A study on HVOF coatings of micron and nano WC-Co powders

被引:78
|
作者
Cho, T. Y. [1 ]
Yoon, J. H. [1 ]
Kim, K. S. [1 ]
Song, K. O. [1 ]
Joo, Y. K. [1 ]
Fang, W. [1 ]
Zhang, S. H. [1 ]
Youn, S. J. [2 ]
Chun, H. G. [3 ]
Hwang, S. Y. [4 ]
机构
[1] Changwon Natl Univ, Sch Nano Adv Mat Engn, Chang Won 641773, South Korea
[2] Sermatech Korea, Chang Won, South Korea
[3] Univ Ulsan, Sch Mat Sci & Engn, Ulsan, South Korea
[4] RIST, Minist Sci & Technol, 21st Century Frontier R&D Programs, Ctr Nanostructured Mat Technol, Pohang 790330, South Korea
来源
SURFACE & COATINGS TECHNOLOGY | 2008年 / 202卷 / 22-23期
关键词
HVOF coating; WC-Co powder; Hardness; Friction coefficient; Adhesive wear;
D O I
10.1016/j.surfcoat.2008.06.106
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
High velocity oxy-fuel (HVOF) spray coating of micron (m) and nano (n) WC-Co powders has been studied for the improvement of durability of sliding machine components (SMC). In this work, optimal coating process (OCP) is obtained from the best surface properties of coating prepared by the Taguchi program. Hardness of coating is strongly dependent on powder size and spray parameters (SP) because of their strong influence on in-flight parameters. Hardness of n WC-Co is lower than that of m WC-Co since the degree of hard WC decomposition to less hard W2C, W and graphite is larger due to the larger specific surface area. Coating is porous since the decomposed graphite forms carbon oxide gasses by reaction with excess oxygen, and the gas evolution from coating makes porous coating. Porosity of n WC-Co coating is larger than that of m WC-Co because of larger evolution of carbon oxide gasses through n WC-Co coating. Friction coefficient (FC) is strongly dependent on the coating process (CP) since hardness and porosity of coating are dependent on the CP. FC of n WC-Co is lower than that of m WC-Co both at 25 degrees C and 500 degrees C, because of the more decomposition of n WC-Co. FC increases with increasing coating temperature (CT) from 25 degrees C to 500 degrees C both at in and n WC-Co because of the increase of adhesion by increasing surface temperature. WC-Co coating is very protective for the machine component since hardness of the coating is 2-3 times higher than those of machine component materials. Stick friction on WC-Co coating Surface occurs easily at higher temperature due to the higher FC at the higher temperature. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:5556 / 5559
页数:4
相关论文
共 50 条
  • [11] Fatigue cracks in HVOF thermally sprayed WC-Co coatings
    Watanabe, S
    Tajiri, T
    Sakoda, N
    Amano, J
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 1998, 7 (01) : 93 - 96
  • [12] Mechanical and tribocorrosion properties of HVOF sprayed WC-Co coatings
    Valentinelli, L
    Valente, T
    Casadei, F
    Fedrizzi, L
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2004, 39 (04) : 301 - 307
  • [13] Pack boronizing of HVOF-sprayed WC-Co coatings
    Niinobe, K
    Watanabe, S
    Itakura, K
    Sakoda, N
    Tajiri, T
    Thermal Spray 2004: Advances in Technology and Application, Proceedings, 2004, : 895 - 897
  • [14] Nanostructured wear resistant WC-Co coatings deposited by HVOF
    Bartuli, C
    Valente, T
    Cipri, F
    Bemporad, E
    SURFACE ENGINEERING: COATING AND HEAT TREATMENTS, PROCEEDINGS, 2003, : 480 - 487
  • [15] Characterization of WC-Co coatings using HP/HVOF process
    Hwang, SY
    Seong, BG
    Kim, MC
    THERMAL SPRAY: PRACTICAL SOLUTIONS FOR ENGINEERING PROBLEMS, 1996, : 107 - 112
  • [16] Fatigue cracks in HVOF thermally sprayed WC-Co coatings
    Watanabe S.
    Tajiri T.
    Sakoda N.
    Amano J.
    Journal of Thermal Spray Technology, 1998, 7 (1) : 93 - 96
  • [17] Pack boronizing of HVOF-sprayed WC-Co coatings
    ASM Thermal Spray Society, TSS; Deutscher Verband fuer Schweisstechnik, DVS; International Welding Institute, IIW; ASM International (ASM International):
  • [18] Fatigue cracks in HVOF thermally sprayed WC-Co coatings
    Watanabe S.
    Amano J.
    Tajiri T.
    Sakoda N.
    Journal of Thermal Spray Technology, 1998, 7 (1) : 93 - 96
  • [19] Deposition of WC-Co Coatings by a Novel High Pressure HVOF
    Bo Sun
    Hirokata Fukanuma
    Journal of Thermal Spray Technology, 2013, 22 : 263 - 271
  • [20] Rietveld analysis for studying the decarburisation in HVOF WC-CO coatings
    Bouaricha, Salim
    Ouchene, Amina
    Legoux, Jean-Gabriel
    SURFACE ENGINEERING, 2018, 34 (10) : 747 - 754