Effect of thickness, translucency, and firing protocol on the masking ability of a CAD/CAM zirconia-reinforced lithium silicate for different backgrounds

被引:0
|
作者
Passos, L. [1 ,2 ]
Linke, B. [3 ]
Street, A. [4 ]
Torrealba, Y. [3 ]
机构
[1] Fed Fluminense Univ, Sch Dent, Hlth Inst Nova Friburgo, Dept Prosthet Dent, Rua Doutor Silvio Henrique Braune 22, BR-28625650 Nova Friburgo, RJ, Brazil
[2] Univ Alberta, Edmonton Clin Hlth Acad, Fac Med & Dent, Dept Dent,Sch Dent, Edmonton, AB, Canada
[3] Univ Alberta, Edmonton Clin Hlth Acad, Fac Med & Dent, Sch Dent, Edmonton, AB, Canada
[4] Pontifical Catholic Univ Rio de Janeiro, Sch Engn, Elect Engn Dept, Rio De Janeiro, Brazil
关键词
color; spectrophotometry; computer-aided design/computer-aided manufacturing (CAD/CAM); zirconia-reinforced lithium silicate (ZLS) glass-ceramic; visual perception; CERAMIC THICKNESS; COLOR; SHADE; ACCEPTABILITY; RESIN;
D O I
暂无
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the masking ability of computer-aided design/computer-aided manufacturing (CAD/CAM) zirconia-reinforced lithium silicate (ZLS) glass-ceramic under the different material configurations of thickness, translucency, and finishing protocol as well as significance of the color difference due to the manufacturer's one-firing protocol. Materials and methods: Ninety high-translucency (HT) and low-translucency (LT) ZLS glass-ceramic discs of different thicknesses (1.0, 1.5, and 2.0 mm) were evaluated as a monolithic structure with and without the use of a one-firing protocol. Disc samples were placed onto the substrates for measurement; a spectrophotometer measured the L*, a*, and b* color attributes of each specimen. Delta E value was calculated for determining color differences in tooth-colored substrate specimens (shade B1) compared with three darker backgrounds (shade C2, and two metal substrates - gold and silver). Delta E values were then compared against clinically acceptable (Delta E = 5.5) and ideal (Delta E = 2.6) thresholds. Color differences between the control and test groups were evaluated under different effects using a series of one-sided paired t tests (P < 0.01). The 99% confidence interval (CI) for the true Delta E mean and P values are reported and discussed. A complementary regression analysis depicts the effect size of translucency and firing protocol. Results: Over C2, a 1-mm thickness demonstrated P < 0.01 for the clinically acceptable threshold, whereas the ideal threshold was ensured only with P < 0.01 under a 2-mm thickness. Over silver, only the clinically acceptable standard was met with P < 0.01 under a 2-mm thickness. Over gold, a 1-mm thickness was clinically acceptable with P < 0.01, and the ideal standard was met with P < 0.01 under a 1.5-mm thickness. These results remained valid regardless of the firing protocol or translucency; however, significant (P < 0.01) yet small-sized effects were found for translucency and firing protocol over gold, and for translucency over silver, through multiple regression analysis. Conclusions: To achieve ideal masking, the minimum thickness of CAD/CAM ZLS glass-ceramic should be 1.5 mm over a gold background, and 2 mm over a C2 background. The silver background did not achieve ideal masking in any situation. The one-firing protocol did not affect the final color and can be used to increase restoration strength.
引用
下载
收藏
页码:29 / 38
页数:10
相关论文
共 50 条
  • [31] Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: Effect of ceramic thickness
    Monteiro, Jaiane Bandoli
    Riquieri, Hilton
    Prochnow, Catina
    Guilardi, Luis Felipe
    Rocha Pereira, Gabriel Kalil
    Souto Borges, Alexandre Luiz
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    DENTAL MATERIALS, 2018, 34 (06) : 891 - 900
  • [32] Effect of incisal preparation design on the fracture strength of monolithic zirconia-reinforced lithium silicate laminate veneers
    Jurado, Carlos A.
    Sadid-Zadeh, Ramtin
    Watanabe, Hidehiko
    Robbins, Craig E.
    Afrashtehfar, Kelvin I.
    Fischer, Nicholas G.
    Lee, Damian J.
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2024, 33 (03): : 281 - 287
  • [33] Effect of self-etching ceramic primer on bond strength of zirconia-reinforced lithium silicate ceramics
    Awad, Mohamed M.
    Al Jeaidi, Zaid A.
    Almutairi, Nader
    Vohra, Fahim
    Oezcan, Mutlu
    Alrahlah, Ali
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2020, 34 (01) : 91 - 101
  • [34] Effect of CAD/CAM Ceramic Thickness on Shade Masking Ability of Discolored Teeth: In Vitro Study
    Ellakany, Passent
    Madi, Marwa
    Aly, Nourhan M.
    Al-Aql, Zainb S.
    AlGhamdi, Maher
    AlJeraisy, Abdulrahman
    Alagl, Adel S.
    INTERNATIONAL JOURNAL OF ENVIRONMENTAL RESEARCH AND PUBLIC HEALTH, 2021, 18 (24)
  • [35] Survival probability of zirconia-reinforced lithium silicate ceramic: Effect of surface condition and fatigue test load profile
    de Oliveira Dal Piva, Amanda Maria
    Mendes Tribst, Joao Paulo
    Venturini, Andressa Borin
    Anami, Lilian Costa
    Bonfante, Estevam Augusto
    Bottino, Marco Antonio
    Kleverlaan, Cornelis Johannes
    DENTAL MATERIALS, 2020, 36 (06) : 808 - 815
  • [36] Colour agreement between try-in paste and resin cement: effect of background on zirconia-reinforced lithium silicate
    Paken, G.
    Yildirim, B.
    Unal, M.
    Tekeli, A.
    Kirarslan, O.
    AUSTRALIAN DENTAL JOURNAL, 2021, 66 (04) : 406 - 412
  • [37] Effect of Two Different Intraoral Polishing Systems on Surface Roughness, Color Stability, and Bacterial Accumulation of Zirconia-Reinforced Lithium Silicate Ceramic
    Makkeyah, Fatma
    Moustafa, Dina Mohamed
    Bakr, Mahmoud M.
    Al Ankily, Mahmoud
    EUROPEAN JOURNAL OF DENTISTRY, 2024,
  • [38] Staining and bleaching susceptibility of zirconia-reinforced lithium silicate glass-ceramics with different thicknesses, translucencies, and fabrication methods
    Al-Johani, Hanan
    Alhotan, Abdulaziz
    Alhijji, Saleh
    Silikas, Nick
    Satterthwaite, Julian
    JOURNAL OF PROSTHETIC DENTISTRY, 2024, 131 (03): : 530.e1 - 530.e11
  • [39] SEM Evaluation of the Marginal Gap of Zirconia-Reinforced Lithium Silicate Full Crowns and the Effect of Post Crystallization: An In Vitro Study
    Shely, Asaf
    Lugassy, Diva
    Anufriev, Maxim
    Nissan, Joseph
    Rauchwerger, Olisya
    Ben-Izhack, Gil
    DENTISTRY JOURNAL, 2024, 12 (03)
  • [40] Masking ability of CAD/CAM monolithic ceramics: effect of ceramic type and thickness, and try-in paste shade
    Fachinetto, Eduarda
    Chiapinotto, Gratcheva Falcao
    Barreto, Valentina Soares Menna
    Pecho, Oscar
    Pereira, Gabriel Kalil Rocha
    Bacchi, Atais