Effects of Dynamic Strain Hardening Exponent on Abnormal Cleavage Fracture Occurring During Drop Weight Tear Test of API X70 and X80 Linepipe Steels

被引:22
|
作者
Kang, Minju [1 ]
Kim, Hyunmin [1 ]
Lee, Sunghak [1 ,2 ]
Shin, Sang Yong [3 ]
机构
[1] Pohang Univ Sci & Technol, Ctr Adv Aerosp Mat, Pohang 790784, South Korea
[2] Pohang Univ Sci & Technol, Pohang 790784, South Korea
[3] Univ Ulsan, Sch Mat Sci & Engn, Ulsan 680749, South Korea
关键词
LOW-CARBON; IMPACT PROPERTIES; ACICULAR FERRITE; STRENGTH STEELS; MICROSTRUCTURE; PHASE; BEHAVIOR; TENSILE; RATES; SHAPE;
D O I
10.1007/s11661-013-2046-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, drop weight tear tests (DWTT) were conducted on API X70 and X80 linepipe steels fabricated with various compositions and rolling and cooling conditions in order to correlate the strain hardening with the abnormal cleavage fracture occurring in the hammer-impacted area. Area fractions of fracture modes were measured from fractured DWTT specimens, and the measured data were analyzed in relation to microstructures, Charpy impact energy, and strain hardening. All the steels consisted of fine acicular ferrite, together with some bainitic ferrite, granular bainite, and martensite-austenite constituent. As the volume fraction of acicular ferrite increased, the area fraction of DWTT abnormal cleavage fracture decreased because the toughness of acicular ferrite was higher than other microstructures. The area fraction of abnormal cleavage fracture was weakly related with strain hardening exponents obtained from the quasi-static tensile and compressive tests, but showed better correlation with those obtained from the dynamic compressive test. This tendency could be more clearly observed when steels having similar Charpy impact energy levels were grouped. Since the DWTT was performed under a dynamic loading condition, thus, the abnormal cleavage fracture behavior should be related with the strain hardening analyzed under a dynamic loading condition. (C) The Minerals, Metals & Materials Society and ASM International 2013
引用
收藏
页码:682 / 697
页数:16
相关论文
共 33 条
  • [31] Effects of Oxides on Tensile and Charpy Impact Properties and Fracture Toughness in Heat Affected Zones of Oxide-Containing API X80 Linepipe Steels
    Hyo Kyung Sung
    Seok Su Sohn
    Sang Yong Shin
    Kyung Shik Oh
    Sunghak Lee
    Metallurgical and Materials Transactions A, 2014, 45 : 3036 - 3050
  • [32] Correlation of crack-tip opening angle for stable crack propagation with charpy and drop-weight tear test properties in high-toughness API X70 pipeline steels
    Byoungchul Hwang
    Sang Yong Shin
    Sunghak Lee
    Nack J. Kim
    Sangho Kim
    Ki Bong Kang
    Metallurgical and Materials Transactions A, 2006, 37 : 371 - 380
  • [33] Correlation of crack-tip opening angle for stable crack propagation with charpy and drop-weight tear test properties in high-toughness API X70 pipeline steels
    Hwang, B
    Shin, SY
    Lee, S
    Kim, NJ
    Kim, S
    Kang, KB
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (02): : 371 - 380