Effect of Al, Cr and Ta additions on the oxidation behaviour of Nb-Ti-Si in situ composites at 800 °C

被引:166
|
作者
Zelenitsas, K [1 ]
Tsakiropoulos, P [1 ]
机构
[1] Univ Surrey, Met Res Grp, Sch Engn, Surrey GU2 7XH, England
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2006年 / 416卷 / 1-2期
基金
英国工程与自然科学研究理事会;
关键词
silicides; C14 Laves phase; oxidation;
D O I
10.1016/j.msea.2005.10.017
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The oxidation behaviour of as-cast Nb-24Ti-18Si and heat-treated (1500 or 1400 degrees C/100h) Nb-24Ti-18Si-5Al, Nb-24Ti-18Si-5Cr, Nb-24Ti-18Si-5Al-5Cr, Nb-24Ti-18Si-6Ta-5Al-5Cr, Nb-24Ti-18Si-8Cr-4Al and Nb-24Ti-18Si-6Ta-8Cr-4Al (at.%) alloys in static air at 800 degrees C for 100 h has been studied using TG, XRD and EPMA. All the alloys exhibited linear oxidation kinetics. The as-cast (Nb,Ti)(3)Si containing Nb-24Ti-18Si alloy suffered from catastrophic pest oxidation. The other alloys, in which the Nb5Si3 was present, did not pest. Al addition reduced the oxidation rate significantly. Higher oxidation rates and lower adherence of the oxide scale were observed with increase of Cr concentration and/or Ta addition in the Al-containing alloys. In the oxide scales, Si-containing and non-Si-containing oxides of the stoichiometry MO2 were present together with remnants of 5-3 silicide and/or Laves phase. The oxygen solubility in the latter two phases was not high and these phases did not oxidise easily compared to the (Nb,Ti)(ss). Below the oxide scale of the Nb-24Ti-18Si-5Al alloy a thick (similar to 100 mu m) internal oxidation zone was formed where the (Nb,Ti)(ss) contained up to 30 at.% dissolved oxygen. In the Nb-24Ti-18Si-5Cr alloy this zone was thinner and leaner in oxygen. In the Cr- and Al-containing alloys the internal oxidation zone was almost eliminated and the diffusivity of oxygen through the (Nb,Ti)(ss) was reduced owing to the synergy of the Ti, Cr and Al additions, which was not affected by the addition of Ta to the alloy. The presence of Cr-rich C14 silicide Laves phase in the microstructure of some alloys was not beneficial regarding their oxidation at 800 degrees C. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:269 / 280
页数:12
相关论文
共 50 条
  • [31] The effect of Cr and Mo addition on the oxidation behaviour of Ti-46.5Al-3.5Nb-2Cr-0.3B
    Neelam, Naga Sruthi
    Banumathy, S.
    Bhattacharjee, Amit
    NageswaraRao, G. V. S.
    MATERIALS TODAY-PROCEEDINGS, 2019, 15 : 30 - 35
  • [32] EFFECT OF V, MO, AND ZR ADDITIONS ON THE SOLVUS OF THE (NB, TI)CR2 PHASE IN THE NB-TI-AL-CR SYSTEM
    ZHAKHAROV, AM
    PAVLOV, AV
    KARSANOV, GV
    VERGASOVA, LL
    RUSSIAN METALLURGY, 1991, (05): : 208 - 211
  • [33] Effect of tin addition on Nb-Si-based in situ composites. Part II: Oxidation behaviour
    Knittel, S.
    Mathieu, S.
    Portebois, L.
    Vilasi, M.
    INTERMETALLICS, 2014, 47 : 43 - 52
  • [34] Effect of Zr addition on microstructure and oxidation resistance of Nb-Ti-Si base ultrahigh-temperature alloys
    Zeng, Yuxiang
    Guo, Xiping
    Qiao, Yanqiang
    Nie, Zhongyi
    Jinshu Xuebao/Acta Metallurgica Sinica, 2015, 51 (09): : 1049 - 1058
  • [35] EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS
    Zeng Yuxiang
    Guo Xiping
    Qia Yanqiang
    Nie Zhongyi
    ACTA METALLURGICA SINICA, 2015, 51 (09) : 1049 - 1058
  • [36] MICROSTRUCTURE, COMPRESSIVE PROPERTIES AND OXIDATION BEHAVIORS OF THE Nb-Si-Ti-Cr-Al-Ta-Hf ALLOY WITH MINOR HOLMIUM ADDITION
    Wang, Qiaoli
    Xiao, Yinan
    Wu, Di
    Yang, Fang
    Sheng, L. Y.
    ARCHIVES OF METALLURGY AND MATERIALS, 2024, 69 (01) : 181 - 187
  • [37] Effect of Al on oxidation behaviour of Ti-Si eutectic alloys
    Zhan, Y. Z.
    Shi, X. B.
    Yu, Z. W.
    Xu, Y. F.
    Wang, Y.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2007, 42 (03) : 194 - 202
  • [38] Effect of Ta and Zr additions on the oxidation characteristics of Ti-44Al-xNb alloys
    Woo, JC
    Varma, SK
    Mahapatra, RN
    GAMMA TITANIUM ALUMINIDES 2003, 2003, : 585 - 589
  • [39] High-temperature oxidation behaviour of laser in situ synthesised Ti-Al-Cr-Nb alloy coating on Ti-6Al-4V
    Chen, Ting-Ting
    Shi, Yong-Jun
    Li, Xian-Fa
    Wang, Shu-Yao
    Zhao, Xiao-Yu
    MATERIALS AT HIGH TEMPERATURES, 2022, 39 (04) : 290 - 300
  • [40] Effect of Ti/B additions on the formation of Al3Ti of in situ TiB2/Al composites
    Yang, B
    Zhang, JS
    Duan, XJ
    Hu, SC
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 1999, 6 (04): : 285 - 288