Effect of Non-Thermal Atmospheric Pressure Plasma (NTP) and Zirconia Primer Treatment on Shear Bond Strength between Y-TZP and Resin Cement

被引:23
|
作者
Ahn, Jong-Ju [1 ]
Kim, Dae-Sung [1 ]
Bae, Eun-Bin [1 ]
Kim, Gyoo-Cheon [2 ,3 ]
Jeong, Chang-Mo [1 ]
Huh, Jung-Bo [1 ]
Lee, So-Hyoun [1 ]
机构
[1] Pusan Natl Univ, Dent Res Inst, Dent & Life Sci Inst, Dept Prosthodont, Yangsan 50612, South Korea
[2] Pusan Natl Univ, Sch Dent, Dept Oral Anat & Cell Biol, Yangsan 50612, South Korea
[3] FEAGLE Corp, Res & Dev Ctr, Yangsan 50614, South Korea
基金
新加坡国家研究基金会;
关键词
non-thermal atmospheric pressure plasma (NTP); yttria-stabilized tetragonal zirconia polycrystal; surface treatment; zirconia primer; sandblasting; dentistry; bonding; SURFACE CHARACTERIZATION; COMPOSITE RESIN; ADHESION; RESTORATIONS; POLYCRYSTAL; CERAMICS;
D O I
10.3390/ma13183934
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The purpose of this study was to investigate the effect of non-thermal atmospheric pressure plasma (NTP) treatment on the sandblasting of mechanical method and zirconia primer of chemical method used to increase the bond strength between zirconia and resin cement. In this study, Y-TZP was divided into 4 groups according to the surface treatment methods as follows: Zirconia primer (Pr), NTP + Zirconia primer (NTP + Pr), Sandblasting + Zirconia primer (Sb + Pr), Sandblasting + NTP + Zirconia primer (Sb + NTP + Pr). Then, two types of resin cement (G-CEM LinkAce and Rely X-U200) were used to measure the shear bond strength (SBS) and they were divided into non-thermal cycling group and thermal cycling group for aging effect. Statistical analyses were performed using the Kruskal-Wallis test and Mann-Whitney U test. The result of the surface energy (SE), there was no significant difference among the groups (p> 0.05). As a result of the SBS test, the Sb + Pr group had a significantly higher SBS value than the other groups regardless of the resin cement type (p< 0.05), and the decrease rate after thermal cycling treatment was the lowest. On the other hand, the NTP + Pr group showed significantly lower SBS values than the other groups except for the case of using Rely X-U200 (p< 0.05), and the reduction rate after thermal cycling was the highest. The Sb + NTP + Pr group did not differ significantly from the Pr group (p> 0.05). Within the limitations of two successive studies, treatment with NTP after sandblasting used for mechanical bond strength showed a positive effect on initial SBS. However, when NTP was treated before the zirconia primer used for the chemical bond strength, it showed a negative effect on SBS compared to other treatment methods, which was noticeable after the thermal cycling treatment.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Influence of Applied Pressure and Thickness Variation on the Bond Strength Between 3Y-TZP Zirconia and Self-Adhesive Resin Cement
    Pinto, Paulo
    Carvalho, Oscar
    Ferreira, Rita
    Madeira, Sara
    Silva, Filipe S.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2025, 113 (03)
  • [32] The Effect of Surface Treatment on Shear Bond Strength between Y-TZP and Veneer Ceramic: A Systematic Review and Meta-Analysis
    de Mello, Caroline Cantieri
    Bitencourt, Sandro Basso
    dos Santos, Daniela Micheline
    Pesqueira, Aldieris Alves
    Pellizzer, Eduardo Piza
    Goiato, Marcelo Coelho
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2018, 27 (07): : 624 - 635
  • [33] Effects of 10-MDP Based Primer on Shear Bond Strength between Zirconia and New Experimental Resin Cement
    Valente, Francesco
    Mavriqi, Luan
    Traini, Tonino
    MATERIALS, 2020, 13 (01)
  • [34] Shear Bond Strength of MDP-Containing Self-Adhesive Resin Cement and Y-TZP Ceramics: Effect of Phosphate Monomer-Containing Primers
    Ahn, Jin-Soo
    Yi, Young-Ah
    Lee, Yoon
    Seo, Deog-Gyu
    BIOMED RESEARCH INTERNATIONAL, 2015, 2015
  • [35] Evaluation of Self-adhesive Resin Cement Bond Strength to Yttria-stabilized Zirconia Ceramic (Y-TZP) Using Four Surface Treatments
    Miragaya, Luciana
    Maia, Luciane Cople
    Sabrosa, Carlos Eduardo
    de Goes, Mario Fernando
    da Silva, Eduardo Moreira
    JOURNAL OF ADHESIVE DENTISTRY, 2011, 13 (05): : 473 - 480
  • [36] The effect of environmental pressure changes on the bond strength between zirconia ceramic and adhesive resin cement
    Ata, Secil Ozkan
    Akay, Canan
    Ata, Nazim
    AIRCRAFT ENGINEERING AND AEROSPACE TECHNOLOGY, 2022, 94 (08): : 1336 - 1343
  • [37] High shear bond strength between zirconia ceramic and resin cement via surface treatment and cleaning
    Rui, Li
    Ma, Shi Qing
    Liu, Zi Hao
    Chen, Mei Ling
    Liu, Juan
    Wu, Jie
    Wang, Chen
    Liu, Zhen
    Guo, Zi Ge
    Lu, Rui Jie
    Sun, Ying Cun
    MATERIALS RESEARCH EXPRESS, 2021, 8 (10)
  • [38] Effect of hot-etching treatment duration on the shear bond strength of zirconia-to-resin cement
    Lv, Pin
    Yang, Xin
    Jiang, Ting
    DENTAL MATERIALS JOURNAL, 2023, 42 (05) : 641 - 645
  • [39] The Effect of Multiple Applications of Phosphate-Containing Primer on Shear Bond Strength between Zirconia and Resin Composite
    Klaisiri, Awiruth
    Maneenacarith, Apichai
    Jirathawornkul, Nicha
    Suthamprajak, Panattha
    Sriamporn, Tool
    Thamrongananskul, Niyom
    POLYMERS, 2022, 14 (19)
  • [40] Improved resin-to-dentin bond strength and durability via non-thermal atmospheric pressure plasma drying of etched dentin
    Han, Geum-Jun
    Kim, Jun-Min
    Cho, Byeong-Hoon
    Hwang, Yunchan
    Kim, Hae-Young
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2019, 127 (02) : 170 - 178