Stress Wave attenuation in SiC3D/Al Composite

被引:0
|
作者
Yuan Chunyuan [1 ]
Wang Yangwei [1 ]
Li Guoju [1 ]
Zhang Xu [1 ]
Gao Jubin [1 ]
机构
[1] Beijing Inst Technol, Sch Mat Sci & Engn, Beijing 100081, Peoples R China
关键词
PROPAGATION; ROCK;
D O I
10.1088/1742-6596/419/1/012055
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
SiC3D/Al composite is a kind of special composite with interpenetrating network microstructure. The attenuation properties of stress wave propagation along the SiC3D/Al composite are studied by a Split Hopkinson Pressure Bar system & FEM simulations, and the attenuation mechanism is discussed in this paper. Results show that the attenuation rate of the stress wave in the composite is up to 1.73MPa . mm(-1). The reduction of the amplitude of waves is caused by that plenty of interfaces between SiC and Al within the composite acting with stress waves. When the incident plane wave reaches the SiC3D/Al interface, reflection wave and transmission wave propagates in different directions along the irregular interface between SiC phase and aluminium phase due to the impedance mismatch of them, which leads to the divergence of stress wave. At the same time, some stress micro-focuses occurs in the aluminium phase for the complex wave superimposition, and some plastic deformation may take place within such micro-regions, which results in the consumption of stress wave energy. In conclusion, the stress wave attenuation is derived from divergence and consumption of stress wave.
引用
收藏
页数:6
相关论文
共 50 条
  • [41] Formation of SiC-Al interface in SiC whisker reinforced Al composite
    Wei, Hongmei
    Xu, Hongyu
    Geng, Lin
    Huang, Yudong
    EMERGING FOCUS ON ADVANCED MATERIALS, PTS 1 AND 2, 2011, 306-307 : 857 - 860
  • [42] ELECTROPHORETIC DEPOSITION OF AL2O3-SIC COMPOSITE
    JEAN, JH
    MATERIALS CHEMISTRY AND PHYSICS, 1995, 40 (04) : 285 - 290
  • [43] β-Sialon-Al2O3-SiC composite refractories
    Huang, ZH
    Sun, JL
    Wang, JX
    Hong, YR
    HIGH-PERFORMANCE CERAMICS 2001, PROCEEDINGS, 2002, 224-2 : 275 - 279
  • [44] MICROCRACKING AND STRENGTH OF AN AL2O3-SIC COMPOSITE
    LANGE, FF
    ARORA, A
    AMERICAN CERAMIC SOCIETY BULLETIN, 1981, 60 (03): : 394 - 394
  • [45] PREPARATION OF SIC-AL2O3 COMPOSITE POWDER
    KIMURA, I
    HOTTA, N
    MATSUDA, G
    SAITO, N
    YASUKAWA, S
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1987, 6 (11) : 1359 - 1360
  • [46] The Bauschinger effect in a SiC/Al composite
    Arsenault, RJ
    Pillai, UTS
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (04): : 995 - 1001
  • [47] Interfacial structure of a SiC/Al composite
    Romero, JC
    Wang, L
    Arsenault, RJ
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 212 (01): : 1 - 5
  • [48] Porosity shrinkage in the Al/SiC composite
    Tomolya, K
    Gácsi, Z
    Pieczonka, T
    MATERIALS SCIENCE, TESTING AND INFORMATICS, 2003, 414-4 : 153 - 158
  • [49] Interfacial structure of a SiC/Al composite
    Univ of Maryland, College Park, United States
    Materials Science and Engineering A, 1996, A212 (01): : 1 - 5
  • [50] Optical microscopy of a 3-D woven SiC/SiC-based composite
    Davies, IJ
    Ishikawa, T
    Shibuya, M
    Hirokawa, T
    COMPOSITES SCIENCE AND TECHNOLOGY, 1999, 59 (03) : 429 - 437