Fracture load and failure types of different veneered polyetheretherketone fixed dental prostheses

被引:41
|
作者
Taufall, Simon [1 ]
Eichberger, Marlis [1 ]
Schmidlin, Patrick R. [2 ]
Stawarczyk, Bogna [1 ]
机构
[1] Ludwig Maximilians Univ Munchen, Sch Dent, Dept Prosthodont, Goethestr 70, D-80336 Munich, Germany
[2] Univ Zurich, Ctr Dent Med, Clin Prevent Dent Periodontol & Cariol, Zurich, Switzerland
关键词
Fracture load; PEEK; Digital veneering; Veneering resin composite; SHEAR BOND STRENGTH; DIFFERENT SURFACE PRETREATMENTS; RESIN COMPOSITE CEMENTS; BEARING CAPACITY; SULFURIC-ACID; PEEK; IMPLANTS; ADHESIVES; IMPACT; FDPS;
D O I
10.1007/s00784-016-1777-4
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The aim of this study is to investigate the fracture load of different veneered PEEK 3-unit fixed dental prosthesis (FDPs) after different aging regimens. Congruently anatomically shaped 3-unit FDPs were milled using a master stl-data set and randomly divided into four groups (N = 120, n = 30 per veneering group), which were veneered using different veneering methods: (i) digital veneering with breCAM.HIPC, (ii) conventional veneering with crea.lign, (iii) conventional with crea.lign paste, and (iv) using pre-manufactured veneers visio.lign. The FDPs were then adhesively cemented on a metal abutment and fracture loads were measured in a universal testing machine (1 mm/min) before and after aging (10,000 thermal cycles, 5/55 A degrees C). Two- and one-way ANOVA followed by post hoc Scheff, tests were used for data analysis (p < 0.05). This investigation showed an influence of the veneering method on the fracture load results independent of the aging level. The highest fracture load was measured for the FDPs with digital veneering (1882 +/- 152 N at baseline, 2021 +/- 184 N after thermocycling). The remaining groups showed comparable results, and no impact of thermal aging was observed. Digital and conventional veneers showed cracks in the pontic region starting from the connector area as a main failure type after loading, while the pre-manufactured veneers showed predominantly adhesive failures. The digital veneering method showed the highest fracture load resistance. Thermal aging showed no impact on the fracture load of all tested veneered PEEK 3-unit FDPs. According to this study results, reliable veneering of PEEK FDPs can be achieved with digital veneering.
引用
收藏
页码:2493 / 2500
页数:8
相关论文
共 50 条
  • [1] Fracture load and failure types of different veneered polyetheretherketone fixed dental prostheses
    Simon Taufall
    Marlis Eichberger
    Patrick R. Schmidlin
    Bogna Stawarczyk
    Clinical Oral Investigations, 2016, 20 : 2493 - 2500
  • [2] Fracture load of different veneered and implant-supported 4-UNIT cantilever PEEK fixed dental prostheses
    Micovic Soldatovic, Danka
    Liebermann, Anja
    Huth, Karin C.
    Stawarczyk, Bogna
    Journal of the Mechanical Behavior of Biomedical Materials, 2022, 129
  • [3] Fracture load of different veneered and implant-supported 4-UNIT cantilever PEEK fixed dental prostheses
    Soldatovic, Danka Micovic
    Liebermann, Anja
    Huth, Karin C.
    Stawarczyk, Bogna
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2022, 129
  • [4] Comparative fracture behavior of monolithic and veneered zirconia posterior fixed dental prostheses
    Lopez-Suarez, Carlos
    Rodriguez, Veronica
    Pelaez, Jesus
    Agustin-Panadero, Ruben
    Suarez, Maria J.
    DENTAL MATERIALS JOURNAL, 2017, 36 (06) : 816 - 821
  • [5] Polyetheretherketone-A suitable material for fixed dental prostheses?
    Stawarczyk, Bogna
    Beuer, Florian
    Wimmer, Timea
    Jahn, Dirk
    Sener, Beatrice
    Roos, Malgorzata
    Schmidlin, Patrick R.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2013, 101 (07) : 1209 - 1216
  • [6] Fracture Load of Veneered and Monolithic Single-Unit Fixed Dental Prostheses Made from the High-Performance Thermoplastic Polyphenylene Sulfone
    Mayinger, Felicitas
    Eichberger, Marlis
    Schoenhoff, Lisa Marie
    Stawarczyk, Bogna
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2023, 36 (03) : 343 - 353
  • [7] Fracture Load Before and After Veneering Zirconia Posterior Fixed Dental Prostheses
    Rodriguez, Veronica
    Castillo-Oyague, Raquel
    Lopez-Suarez, Carlos
    Gonzalo, Esther
    Pelaez, Jesus
    Suarez-Garcia, Maria-Jesus
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2016, 25 (07): : 550 - 556
  • [8] Static and Fatigue Loading of Veneered Implant-Supported Fixed Dental Prostheses
    Rayyan, Mohammad M.
    Abdallah, Jihad
    Segaan, Lucette G.
    Bonfante, Estevam A.
    Osman, Essam
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2020, 29 (08): : 679 - 685
  • [9] In Vitro Assessment of the Fracture Resistance of Different Prosthodontic Materials for Fixed Dental Prostheses
    Sultan, Sherif El Sayed
    Almuhyi, Nawaf Hussain Saif
    Alzabni, Khalid Maziad
    Alruwaili, Rayan Hamad Qubayl
    JOURNAL OF PHARMACY AND BIOALLIED SCIENCES, 2024, 16 : S2476 - S2478
  • [10] Effects of Different Cavity Designs on Fracture Load of Fiber-reinforced Adhesive Fixed Dental Prostheses in the Anterior Region
    Aktas, Guliz
    Basara, Emine Goncu
    Sahin, Erdal
    Uctasli, Sadullah
    Vallittu, Pekka K.
    Lassila, Lippor V. J.
    JOURNAL OF ADHESIVE DENTISTRY, 2013, 15 (02): : 131 - 135