Swelling and dissolution of silk fibroin (Bombyx mori) in N-methyl morpholine N-oxide

被引:115
|
作者
Freddi, G
Pessina, G
Tsukada, M
机构
[1] Stn Sperimentale Seta, I-20133 Milan, Italy
[2] Natl Inst Sericultural & Entomol Sci, Tsukuba, Ibaraki 305, Japan
关键词
silk fibroin; N-methyl morpholine N-oxide; dissolution; regeneration; membranes;
D O I
10.1016/S0141-8130(98)00087-7
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
Bombyx mori silk fibers were dissolved in N-methyl morpholine N-oxide (MMNO), an organic cyclic amine oxide used for the solvent spinning of regenerated cellulosic fibers. The commercial MMNO monohydrate used in this study as a solvent for silk is a hygroscopic compound crystalline at room temperature, which becomes an active solvent after melting at 76 degrees C. The degree of hydration of MMNO was checked by DSC measurements. The solvation power of MMNO towards silk fibroin drastically decreased at a water content greater than or equal to 20-21% w/w. Dissolution of silk required both thermal and mechanical energy. The optimum temperature was 100 degrees C. At lower temperatures dissolution proceeded very slowly. At higher temperatures, rapid depolymerization of silk fibroin occurred. The value of the Flory-Huggins interaction parameter chi for the MMNO-H2O-silk fibroin system was - 8.5, suggesting that dissolution is a thermodynamically favored process. The extent of degradation of silk fibroin was assessed by measuring the intrinsic viscosity and determining the amino acid composition of silk after regeneration with an aqueous methanol solution, which was effective in removing the solvent and coagulating silk. Regenerated silk fibroin membranes were characterized by infrared spectroscopy, differential scanning calorimetry and scanning electron microscopy. The prevailing molecular conformation of silk fibroin chains was the beta-sheet structure, as shown by the intense amide I-III bands at 1704, 1627, 1515, 1260, and 1230 cm(-1). The value of the I-1260/I-1230 intensity ratio (crystallinity index) was 0.68, comparable to that of the fibers. The DSC thermogram was characteristic of a silk fibroin material with unoriented beta-sheet crystalline structure, with an intense decomposition endotherm at 294 degrees C. The SEM examination of fractured surfaces showed the presence of a dense microstructure with a very fine texture formed by densely packed roundish particles of about 100-200 nm diameter. (C) 1999 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:251 / 263
页数:13
相关论文
共 50 条
  • [41] Swelling kinetic study with mathematical modeling of cellulose pulp in aqueous N-methyl-morpholine-N-oxide solution
    Anwar J. Sayyed
    Lalaso V. Mohite
    Niteen A. Deshmukh
    Dipak V. Pinjari
    Reaction Kinetics, Mechanisms and Catalysis, 2021, 133 : 101 - 115
  • [42] Dissolution properties of ammonium dinitramide in N-methyl pyrrolidone
    Xiao, Li-Bai
    Zhao, Feng-Qi
    Luo, Yang
    Xing, Xiao-Ling
    Gao, Hong-Xu
    Li, Na
    Li, Xin
    Hu, Rong-Zu
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2014, 117 (01) : 517 - 521
  • [43] Dissolution properties of ammonium dinitramide in N-methyl pyrrolidone
    Li-Bai Xiao
    Feng-Qi Zhao
    Yang Luo
    Xiao-Ling Xing
    Hong-Xu Gao
    Na Li
    Xin Li
    Rong-Zu Hu
    Journal of Thermal Analysis and Calorimetry, 2014, 117 : 517 - 521
  • [44] CIS-N-METHYL-N'-CYCLOHEXYLDIIMIDE N-OXIDE(I) AND CIS-N-CYCLOHEXYL-N'-METHYLDIIMIDE N-OXIDE(II)
    BAKER, MS
    WILLIAMS, DE
    ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL SCIENCE, 1977, 33 (JUL15): : 2325 - 2326
  • [45] UTILIZATION OF N-METHYL-MORPHOLINE N-OXIDE IN DELINEATION OF CAUSTIC-WATER INTERACTIONS ON SUBSTITUENT PLACEMENT IN CARBOHYDRATE POLYMERS
    SENEKER, SD
    GLASS, JE
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1985, 189 (APR-): : 11 - PMSE
  • [46] STUDIES ON DISSOLUTION AND DEFORMATION OF CELLULOSE IN N-METHYLMORPHOLINE N-OXIDE
    TAEGER, E
    MICHELS, C
    NECHWATAL, A
    PAPIER, 1991, 45 (12): : 784 - 788
  • [47] NMR study of silk I structure of Bombyx mori silk fibroin with N-15- and C-13-NMR chemical shift contour plots
    Asakura, T
    Demura, M
    Date, T
    Miyashita, N
    Ogawa, K
    Williamson, MP
    BIOPOLYMERS, 1997, 41 (02) : 193 - 203
  • [48] TERNARY-SYSTEM COMPOSED OF H2O, N-METHYL MORPHOLIN N-OXIDE AND NASCN - ULTRASONIC INVESTIGATION
    BERCHIESI, G
    FARHAT, F
    CASTELLANI, F
    VITALI, G
    JOURNAL OF MOLECULAR LIQUIDS, 1992, 51 (1-2) : 51 - 58
  • [49] Determination of Accurate 1H Positions of (Ala-Gly)n as a Sequential Peptide Model of Bombyx mori Silk Fibroin before Spinning (Silk I)
    Asakura, Tetsuo
    Suzuki, Yu
    Yazawa, Koji
    Aoki, Akihiro
    Nishiyama, Yusuke
    Nishimura, Katsuyuki
    Suzuki, Furitsu
    Kaji, Hironori
    MACROMOLECULES, 2013, 46 (19) : 8046 - 8050
  • [50] Testing the adhesion of paint films to metals by swelling in N-methyl pyrrolidone
    Van Ooij, W.J.
    Edwards, R.A.
    Sabata, A.
    Zappia, J.
    1600, Publ by VSP Int Sci Publ, Zeist, Netherlands (07):