING, 2023, 198
  • [42] CHARACTERISTICS OF BASIC OXYGEN FURNACE SLAGS USING PREPARED MOLTEN SLAG
    YUGOV, PI
    PAK, YA
    RYLNIKOVA, AG
    STEEL IN THE USSR, 1980, 10 (03): : 128 - 129
  • [43] Adsorption of acid black 1 wastewater by basic oxygen furnace slag
    Li, YS
    Chiou, CS
    Shieh, YS
    BULLETIN OF ENVIRONMENTAL CONTAMINATION AND TOXICOLOGY, 2000, 64 (05) : 659 - 665
  • [44] Applied Mineralogical Investigation on the Nature of Phosphorous in the Basic Oxygen Furnace Slag
    Sunil Kumar Tripathy
    D. S. Rao
    C. Eswaraiah
    D. Sahoo
    Transactions of the Indian Institute of Metals, 2021, 74 : 2319 - 2334
  • [45] Phosphorus adsorption efficiency and characteristic analysis of basic oxygen furnace slag
    Kuo, Shu-Lung
    Ho, Ching-Lin
    Kao, I-Chan
    INTERNATIONAL JOURNAL OF CHEMICAL KINETICS, 2023, 55 (10) : 642 - 652
  • [46] Applied Mineralogical Investigation on the Nature of Phosphorous in the Basic Oxygen Furnace Slag
    Tripathy, Sunil Kumar
    Rao, D. S.
    Eswaraiah, C.
    Sahoo, D.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2021, 74 (09) : 2319 - 2334
  • [47] Kinetics and, mechanism of hexavalent chromium removal by basic oxygen furnace slag
    Han, Chong
    Jiao, Yanan
    Wu, Qianqian
    Yang, Wangjin
    Yang, He
    Xue, Xiangxin
    JOURNAL OF ENVIRONMENTAL SCIENCES, 2016, 46 : 63 - 71
  • [48] Reduction kinetics of manganese oxide in basic oxygen furnace type slag
    Sohn, HS
    Chen, ZP
    Jung, WG
    STEEL RESEARCH, 2000, 71 (05): : 145 - 152
  • [49] Effects of pH on phosphorus removal capacities of basic oxygen furnace slag
    Han, Chong
    Wang, Zhen
    Yang, Wangjin
    Wu, Qianqian
    Yang, He
    Xue, Xiangxin
    ECOLOGICAL ENGINEERING, 2016, 89 : 1 - 6
  • [50] Sustainable resource conservation through the use of basic oxygen furnace slag
    Nachhaltige ressourcenschonung durch die verwendung von LD-schlacke
    Dohlen, Michael (michael.dohlen@thyssenkrupp.com), 2018, Verlag Stahleisen GmbH (138):