Optimization of mechanical properties of Sn-3.8Ag-0.7Cu alloys by the additions of Bi, In and Ti

被引:11
|
作者
Chen, Youyang [1 ,2 ]
You, Kangdong [2 ]
Yu, Shuting [2 ]
Yang, Tixin [1 ,2 ]
Dong, Ziqiang [2 ]
Zhang, Jincang [2 ]
Jia, Yandong [1 ]
Wang, Gang [1 ,2 ]
Peng, Jubo [3 ]
Cai, Shanshan [3 ]
Luo, Xiaobin [3 ]
Wang, Jiajun [3 ]
Liu, Chen [3 ]
机构
[1] Shanghai Univ, Inst Mat, Shanghai 200444, Peoples R China
[2] Shanghai Univ, Mat Genome Inst, Shanghai 200444, Peoples R China
[3] Yunnan Tin Grp Holding Co Ltd, Kunming 650000, Peoples R China
关键词
Sn-Ag-Cu solder Alloys; Microstructure; Tensile strength; Nanoindentation; LEAD-FREE SOLDER; SN-AG; CREEP-BEHAVIOR; THERMAL-BEHAVIOR; ELASTIC-MODULUS; MICROSTRUCTURE; WETTABILITY; DEFORMATION; JOINTS;
D O I
10.1016/j.pnsc.2022.10.004
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Bi, In and Ti were added to Sn-3.8Ag-0.7Cu (SAC387) solder alloy to optimize the mechanical performance. The alloying effects of Bi, In and Ti on the microstructure, thermal and mechanical properties of SAC387 based solder alloys were investigated. The results demonstrate that adding 3.5 wt % of Bi could refine the microstructure, optimize the thermal properties, and improve the tensile strength. Meanwhile, the ductility of the solder alloys reduced evidently. Adding 2.8 wt % of In into SAC387-3.5 wt %Bi alloy could increase both the strength and ductility, which is attributed to the beneficial effect of In addition, as adding In could improve the solubility of Bi in the beta-Sn matrix. Meanwhile, the melting point was reduced, and the wettability improved with the addition of In. Introducing amounts of Ti into SAC387-3.5 wt % Bi-2.8 wt % In alloy could further increase the strength. However, the ductility was significantly reduced when 0.8 wt % of Ti was added due to the formation of the coarse Ti2Sn3 phase. The undercooling was remarkably reduced with the addition of Ti. The nanoindentation tests demonstrate that the hardness increased mainly due to the hardening effect of the Bi addition. Among all the samples prepared, alloy SAC387-3.5 wt % Bi exhibited the highest creep resistance at the ambient temperature. Further adding In and Ti into SAC387-3.5 wt % Bi alloys reduced the creep resistance of the solder alloys. The mechanism associated with the different mechanical responses is also discussed in this study.
引用
收藏
页码:643 / 654
页数:12
相关论文
共 50 条
  • [21] Viscosity and Electrical Conductivity of the Liquid Sn-3.8Ag-0.7Cu Alloy with Minor Co Admixtures
    A. Yakymovych
    V. Sklyarchuk
    Yu. Plevachuk
    B. Sokoliuk
    Journal of Materials Engineering and Performance, 2016, 25 : 4437 - 4443
  • [22] Viscosity and Electrical Conductivity of the Liquid Sn-3.8Ag-0.7Cu Alloy with Minor Co Admixtures
    Yakymovych, A.
    Sklyarchuk, V.
    Plevachuk, Yu.
    Sokoliuk, B.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (10) : 4437 - 4443
  • [23] 无铅焊料Sn-3.8Ag-0.7Cu的低周疲劳行为
    曾秋莲
    王中光
    冼爱平
    尚建库
    材料研究学报, 2004, (01) : 11 - 17
  • [24] Mechanical property optimization of Sn-1.5Ag-0.5Cu solder alloys with additions of Bi, In, and Te
    Eid, N. A. M.
    El-Daly, A. A.
    Ibrahiem, A. A.
    PHYSICA SCRIPTA, 2024, 99 (06)
  • [25] Nd对Sn-3.8Ag-0.7Cu/Cu焊点高温可靠性的影响
    吴洁
    薛松柏
    于志浩
    Tan Cheeleong
    孙华斌
    徐勇
    焊接学报, 2021, 42 (07) : 9 - 13+97
  • [26] Effects of Microstructure and Loading on Fracture of Sn-3.8Ag-0.7Cu Joints on Cu Substrates with ENIG Surface Finish
    Huang, Z.
    Kumar, P.
    Dutta, I.
    Sidhu, R.
    Renavikar, M.
    Mahajan, R.
    JOURNAL OF ELECTRONIC MATERIALS, 2014, 43 (12) : 4485 - 4496
  • [27] Effects of Microstructure and Loading on Fracture of Sn-3.8Ag-0.7Cu Joints on Cu Substrates with ENIG Surface Finish
    Z. Huang
    P. Kumar
    I. Dutta
    R. Sidhu
    M. Renavikar
    R. Mahajan
    Journal of Electronic Materials, 2014, 43 : 4485 - 4496
  • [28] Interfacial reaction and dissolution behavior of Cu substrate in molten Sn-3.8Ag-0.7Cu in the presence of Mo nanoparticles
    Arafat, M. M.
    Haseeb, A. S. M. A.
    Johan, Mohd Rafie
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2011, 23 (03) : 140 - 149
  • [29] Addition of cobalt nanoparticles into Sn-3.8Ag-0.7Cu lead-free solder by paste mixing
    Tay, S. L.
    Haseeb, A. S. M. A.
    Johan, Mohd Rafie
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2011, 23 (01) : 10 - 14
  • [30] Effect of Aging Time on Interfacial Microstructure of Sn-3.8Ag-0.7Cu Solder Reinforced with Co Nanoparticles
    Tay, S. L.
    Haseeb, A. S. M. A.
    Johan, Mohd Rafie
    2009 INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING (ICEPT-HDP 2009), 2009, : 579 - 585