Corrosion behavior of (Zr51.6Cu48.4)93Al7 bulk metallic glass

被引:2
|
作者
Chen, Tie Jun [1 ]
机构
[1] Hebei Vocat & Tech Coll Bldg Mat, Qinhuangdao 066004, Peoples R China
来源
关键词
Bulk metallic glass; Corrosion; Passivate; SUPERCOOLED LIQUID; STABILIZATION; ALLOYS;
D O I
10.4028/www.scientific.net/AMR.479-481.1795
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Corrosion behavior of (Zr51.6Cu48.4)(93)Al-7 bulk metallic glass in 3M HCl, 3M H2SO4, 3M HNO3, 3M NaOH and 3.5 mass%(0.6M)NaCl solutions was studied by immersion test and electrochemical measurements. The bulk metallic glass was spontaneously passivated in the acids, alkali and brine, although it exhibits distinct spontaneous passivation with high passive current density in the Cl-containing solutions. The immersion test indicated, except for 3 M HCl solution, low corrosion rates of the order of 10-2 mm/year for (Zr51.6Cu48.4)(93)Al-7 bulk metallic glass in the other solutions, The quantitative X-ray energy disperse spectroscopy(EDS) analysis revealed that the high corrosion resistance of the bulk metallic glass was due to the formation of aluminium and zirconium-enriched passive film. Corrosion products were mainly copper chloride and oxides in the Cl-containing solutions. The growth mechanism of the passive film is also discussed.
引用
收藏
页码:1795 / 1798
页数:4
相关论文
共 50 条
  • [21] Oxidation behaviour of a Cu-Zr-Al bulk metallic glass
    Tam, C. Y.
    Shek, C. H.
    Wang, W. H.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2008, 18 (02) : 107 - 111
  • [22] Glass Forming Ability and Corrosion Resistance of Zr-Cu- Ni-Al-Ag Bulk Metallic Glass
    Zhou, Wei
    Zhang, Caiwei
    Sheng, Minqi
    Hou, Jixin
    METALS, 2016, 6 (10):
  • [23] Phase separation in Cu43Zr43Al7Ag7 bulk metallic glass
    Oh, JC
    Ohkubo, T
    Kim, YC
    Fleury, E
    Hono, K
    SCRIPTA MATERIALIA, 2005, 53 (02) : 165 - 169
  • [24] Effect of the countermaterial on the tribological behavior of Cu45Zr46Al7Nb2 bulk metallic glass
    Barlemont, Solene
    Colas, Guillaume
    Lenain, Alexis
    Cornuault, Pierre-Henri
    WEAR, 2023, 522
  • [25] Thermal oxidation effect on corrosion behavior of Zr46Cu37.6Ag8.4Al8 bulk metallic glass
    Nie, X. P.
    Yang, X. H.
    Ma, Y.
    Chen, L. Y.
    Yeap, K. B.
    Zeng, K. Y.
    Li, D.
    Pan, J. S.
    Wang, X. D.
    Cao, Q. P.
    Ding, S. Q.
    Jiang, J. Z.
    INTERMETALLICS, 2012, 22 : 84 - 91
  • [26] Dynamic glass transition in Zr-Al-Ni-Cu bulk metallic glass
    Hojo, M.
    Numakura, H.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 442 (1-2): : 268 - 272
  • [27] The Microstructure and Nanocrystallization Behavior of Cu-Zr-Ti-Al Bulk Metallic Glass Matrix Composites
    Zhou, Guorong
    Hur, Boyoung
    Teng, Xinying
    Yue, Xuezheng
    ADVANCED MATERIALS AND PROCESSES II, PTS 1-3, 2012, 557-559 : 228 - +
  • [28] Strain Rate Dependence of Tensile Behavior in Hypoeutectic Zr-Cu-Al Bulk Metallic Glass
    Shirota, Akinori
    Tokunaga, Hitoo
    Fujita, Kazutaka
    Yokoyama, Yoshihiko
    Kimura, Hisamichi
    Inoue, Akihisa
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2008, 72 (09) : 722 - 727
  • [29] In situ observation of pitting corrosion of the Zr50Cu40Al10 bulk metallic glass
    Green, B. A.
    Steward, R. V.
    Kim, I.
    Choi, C. K.
    Liaw, P. K.
    Kihm, K. D.
    Yokoyama, Y.
    INTERMETALLICS, 2009, 17 (07) : 568 - 571
  • [30] Electrochemical corrosion behavior of a Zr-based bulk-metallic glass
    Jiang, W. H.
    Jiang, F.
    Green, B. A.
    Liu, F. X.
    Liaw, P. K.
    Choo, H.
    Qiu, K. Q.
    APPLIED PHYSICS LETTERS, 2007, 91 (04)