Corrosion behavior of 316 stainless steel arc parts in liquid lead at 650 °C under high oxygen concentrations

被引:1
|
作者
Wang, Ruizhong [1 ,4 ]
Qiu, Xi [2 ,3 ]
Gao, Shixin [2 ,3 ]
Liu, Weihua [4 ]
Li, Wenjie [2 ,3 ]
Li, Yuanming [2 ,3 ]
Tang, Zhongfeng [1 ,4 ]
机构
[1] Qinghai Univ, Xining 810016, Peoples R China
[2] Sci & Technol Reactor Syst Design Technol Lab, Chengdu 610213, Peoples R China
[3] Nucl Power Inst China, Chengdu 610213, Peoples R China
[4] Chinese Acad Sci, Shanghai Inst Appl Phys, Shanghai 201800, Peoples R China
基金
中国国家自然科学基金;
关键词
MOLECULAR-DYNAMICS SIMULATIONS; STRUCTURAL-MATERIALS; AUSTENITIC STEELS; 20KH13; STEEL; BISMUTH; ALLOY; OXIDATION; LBE; TEMPERATURE; MECHANISM;
D O I
10.1039/d2ra05165f
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The corrosion of 316SS in contact with lead complicates the realization of high coolant temperature. To explore the corrosion behavior at high temperature, the corrosion test of 316SS was performed in liquid lead at a high temperature of 650 degrees C under Ar with oxygen levels of 10(-2) wt% and 10(-5) wt% by the static corrosion method. The mass changes after corrosion were determined; then, the corrosion depth and the oxide product formed were further characterized. A multi-oxide layer was formed on the 316SS alloy surface, and the thickness reached 17.5 mu m over a period of 100 h at the oxygen level of similar to 10(-2) wt%. Fe oxide was the main product in the outer layer; the dense Fe-Cr oxide was formed in the inner layer and lead was isolated from the metal substrate. When the oxygen content was 10(-5) wt%, corrosion by dissolution at a rather high rate was dominant, and the corrosion depth was as high as 50 mu m for 100 h. It is speculated that the oxide layer is also formed at the initial stage but gets dissociated when there is no oxygen supply to sustain the oxide layer with prolonged exposure time. The oxygen content in the cover gas greatly influences the corrosion behavior of 316SS, thus directly affecting the application of 316SS immersed in liquid lead at high temperature.
引用
收藏
页码:32700 / 32707
页数:8
相关论文
共 50 条
  • [31] Influence of surface mechanical attrition treatment (SMAT) on oxidation behavior of 316L stainless steel at 650°C
    Benafia, S.
    Retraint, D.
    Panicaud, B.
    Poussard, J. L. Grosseau
    RESIDUAL STRESSES IX, 2014, 996 : 906 - +
  • [32] A study on corrosion behavior of austenitic stainless steel in liquid metals at high temperature
    Shin, Sang Hun
    Kim, Jong Jin
    Jung, Ju Ang
    Choi, Kyoung Joon
    Bang, In Cheol
    Kim, Ji Hyun
    JOURNAL OF NUCLEAR MATERIALS, 2012, 422 (1-3) : 92 - 102
  • [33] Corrosion-wear behavior of 316L stainless steel under different applied potentials
    Han, Gaofeng
    Jiang, Pengfei
    Wang, Jianzhang
    Yan, Fengyuan
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2017, 69 (02) : 234 - 240
  • [34] Corrosion behavior of additively manufactured AISI 316L stainless steel under atmospheric conditions
    Helbert, Varvara
    Rioual, Stephane
    Le Bozec, Nathalie
    Thierry, Dominique
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2022, 73 (11): : 1833 - 1843
  • [35] Corrosion of 304 stainless steel in static liquid lithium under high vacuum
    Meng, X. C.
    Huang, M.
    Li, C. L.
    Xu, W.
    Sun, Z.
    Qian, Y. Z.
    Li, L.
    Yuan, X. L.
    Huang, J. J.
    Gao, X.
    Li, J. G.
    Zuo, G. Z.
    Hu, J. S.
    NUCLEAR MATERIALS AND ENERGY, 2020, 25
  • [36] Superior corrosion resistance of a slurry FeAl coating on 316LN stainless steel in 550 °C liquid lead-bismuth eutectic
    Wang, Wen
    Zhu, Zhaoguang
    Yang, Liujie
    Lu, Jintao
    Huang, Jinyang
    Tan, Jibo
    Kuang, Wenjun
    CORROSION SCIENCE, 2024, 227
  • [37] Effect of pH on corrosion behavior of 316L stainless steel in hydrogenated high temperature water
    Wang, Jiazhen
    Wang, Jianqiu
    Ming, Hongliang
    Zhang, Zhiming
    Han, En-Hou
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (05): : 580 - 589
  • [38] Stress corrosion cracking behavior of cold-deformed 316 stainless steel in high temperature water
    Corrosion Laboratory for Nuclear Power Materials, Shanghai Jiao Tong University, Shanghai
    200240, China
    不详
    200233, China
    Yuanzineng Kexue Jishu, 11 (1977-1983):
  • [39] Influence of Plastic Deformation on Dissolution Corrosion of Type 316L Austenitic Stainless Steel in Static, Oxygen-Poor Liquid Lead-Bismuth Eutectic at 500°C
    Klok, Oksana
    Lambrinou, Konstantina
    Gavrilov, Serguei
    Stergar, Erich
    Van der Donck, Tom
    Huang, Shuigen
    Tunca, Bensu
    De Graeve, Iris
    CORROSION, 2017, 73 (09) : 1078 - 1090
  • [40] Oxidation behavior of modified SUS316 (PNC316) stainless steel under low oxygen partial pressure
    Sato, I
    Takaki, M
    Arima, T
    Furuya, H
    Idemitsu, K
    Inagaki, Y
    Momoda, M
    Namekawa, T
    JOURNAL OF NUCLEAR MATERIALS, 2002, 304 (01) : 21 - 28