Effect of Strain Hardened Inner Surface Layers on Stress Corrosion Cracking of Type 316 Stainless Steel in Simulated PWR Primary Water

被引:7
|
作者
Yonezawa, Toshio [1 ]
Watanabe, Masashi [1 ]
Hashimoto, Atsushi [2 ]
Olson, M. D. [3 ]
Dewald, A. T. [3 ]
Hill, M. R. [4 ]
机构
[1] Tohoku Univ, NICHe, FRI, Aoba Ku, 6-6-10 Aoba, Sendai, Miyagi 9808579, Japan
[2] Kobe Mat Testing Lab Co Ltd, 47-13 Niijima, Harima 6750155, Japan
[3] Hill Engn LLC, 3083 Gold Canal Dr, Rancho Cordova, CA USA
[4] Univ Calif Davis, Dept Mech & Aerosp Engn, One Shields Ave, Davis, CA 95616 USA
关键词
DISSOLVED HYDROGEN; INITIATION; BEHAVIOR; GROWTH;
D O I
10.1007/s11661-019-05137-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the relationship between SCC growth rate and Vickers hardness for Type 316 stainless steel at various temperatures in simulated PWR primary water was investigated. In addition, IGSCC growth measurements were conducted using so-called functionally graded cold-rolled specimens made of Type 316 stainless steel, in simulated PWR primary water. Residual stress measurements were performed using the contour and slitting methods on the functionally graded cold-rolled specimens. The contour method measurements found highly tensile stress (350MPa) toward the surface of the side with a larger thickness reduction and low-magnitude stress elsewhere. The purpose of these latter specimens was to evaluate the effect of heavily cold-worked layers on the inner surface of components made of Type 316 stainless steel on the possibility that IGSCC could penetrate through the wall thickness. The test data showed that the work-hardened inner surface does not always have a detrimental effect on SCC susceptibility. However, if any surface cracks exist within the work-hardened inner surface layer of any components, the stress at the crack tip becomes very large and SCC easily initiates. Nevertheless, even if IGSCC initiates from a heavily cold-worked layer at the inner surface, IGSCC growth rate in Type 316 stainless steel was found to eventually become negligibly small or arrests in the soft base material. (C) The Minerals, Metals & Materials Society and ASM International 2019
引用
收藏
页码:2462 / 2485
页数:24
相关论文
共 50 条
  • [1] Effect of Strain Hardened Inner Surface Layers on Stress Corrosion Cracking of Type 316 Stainless Steel in Simulated PWR Primary Water
    Toshio Yonezawa
    Masashi Watanabe
    Atsushi Hashimoto
    M. D. Olson
    A. T. DeWald
    M. R. Hill
    Metallurgical and Materials Transactions A, 2019, 50 : 2462 - 2485
  • [2] Effect of surface machining on the corrosion behaviour of 316 austenitic stainless steel in simulated PWR water
    Wang, Siyang
    Hu, Yujin
    Fang, Kewei
    Zhang, Wenqian
    Wang, Xuelin
    CORROSION SCIENCE, 2017, 126 : 104 - 120
  • [3] Evaluation of stress corrosion cracking susceptibility of forged 316 stainless steel in simulated primary water
    Zhu, Ruolin
    Wang, Jianqiu
    Ming, Hongliang
    Zhang, Zhiming
    Han, En-Hou
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (03): : 328 - 336
  • [4] Stress Corrosion Behaviors of 316LN Stainless Steel in a Simulated PWR Primary Water Environment
    Huang, Yong
    Wu, Weisong
    Cong, Shuo
    Ran, Guang
    Cen, Danxia
    Li, Ning
    MATERIALS, 2018, 11 (09)
  • [5] FATIGUE LIFE OF THE STRAIN HARDENED AUSTENITIC STAINLESS STEEL IN SIMULATED PWR PRIMARY WATER
    Tsutsumi, Kazuya
    Huin, Nicolas
    Couvant, Thierry
    Henaff, Gilbert
    Mendez, Jose
    Chollet, Denis
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, PVP 2012, VOL 1, 2012, : 155 - 164
  • [6] Effects of Aluminum Addition on the Corrosion of 316 Stainless Steel in the Simulated Primary Circuit Water of PWR
    Song, Xiao-Fang
    Khalil, Rabah A.
    Zhang, Ke-Gang
    Zhang, Sheng-Han
    INTERNATIONAL CONFERENCE ON ENERGY DEVELOPMENT AND ENVIRONMENTAL PROTECTION (EDEP 2017), 2017, 168 : 141 - 146
  • [7] CONTINUITY OF ENVIRONMENTALLY ASSISTED FATIGUE AND STRESS CORROSION CRACKING BASED ON SHORT CRACK GROWTH BEHAVIOR OF 316 STAINLESS STEEL IN SIMULATED PWR PRIMARY WATER
    Shim, Choongmoo
    Takeda, Yoichi
    Shoji, Tetsuo
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2017, VOL 3B, 2017,
  • [8] BEHAVIOR OF STRESS CORROSION CRACKING FOR TYPE 316L STAINLESS STEEL WITH CONTROLLED DISTRIBUTION OF SURFACE WORK HARDENED LAYER IN SIMULATED BOILING WATER REACTORS ENVIRONMENT
    Miura, Yasufumi
    Miyahara, Yuichi
    Sato, Masaru
    Kako, Kenji
    Tani, Jun-ichi
    15TH INTERNATIONAL CONFERENCE ON ENVIRONMENTAL DEGRADATION OF MATERIALS IN NUCLEAR POWER SYSTEMS-WATER REACTORS, 2011, : 439 - 449
  • [9] Influences of boric acid and lithium hydroxide in simulated primary water of PWR on intergranular stress corrosion cracking of stainless steel
    Institute of Nuclear Safety System, Incorporated, 64 Sata, Mihama-cho, Mikata-gun, Fukui 919-1205, Japan
    不详
    Trans. At. Energy Soc. Jpn., 1 (77-90):
  • [10] Effect of Grain Orientation on Irradiation Assisted Corrosion of 316L Stainless Steel in Simulated PWR Primary Water
    Hanbury, Rigel D.
    Was, Gary S.
    PROCEEDINGS OF THE 18TH INTERNATIONAL CONFERENCE ON ENVIRONMENTAL DEGRADATION OF MATERIALS IN NUCLEAR POWER SYSTEMS - WATER REACTORS, VOL 2, 2018, : 1087 - 1096