An investigative study on the performance of twist roll machine in a continuous cold strip rolling mill

被引:0
|
作者
Mostashfi, Amir [1 ]
Kadkhodaei, Mahmoud [1 ]
Poursina, Mehrdad [2 ]
Bakhshi, Saeid R. [3 ]
机构
[1] Isfahan Univ Technol, Dept Mech Engn, Esfahan 8415683111, Iran
[2] Univ Isfahan, Dept Mech Engn, Fac Engn, Esfahan, Iran
[3] Malek Ashtar Univ Technol, Dept Mat Engn, Esfahan, Iran
关键词
Twist roll; continuous rolling; wear; guide roller; strip defect; WEAR BEHAVIOR; FRICTION; POLYMERS;
D O I
10.1177/0954406212469149
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In many modern continuous production lines of steel sheets, a twist roll machine is used to change the strip direction for shortening the production line. A twist roll machine typically consists of a cylindrical body on which some guide rollers are mounted in rows to gradually change the traveling direction of the strip when passes over the guide rollers. In this article, quality of the sheets after exiting an industrial twist roll machine is first investigated. The amount and distribution of wear on the guide rollers are also assessed by measuring and comparing diameter at different sections of selected worn and new guide rollers. The specific wear rate as well as friction coefficient for guide rollers made of two different popular polymers is measured by pin-on-disk wear tests. Details of the strip path on the twist roll machine as well as contact between the strip and all the guide rollers are specified, and stress distribution in strip and the guide rollers is studied by finite element analysis. Effects of the guide rollers material and arrangement, the bridle rolls tension, and width and thickness of the strip on the amount and distribution of wear on the guide rollers as well as the elasto-plastic response of the strip are studied. The results are utilized to propose techniques for reducing defects on the sheet and the guide rollers, and finite element simulations show the effectiveness of these techniques.
引用
收藏
页码:1633 / 1649
页数:17
相关论文
共 50 条
  • [21] Dynamic Strip Thickness Simulation on Five-Stand Cold Continuous Rolling Mill
    SUN Deng-yue1
    2. Baosteel Technology Center
    JournalofIronandSteelResearch(International), 2006, (02) : 30 - 32
  • [22] Roll wear of finishing stands of hot strip rolling mill
    Chen, LS
    Gao, AM
    Huang, CQ
    Lian, JC
    PROCEEDINGS OF THE SECOND INTERNATIONAL SYMPOSIUM ON INSTRUMENTATION SCIENCE AND TECHNOLOGY, VOL 1, 2002, : 816 - 822
  • [23] Development of HOFC Work Roll Curve for Strip Rolling Mill
    Liu, Yuanming
    Hao, Pingju
    Gong, Dianyao
    Xu, Jianzhong
    Di, Hongshuang
    Zhang, Dianhua
    MATERIALS PROCESSING AND MANUFACTURING III, PTS 1-4, 2013, 753-755 : 225 - 229
  • [24] Numerical simulation for shape of cold rolling aluminum strip on 4-high mill with roll shifted
    Wang, HX
    Liu, JJ
    Lian, JC
    Liu, JB
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 1998, 8 (03) : 385 - 391
  • [26] FAILURE OF WORK ROLL OF COLD-ROLLING MILL
    SINHA, AN
    SIVARAMAKRISHNAN, CS
    IRONMAKING & STEELMAKING, 1994, 21 (02) : 154 - 157
  • [27] INVESTIGATION OF ROLL WEAR IN COLD-ROLLING MILL
    NIKOLAEV, VA
    POLUKHIN, VP
    POPOV, GM
    PILIPENKO, SS
    SHEBANITS, EN
    DUBINSKII, BE
    STEEL IN THE USSR, 1982, 12 (09): : 425 - 426
  • [28] Numerical simulation for shape of cold rolling aluminum strip on 4-high mill with roll shifted
    Yanshan Univ, Qinhuangdao, China
    Trans Nonferrous Met Soc China, 3 (385-391):
  • [29] MODERNIZATION OF A BROAD STRIP COLD ROLLING-MILL
    ESPENHAHN, M
    SCHMITZ, H
    UHLIG, E
    WEBER, F
    STAHL UND EISEN, 1977, 97 (22): : 42 - 42
  • [30] STUDY ON STRIP RUPTURE DURING COLD-ROLLING .2. CAUSE OF SMOOTHING ROLL SURFACE DURING COLD-ROLLING CONTINUOUS CAST STEEL
    YASUDA, A
    TSUNOYAMA, K
    KITAMURA, K
    ITO, K
    KUGUMINATO, H
    YANAGISHIMA, F
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1983, 23 (05) : B176 - B176