Effect of Strain Hardened Inner Surface Layers on Stress Corrosion Cracking of Type 316 Stainless Steel in Simulated PWR Primary Water

被引:7
|
作者
Yonezawa, Toshio [1 ]
Watanabe, Masashi [1 ]
Hashimoto, Atsushi [2 ]
Olson, M. D. [3 ]
Dewald, A. T. [3 ]
Hill, M. R. [4 ]
机构
[1] Tohoku Univ, NICHe, FRI, Aoba Ku, 6-6-10 Aoba, Sendai, Miyagi 9808579, Japan
[2] Kobe Mat Testing Lab Co Ltd, 47-13 Niijima, Harima 6750155, Japan
[3] Hill Engn LLC, 3083 Gold Canal Dr, Rancho Cordova, CA USA
[4] Univ Calif Davis, Dept Mech & Aerosp Engn, One Shields Ave, Davis, CA 95616 USA
关键词
DISSOLVED HYDROGEN; INITIATION; BEHAVIOR; GROWTH;
D O I
10.1007/s11661-019-05137-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the relationship between SCC growth rate and Vickers hardness for Type 316 stainless steel at various temperatures in simulated PWR primary water was investigated. In addition, IGSCC growth measurements were conducted using so-called functionally graded cold-rolled specimens made of Type 316 stainless steel, in simulated PWR primary water. Residual stress measurements were performed using the contour and slitting methods on the functionally graded cold-rolled specimens. The contour method measurements found highly tensile stress (350MPa) toward the surface of the side with a larger thickness reduction and low-magnitude stress elsewhere. The purpose of these latter specimens was to evaluate the effect of heavily cold-worked layers on the inner surface of components made of Type 316 stainless steel on the possibility that IGSCC could penetrate through the wall thickness. The test data showed that the work-hardened inner surface does not always have a detrimental effect on SCC susceptibility. However, if any surface cracks exist within the work-hardened inner surface layer of any components, the stress at the crack tip becomes very large and SCC easily initiates. Nevertheless, even if IGSCC initiates from a heavily cold-worked layer at the inner surface, IGSCC growth rate in Type 316 stainless steel was found to eventually become negligibly small or arrests in the soft base material. (C) The Minerals, Metals & Materials Society and ASM International 2019
引用
收藏
页码:2462 / 2485
页数:24
相关论文
共 50 条
  • [11] Proton irradiation assisted localized corrosion and stress corrosion cracking in 304 nuclear grade stainless steel in simulated primary PWR water
    Ping Deng
    Qunjia Peng
    En-Hou Han
    Wei Ke
    Chen Sun
    JournalofMaterialsScience&Technology, 2021, 65 (06) : 61 - 71
  • [12] Proton irradiation assisted localized corrosion and stress corrosion cracking in 304 nuclear grade stainless steel in simulated primary PWR water
    Deng, Ping
    Peng, Qunjia
    Han, En-Hou
    Ke, Wei
    Sun, Chen
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 65 : 61 - 71
  • [13] TEM investigation of intergranular stress corrosion cracking for 316 stainless steel in PWR environment
    Huang, YZ
    Titchmarsh, JM
    ACTA MATERIALIA, 2006, 54 (03) : 635 - 641
  • [14] Effect of Thermal Treatment on Stress Corrosion Cracking Susceptibility in Alloy 600 and Type 316 Stainless Steel Under Simulated Pressurized Water Reactor Primary Conditions
    Kanzaki, Manabu
    Masaki, Yasuhiro
    Kudo, Takeo
    CORROSION, 2015, 71 (01) : 57 - 64
  • [15] The effects of cold rolling orientation and water chemistry on stress corrosion cracking behavior of 316L stainless steel in simulated PWR water environments
    Chen, Junjie
    Lu, Zhanpeng
    Xiao, Qian
    Ru, Xiangkun
    Han, Guangdong
    Chen, Zhen
    Zhou, Bangxin
    Shoji, Tetsuo
    JOURNAL OF NUCLEAR MATERIALS, 2016, 472 : 1 - 12
  • [16] IG-Crack Susceptibility of Type-316 Stainless Steel in the Simulated PWR Primary Water
    Takemoto, Mikio
    Takeda, Kiyoko
    Kudo, Takeo
    Zairyo to Kankyo/ Corrosion Engineering, 2021, 69 (12): : 333 - 350
  • [17] Stress corrosion cracking of uni-directionally cold worked 316NG stainless steel in simulated PWR primary water with various dissolved hydrogen concentrations
    Meng, Fanjiang
    Lu, Zhanpeng
    Shoji, Tetsuo
    Wang, Jianqiu
    Han, En-hou
    Ke, Wei
    CORROSION SCIENCE, 2011, 53 (08) : 2558 - 2565
  • [18] Effects of dissolved hydrogen and surface condition on the intergranular stress corrosion cracking initiation and short crack growth behavior of non-sensitized 316 stainless steel in simulated PWR primary water
    Zhong, Xiangyu
    Bali, Shirish Chandrakant
    Shoji, Tetsuo
    CORROSION SCIENCE, 2017, 118 : 143 - 157
  • [19] Effect of irradiation on corrosion of 304 nuclear grade stainless steel in simulated PWR primary water
    Deng, Ping
    Peng, Qunjia
    Han, En-Hou
    Ke, Wei
    Sun, Chen
    Jiao, Zhijie
    CORROSION SCIENCE, 2017, 127 : 91 - 100
  • [20] Irradiation assisted stress corrosion cracking of 347 stainless steel in simulated PWR primary water containing lithium hydroxide or potassium hydroxide
    Sinjlawi, Abdullah S.
    Dong, Lijin
    Ickes, Mickael
    Sun, Kai
    Was, Gary S.
    JOURNAL OF NUCLEAR MATERIALS, 2023, 586