Prelithiation Activates Li(Ni0.5Mn0.3Co0.2)O2 for High Capacity and Excellent Cycling Stability

被引:72
|
作者
Wu, Zhongzhen [1 ]
Ji, Shunping [1 ]
Zheng, Jiaxin [1 ]
Hu, Zongxiang [1 ]
Xiao, Shu [1 ]
Wei, Yi [1 ]
Zhuo, Zengqing [1 ,2 ]
Lin, Yuan [1 ]
Yang, Wanli [2 ]
Xu, Kang [3 ]
Amine, Khalil [1 ,4 ]
Pan, Feng [1 ]
机构
[1] Peking Univ, Shenzhen Grad Sch, Sch Adv Mat, Shenzhen 518055, Peoples R China
[2] Univ Calif Berkeley, Lawrence Berkeley Natl Lab, Adv Light Source, Berkeley, CA 94720 USA
[3] US Army Res Lab, Adelphi, MD 20783 USA
[4] Argonne Natl Lab, Chem Sci & Engn Div, Electrochem Technol Program, Argonne, IL 60439 USA
基金
美国国家科学基金会;
关键词
prelithiation; two-layer Li; Li(Ni0.5Mn0.3Co0.2)O-2; carbint nanotube (CNT); solid electrolyte interface (SEI); ATOMIC LAYER DEPOSITION; CATHODE MATERIALS; ION; ELECTRODES; NI; HYDROGENATION; FADE; CO;
D O I
10.1021/acs.nanolett.5b02246
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Transition metal oxide materials Li(NiMnyCoz)O-2 (NMC) based on layered structures are expected to replace LiFePO4 in automotive Li-ion batteries because of their higher specific capacity and operating potential. However, the actual usable capacity is much lower than the promised theoretical value [Uchaker, E.; Cao, G. Nano Today 2014 9, 499-524; Tarascon, J.-M.; Armand, M. Nature 2001 414, 359-367], in addition to the often poor cycling performance and the first-cycle Coulombic efficiency, for which Mn(II)-dissolution, its immobilization in solid electrolyte interface (SEI), oxidation of electrolytes by Ni, and other parasitic process thereat have been held responsible [Zhan, C., et al. Nat. Commun. 2013 4, 2437; Wang, L,et al. J. Solid State Electrochem. 2009 13, 1157-1164; Lin, F., et al. Nat. Commun. 2014.5, 4529]. Previously, we reported a composite Li(Ni0.5Mn0.3Co0.2)O-2 (NMC532) depolarized by the embedded carbon nanotube (CNT) and achieved capacity close to the theoretical limit [Wu, Z., et al. Nano. Lett. 2014 14, 4700-4706]; unfortunately, this high capacity failed to be maintained in long-term cycling due to the degrading contacts between the active ingredient and CNT network. On the basis of that NMC532/ CNT composite, the present work proposes a unique "prelithiation process", which brought the cathode to low potentials before regular cycling and led to an intetphase that is normally formed only on anode surfaces. The complete coverage of cathode surface by this, similar to 40 nm thick interphase effectively prevented Mn(II) dissolution and minimized the side reactions of Ni, Co, and Mn at the NMC interface during the subsequent cycling process. More importantly, such a "prelithiation" process activated a structure containing two Li layers near the surface of NMC532 particles, as verified by XRD and first principle calculation. Hence, a new cathode material of both high capacity with depolarized structure and excellent cycling performance was generated. This new structure can be incorporated in essentially all the NMC-based layered cathode materials, providing us with an effective tool to tailor-design future new cathode materials for lithium batteries.
引用
下载
收藏
页码:5590 / 5596
页数:7
相关论文
共 50 条
  • [11] The effects of FePO4-coating on high-voltage cycling stability and rate capability of Li[Ni0.5Co0.2Mn0.3]O2
    Bai, Yansong
    Wang, Xianyou
    Yang, Shunyi
    Zhang, Xiaoyan
    Yang, Xiukang
    Shu, Hongbo
    Wu, Qiang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 541 : 125 - 131
  • [12] The effect of the SEI layer on the electrochemical impedance in the graphite/ Li[Ni0.5Mn0.3Co0.2]O2 lithium-ion full cells
    Kiani, Sedighe
    Gharibi, Hussein
    Javadian, Soheila
    Zhiani, Mohammad
    Kashani, Hamideh
    APPLIED SURFACE SCIENCE, 2023, 633
  • [13] Highly textured Li(Ni0.5Mn0.3Co0.2)O2 thin films on stainless steel as cathode for lithium-ion battery
    Jacob, Clement
    Lynch, Tommy
    Chen, Aiping
    Jian, Jie
    Wang, Haiyan
    JOURNAL OF POWER SOURCES, 2013, 241 : 410 - 414
  • [14] Fluorinated Carbonate-Based Electrolyte for High-Voltage Li(Ni0.5Mn0.3Co0.2)O2/Graphite Lithium-Ion Battery
    Im, Jinsol
    Lee, Jieun
    Ryou, Myung-Hyun
    Lee, Yong Min
    Cho, Kuk Young
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2017, 164 (01) : A6381 - A6385
  • [15] CuO-coated Li[Ni0.5Co0.2Mn0.3]O2 cathode material with improved cycling performance at high rates
    Liu, Ting
    Zhao, Shi-Xi
    Wang, Kezhen
    Nan, Ce-Wen
    ELECTROCHIMICA ACTA, 2012, 85 : 605 - 611
  • [16] LiLaPO4-coated Li[Ni0.5Co0.2Mn0.3]O2 and AlF3-coated Li[Ni0.5Co0.2Mn0.3]O2 blend composite for lithium ion batteries
    Song, Han Gab
    Park, Yong Joon
    MATERIALS RESEARCH BULLETIN, 2012, 47 (10) : 2843 - 2846
  • [17] Enhanced cycling stability and rate performance of Li[Ni0.5Co0.2Mn0.3] O2 by CeO2 coating at high cut-off voltage
    Liu, Kun
    Yang, Gao-Li
    Dong, Yue
    Shi, Ting
    Chen, Li
    JOURNAL OF POWER SOURCES, 2015, 281 : 370 - 377
  • [18] Effect of overcharge on Li(Ni0.5Mn0.3Co0.2)O2 cathodes: NMP-soluble binder. II - Chemical changes in the anode
    Bloom, Ira
    Bareno, Javier
    Rago, Nancy Dietz
    Dogan, Fulya
    Graczyk, Donald G.
    Tsai, Yifen
    Naik, Seema R.
    Han, Sang-Don
    Lee, Eungje
    Du, Zhijia
    Sheng, Yangping
    Li, Jianlin
    Wood, David L., III
    Steele, Leigh Anna
    Lamb, Joshua
    Spangler, Scott
    Grosso, Christopher
    Fenton, Kyle
    JOURNAL OF POWER SOURCES, 2018, 385 : 156 - 164
  • [19] Impact of a Titanium-Based Surface Coating Applied to Li[Ni0.5Mn0.3Co0.2]O2 on Lithium-Ion Cell Performance
    Ma, Lin
    Young, Scott
    Ellis, L. D.
    Huang, Que
    Ma, Xiaowei
    Chatzidakis, M.
    Li, Hongyang
    Thompson, Lauren
    Eldesoky, Ahmed
    McFarlane, C. R. M.
    Botton, G. A.
    Hill, Ian G.
    Dahn, J. R.
    ACS APPLIED ENERGY MATERIALS, 2018, 1 (12): : 7052 - 7064
  • [20] Li[Ni0.5Mn0.3Co0.2]O2 as a Superior Alternative to LiFePO4 for Long-Lived Low Voltage Li-Ion Cells
    Aiken, C. P.
    Logan, E. R.
    Eldesoky, A.
    Hebecker, H.
    Oxner, J. M.
    Harlow, J. E.
    Metzger, Michael
    Dahn, J. R.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2022, 169 (05)