The solder balls on the plastic ball grid array (PBGA) packages provide both electrical input/output and mechanical supports. Mechanical properties and strengths of solder balls significantly influence the PBGA package reliability. Temperature cycling test has been widely used in flip-chip technology (FCT) ([1-3]) in order to simulate the failure mode due to fatigue and aging under repeatedly heat treatment. In this study, ball shear test was employed for measuring mechanical properties in the joint of the Sn-3Ag-0.5Cu solder ball(phi = 100 mu m) attached to Ti/Ni(V)/Cu UBM. The alloys studied included Sn-3Ag-0.5Cu and baseline eutectic Sn-37Pb. FE-EPMA was used to quantitatively analyze intermetallic compounds and to observe fracture surface. After repeatedly heat treatments, there are some differences on fracture surfaces between Sn-3Ag-0.5Cu and Sn-37Pb joint. The fracture surface of Sn-37Pb joint was ductile after TCT treatment. Only tin rich and lead rich phase were observed in the solder matrix of Sn-37Pb system, and no precipitated compound formed during the heat treatment. The force of shear test was almost the same after 1000 times TCT. In the Sn-3Ag-0.5Cu system, Ag would dissolve in Sri to form Ag3Sn. There were (Cu, Ni)(6)Sn-5 and (Cu, Ni)(3)Sn IMC formation between Sn-3Ag-0.5Cu solder and Ti/Ni(V)/Cu UBM.([4-6]) After TCT treatment, the growth of (Cu, Ni)(6)Sn-5 IMCs would affect the fracture surface. In this study, the compounds of Ag3Sn and (Cu, Ni)(6)Sn-5 in the Sn-3Ag-0.5Cu joint grew slowly. After shear test, the fracture surface appeared brittle. The shear strength of Sn-3Ag-0.5Cu was higher than Sn-37Pb. The relationships between microstructure and strength of the joints as functions of thermal cycling test (TCT) cycle were investigated and discussed.
引用
收藏
页码:927 / 930
页数:4
相关论文
共 50 条
  • [21] Mechanical properties versus temperature relation of individual phases in Sn-3.0Ag-0.5Cu lead-free solder alloy
    Gao, Feng
    Nishikawa, Hiroshi
    Takemoto, Tadashi
    Qu, Jianmin
    MICROELECTRONICS RELIABILITY, 2009, 49 (03) : 296 - 302
  • [22] The Role of Lengthscale in the Creep of Sn-3Ag-0.5Cu Solder Microstructures
    Gu, Tianhong
    Gourlay, Christopher M.
    Britton, T. Ben
    JOURNAL OF ELECTRONIC MATERIALS, 2021, 50 (03) : 926 - 938
  • [23] In-situ study of creep in Sn-3Ag-0.5Cu solder
    Gu, Tianhong
    Tong, Vivian S.
    Gourlay, Christopher M.
    Ben Britton, T.
    ACTA MATERIALIA, 2020, 196 (196) : 31 - 43
  • [24] Electromigration effect on solder bump in Cu/Sn-3Ag-0.5Cu/Cu system
    Yamanaka, Kimihiro
    Tsukada, Yutaka
    Suganuma, Katsuaki
    SCRIPTA MATERIALIA, 2006, 55 (10) : 867 - 870
  • [25] The Microstructure and Fracture Behavior of Sn-3Ag-0.5Cu Solder Joints
    Wang, T. S.
    Liu, S. C.
    Huang, Y. L.
    Lin, K. L.
    Lai, Y. S.
    2008 EMAP CONFERENCE PROCEEDINGS, 2008, : 293 - +
  • [26] Effects of impurities on solderability of Sn-3.0Ag-0.5Cu lead-free solder
    Katayama, N
    Tanaka, H
    Akanuma, M
    Miyazaki, M
    Nomura, S
    Takei, T
    Takemoto, T
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 1027 - 1030
  • [27] Studies on solder bump electromigration in Cu/Sn-3Ag-0.5Cu/Cu system
    Yamanaka, Kimihiro
    Tsukada, Yutaka
    Suganuma, Katsuaki
    MICROELECTRONICS RELIABILITY, 2007, 47 (08) : 1280 - 1287
  • [28] Corrosion behavior of Sn-3.0Ag-0.5Cu lead-free solder joints
    Wang, Mingna
    Wang, Jianqiu
    Ke, Wei
    MICROELECTRONICS RELIABILITY, 2017, 73 : 69 - 75
  • [29] The Role of Lengthscale in the Creep of Sn-3Ag-0.5Cu Solder Microstructures
    Tianhong Gu
    Christopher M. Gourlay
    T. Ben Britton
    Journal of Electronic Materials, 2021, 50 : 926 - 938
  • [30] Creep Behavior Investigation of Lead-Free Solder Alloy Sn96.5Ag3Cu0.5
    Zhu, Fulong
    Song, Shao
    Zhang, Wei
    Liu, Sheng
    2010 11TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING (ICEPT-HDP), 2010, : 195 - 198