Effect of adding chromium to Ti-Zr-Ni-V-Mn alloy on its cycle life as an Ni/metal-hydride battery material

被引:5
|
作者
Lee, SF
Wang, YY
Wan, CC
机构
[1] Department of Chemical Engineering, Tsing-Hua University Hsinchu, Hsinchu
关键词
hydrogen absorption; metal-hydride alloys; hydrogen desorption;
D O I
10.1016/S0378-7753(96)02539-6
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Chromium is added to Ti-Zr-Ni-V-based AB(2)-type alloys to investigate its effect on the cycle-life performance of Ni/metal-hydride batteries made from these alloys. It is found that the addition of chromium significantly reduces the discharge capacity although it has only a limited effect on the hydrogen absorption/desorption performance. Presumably, chromium has a negative effect on the discharge kinetics. In addition, chromium controls the dissolution of V and Zr and hence, extends cycle life. An optimal material, Ti0.35Zr0.65Ni1.2V0.6Mn0.2Cr0.2 is identified and prepared. This possesses acceptable performance with respect to both discharge capacity and cycle life.
引用
收藏
页码:165 / 168
页数:4
相关论文
共 50 条
  • [31] Effect of microstructure on the properties of Zr-Mn-V-Ni AB, type hydride electrode alloys
    Song, XY
    Zhang, XB
    Lei, YQ
    Zhang, Z
    Wang, QD
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 1999, 24 (05) : 455 - 459
  • [32] AC impedance behaviour and state-of-charge dependence of Zr0.5Ti0.5V0.6Cr0.2Ni1.2 metal-hydride electrodes
    Rodrigues, S
    Munichandraiah, N
    Shukla, AK
    PROCEEDINGS OF THE INDIAN ACADEMY OF SCIENCES-CHEMICAL SCIENCES, 2001, 113 (5-6): : 527 - 537
  • [33] Microstructure and Electrode Characteristics of Ti-V-Cu-Cr-Ni Metal Hydride Electrode Alloy
    Qiao Yu-Qing
    Zhao Min-Shou
    Wang Li-Min
    RENEWABLE AND SUSTAINABLE ENERGY II, PTS 1-4, 2012, 512-515 : 1933 - +
  • [34] The inner cell, pressure characteristics of sealed type Ni-MH rechargeable battery using Zr-Ti-Mn-V-Ni hydrogen storage alloy as anode
    Kim, DM
    Yu, JS
    Lee, SM
    Jang, KJ
    Lee, JY
    HYDROGEN ENERGY PROGRESS XII, VOLS 1-3, 1998, : 1153 - 1162
  • [35] Effect of copper additive on Zr0.9Ti0.1V0.2Mn0.6Cr0.05Co0.05Ni1.2 alloy anode for nickel-metal hydride batteries
    Hariprakash, B
    Martha, SK
    Shukla, AK
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2003, 33 (06) : 497 - 504
  • [36] Microstructural evolution of body-centered cubic structure related Ti–Zr–Ni phases in non-stoichiometric Zr-based Zr–Ti–Mn–V–Ni hydride electrode alloys
    Xueyan Song
    Yun Chen
    Cesar Sequeira
    Yongquan Lei
    Qidong Wang
    Ze Zhang
    Journal of Materials Research, 2003, 18 : 37 - 44
  • [37] Improvement of hydrogenation sorption properties of Ti0.90V0.30 Mn1.00Ni0.80 for ultra-high pressure metal-hydride compressor
    Charbonnier, V.
    Enoki, H.
    Asano, K.
    Kim, H.
    Sakaki, K.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (75) : 32252 - 32261
  • [38] An enhanced quasicrystalline Ti1.4V0.6Ni alloy electrode modified by uniformly covered RGO for nickel metal hydride battery
    Ding, Nan
    Liu, Wanqiang
    Sun, Lianshan
    Lin, Jin
    Liang, Fei
    Wang, Limin
    INTERMETALLICS, 2020, 127
  • [39] Development of AB2-type Zr-Ti-Mn-V-Ni-Fe hydride electrodes for Ni-MH secondary batteries
    Song, MY
    Ahn, D
    Kwon, I
    Lee, R
    Rim, H
    JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 298 (1-2) : 254 - 260
  • [40] Effect of annealing on the discharge characteristics of a Zr-V-Mn-Ni hydrogen storage alloy
    Lee, SM
    Kim, DM
    Ya, JS
    Jang, KJ
    Lee, JY
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (06) : 1953 - 1957